Shoji Miyanishi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Shoji Miyanishi has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Takeo Yamaguchi
Institute of Science Tokyo
10 shared publications - Hidenori Kuroki
Institute of Science Tokyo
3 shared publications - Sreekanth Narayanaru
Institute of Science Tokyo
3 shared publications - Gopinathan M. Anilkumar
Institute of Science Tokyo R1-17, 4259 Nagatsuta-cho, Midori-ku
2 shared publications - Erjun Zhou
College of Biological and Chemical Engineering Jiaxing University Jiaxing People's Republic of China
1 shared publication - Hafis Pratama Rendra Graha
Institut Teknologi Bandung
1 shared publication
Latest Publications
- Open Access
- 2 January 2026
- Published by Wiley in Advanced Energy and Sustainability Research
- Vol. 7 (1)
Perfluorosulfonic Acid Membrane with Engineered Ionic Cluster Channels and Pore‐Filling Structure for Efficient Alkaline Water Electrolysis
A novel separator for alkaline water electrolysis (AWE) is developed by structurally engineering a pore‐filling perfluorosulfonic acid (PFSA) membrane, effectively mitigating the energy inefficiency and hydrogen crossover challenges associated with conventional AWE separators. A pore‐filling PFSA membrane with an extended polytetrafluoroethylene matrix is heated in a high‐boiling‐point polar organic solvent to generate enlarged phase‐separated nanoscale ionic cluster channels, yielding a swollen membrane with improved ionic conductivity. This swollen pore‐filling PFSA membrane demonstrates enhanced selectivity for OH − transport over H 2 permeability under electrolysis conditions. An AWE with a zero‐gap electrode configuration comprising this membrane and nonprecious metal electrodes is operated in 1 M KOH at 80 °C, exhibiting a current density of 1.0 A cm −2 at a cell voltage of 1.76 V, a corresponding energy efficiency of 84%, and a low H 2 crossover rate (0.9% H 2 in the anode gas stream at 1.0 A cm −2 ). The integration of a high‐performance cathode catalyst within a pore‐filling swollen‐PFSA membrane‐based membrane–electrode assembly further enhances the performance (1.0 A cm −2 at 1.68 V with an energy efficiency of 88%). These findings emphasize the potential of this membrane as a next‐generation separator for AWE, a compelling combination of ionic conductivity, low gas‐crossover, and efficiency.
- 2 January 2026
- Published by Wiley in Advanced Energy and Sustainability Research
- Vol. 7 (1)
Open AccessPerfluorosulfonic Acid Membrane with Engineered Ionic Cluster Channels and Pore‐Filling Structure for Efficient Alkaline Water Electrolysis
A novel separator for alkaline water electrolysis (AWE) is developed by structurally engineering a pore‐filling perfluorosulfonic acid (PFSA) membrane, effectively mitigating the energy inefficiency and hydrogen crossover challenges associated with conventional AWE separators. A pore‐filling PFSA membrane with an extended polytetrafluoroethylene matrix is heated in a high‐boiling‐point polar organic solvent to generate enlarged phase‐separated nanoscale ionic cluster channels, yielding a swollen membrane with improved ionic conductivity. This swollen pore‐filling PFSA membrane demonstrates enhanced selectivity for OH − transport over H 2 permeability under electrolysis conditions. An AWE with a zero‐gap electrode configuration comprising this membrane and nonprecious metal electrodes is operated in 1 M KOH at 80 °C, exhibiting a current density of 1.0 A cm −2 at a cell voltage of 1.76 V, a corresponding energy efficiency of 84%, and a low H 2 crossover rate (0.9% H 2 in the anode gas stream at 1.0 A cm −2 ). The integration of a high‐performance cathode catalyst within a pore‐filling swollen‐PFSA membrane‐based membrane–electrode assembly further enhances the performance (1.0 A cm −2 at 1.68 V with an energy efficiency of 88%). These findings emphasize the potential of this membrane as a next‐generation separator for AWE, a compelling combination of ionic conductivity, low gas‐crossover, and efficiency.
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (40) , 1989
Effect of π- π Stacking in the Anion Exchange Membrane on the Durability and Gas Crossover
Anion exchange membrane water electrolyzer (AEMWE) with non-noble metal catalyst and electrolyzer components and energy efficiency close to proton exchange membrane water electrolyzer (PEMWE) is suitable to reduce the cost of green hydrogen. [1] The lack of membrane durability is the fundamental issue for the commercialization of AEMWE. [2] The durability of AEMs are depend on the stability of polymeric back bone and the ion exchange group. Earlier, to improve the performance of AEMWE, AEM with high ion exchange capacity (IEC) was used. However, high IEC increases the membrane swelling, thereby leading to poor mechanical stability. It is important to address the trade-off between the performance and durability of the AEM. In this point, we found that increasing π–π stacking between the polymeric backbone chains effectively reduces the swelling of the AEMs with high IEC. In this work, we present the effect of π–π interaction between the polymeric backbone on the durability and hydrogen crossover of the AEM. We developed two types of AEMs, PFT-C 10 -TMA [3] (Figure 1a) and PFT-C 6 -TMA-C 1 (Figure 1b), both have aromatic backbone and aliphatic side chains with ion exchange group, and having similar IEC values (2.7 meq/g). PFT-C 6 -TMA-C 1 AEM has aromatic groups with shorter aliphatic side chains (C 6 ) with ion exchange group and (C1) without ion exchange groups in the polymeric backbone, leading to the formation of π–π interaction. Membrane electrode assemblies (MEA) were prepared using these membranes, and their durability and hydrogen gas crossover were tested. Under similar test conditions, the MEA with PFT-C 6 -TMA-C 1 showed lower hydrogen crossover than the MEA based on PFT-C 10 -TMA (Figure 1c). Furthermore, the PFT-C 6 -TMA-C 1 membrane showed stable performance in load cycle durability tests conducted between 0.1–3 A/cm 2 at 80 °C. These results suggest that PFT-C 6 -TMA-C 1 membrane has stronger π–π stacking between the polymeric backbone chains, which increases the durability and reduces the hydrogen gas crossover for AEMWE. Acknowledgement This presentation is based on results obtained from a project, JPNP20003, commissioned by the New Energy and Industrial Technology Development Organization (NEDO), Japan. References A. Miller, K. Bouzek, J. Hnat, S. Loos, C.I. Bernäcker, T. Weißgärber, L. Röntzsch, J. Meier-Haack, Sustain. Energy Fuels, 4 , 2114–2133 (2020). Li, A.R. Motz, C. Bae, C. Fujimoto, G. Yang, F. Y. Zhang, K. E. Ayers, Y. S. Kim, Energy Environ. Sci., 14 , 3393- 3419 (2021). Miyanishi, T. Yamaguchi, Polym. Chem., 11 , 3812–3820, (2020) Figure 1. Chemical structures of (a) PFT-C 10 -TMA, (b) PFT-C 6 -TMA-C 1 . (c) Hydrogen crossover values of PFT-C 10 -TMA and PFT-C 6 -TMA-C 1 membrane based MEAs measured by performing electrolysis at 2A/cm 2 and in 1 M KOH at 80°C. Figure 1
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02 (40) , 1989
Effect of π- π Stacking in the Anion Exchange Membrane on the Durability and Gas Crossover
Anion exchange membrane water electrolyzer (AEMWE) with non-noble metal catalyst and electrolyzer components and energy efficiency close to proton exchange membrane water electrolyzer (PEMWE) is suitable to reduce the cost of green hydrogen. [1] The lack of membrane durability is the fundamental issue for the commercialization of AEMWE. [2] The durability of AEMs are depend on the stability of polymeric back bone and the ion exchange group. Earlier, to improve the performance of AEMWE, AEM with high ion exchange capacity (IEC) was used. However, high IEC increases the membrane swelling, thereby leading to poor mechanical stability. It is important to address the trade-off between the performance and durability of the AEM. In this point, we found that increasing π–π stacking between the polymeric backbone chains effectively reduces the swelling of the AEMs with high IEC. In this work, we present the effect of π–π interaction between the polymeric backbone on the durability and hydrogen crossover of the AEM. We developed two types of AEMs, PFT-C 10 -TMA [3] (Figure 1a) and PFT-C 6 -TMA-C 1 (Figure 1b), both have aromatic backbone and aliphatic side chains with ion exchange group, and having similar IEC values (2.7 meq/g). PFT-C 6 -TMA-C 1 AEM has aromatic groups with shorter aliphatic side chains (C 6 ) with ion exchange group and (C1) without ion exchange groups in the polymeric backbone, leading to the formation of π–π interaction. Membrane electrode assemblies (MEA) were prepared using these membranes, and their durability and hydrogen gas crossover were tested. Under similar test conditions, the MEA with PFT-C 6 -TMA-C 1 showed lower hydrogen crossover than the MEA based on PFT-C 10 -TMA (Figure 1c). Furthermore, the PFT-C 6 -TMA-C 1 membrane showed stable performance in load cycle durability tests conducted between 0.1–3 A/cm 2 at 80 °C. These results suggest that PFT-C 6 -TMA-C 1 membrane has stronger π–π stacking between the polymeric backbone chains, which increases the durability and reduces the hydrogen gas crossover for AEMWE. Acknowledgement This presentation is based on results obtained from a project, JPNP20003, commissioned by the New Energy and Industrial Technology Development Organization (NEDO), Japan. References A. Miller, K. Bouzek, J. Hnat, S. Loos, C.I. Bernäcker, T. Weißgärber, L. Röntzsch, J. Meier-Haack, Sustain. Energy Fuels, 4 , 2114–2133 (2020). Li, A.R. Motz, C. Bae, C. Fujimoto, G. Yang, F. Y. Zhang, K. E. Ayers, Y. S. Kim, Energy Environ. Sci., 14 , 3393- 3419 (2021). Miyanishi, T. Yamaguchi, Polym. Chem., 11 , 3812–3820, (2020) Figure 1. Chemical structures of (a) PFT-C 10 -TMA, (b) PFT-C 6 -TMA-C 1 . (c) Hydrogen crossover values of PFT-C 10 -TMA and PFT-C 6 -TMA-C 1 membrane based MEAs measured by performing electrolysis at 2A/cm 2 and in 1 M KOH at 80°C. Figure 1
- 10 September 2025
- Published by Royal Society of Chemistry (RSC) in Polymer Chemistry
- Vol. 16 (40) , 4423-4432
Synthesis and properties of highly durable poly(fluorene-alt-tetrafluorophenylene) anion-conducting membranes with cyclic ammonium groups
The alkaline durability of anion exchange membranes is essential for the long-term operation of anion exchange membrane water electrolyzers and fuel cells. In this study, we investigated the alkaline durability of anion exchange groups incorporated into the alkyl side-chain terminals of model low-molecular-weight fluorene compounds. As a result, we found that quaternary ammonium groups with a cyclic structure such as quinuclidinium and piperidinium have high durability. These cyclic ammonium groups were incorporated into high-molecular-weight poly-(fluorene-alt-tetrafluorophenylene) to form membranes with high OH− conductivity (>100 mS cm−1) in water at 80 °C and higher alkaline durability than similar polymers with linear alkyl trimethyl ammonium groups as the anion exchange group. A synthesized polymer with the piperidinium group showed optimal alkaline durability among all membranes examined in this study, with almost no decrease in ionic conductivity observed for 240 h under the accelerated test conditions at 80 °C in 8 M NaOH solution.
- 10 September 2025
- Published by Royal Society of Chemistry (RSC) in Polymer Chemistry
- Vol. 16 (40) , 4423-4432
Synthesis and properties of highly durable poly(fluorene-alt-tetrafluorophenylene) anion-conducting membranes with cyclic ammonium groups
The alkaline durability of anion exchange membranes is essential for the long-term operation of anion exchange membrane water electrolyzers and fuel cells. In this study, we investigated the alkaline durability of anion exchange groups incorporated into the alkyl side-chain terminals of model low-molecular-weight fluorene compounds. As a result, we found that quaternary ammonium groups with a cyclic structure such as quinuclidinium and piperidinium have high durability. These cyclic ammonium groups were incorporated into high-molecular-weight poly-(fluorene-alt-tetrafluorophenylene) to form membranes with high OH− conductivity (>100 mS cm−1) in water at 80 °C and higher alkaline durability than similar polymers with linear alkyl trimethyl ammonium groups as the anion exchange group. A synthesized polymer with the piperidinium group showed optimal alkaline durability among all membranes examined in this study, with almost no decrease in ionic conductivity observed for 240 h under the accelerated test conditions at 80 °C in 8 M NaOH solution.
- Open Access
- 1 August 2025
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 15 (34) , 27924-27932
Highly phase-separated alternating copolymer of alkyl vinyl ether and sulfonic acid group-containing trifluoro vinyl ether
Alternating copolymers of alkyl vinyl ethers and perfluorosulfonic acid monomer were synthesized, forming lamellar structures. Longer side chains resulted in more ordered morphologies and enhanced water diffusion.
- 1 August 2025
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 15 (34) , 27924-27932
Open AccessHighly phase-separated alternating copolymer of alkyl vinyl ether and sulfonic acid group-containing trifluoro vinyl ether
Alternating copolymers of alkyl vinyl ethers and perfluorosulfonic acid monomer were synthesized, forming lamellar structures. Longer side chains resulted in more ordered morphologies and enhanced water diffusion.
- 27 February 2025
- Published by Royal Society of Chemistry (RSC) in Sustainable Energy & Fuels
- Vol. 9 (8) , 2022-2030
A polyfluorene-based electrolyte membrane for hydrogen/oxygen gas separation under humidified conditions
Hydrogen/oxygen separation under wet conditions has recently become important in the production of hydrogen. This study developed an electrolyte membrane, PFST-C8-SO3H, with a poly(fluorene-alt-tetrafluorophenylene) backbone and achieved high hydrogen/oxygen separation performance under wet conditions. Polymer membranes with a normal aromatic backbone frequently exhibit high rigidity and low gas permeability due to π stacking. However, by introducing a long alkyl sulfonic acid side chain and a three-dimensionally twisted structure into the skeleton, it had a high free volume and a specifically high permeability for hydrogen. The membrane shows lower water vapor absorption than a typical polyelectrolyte membrane, leading to retain high permselectivity under wet conditions. By optimizing the structure of the proposed polymer membrane, it is expected to exhibit better separation performance.
- 27 February 2025
- Published by Royal Society of Chemistry (RSC) in Sustainable Energy & Fuels
- Vol. 9 (8) , 2022-2030
A polyfluorene-based electrolyte membrane for hydrogen/oxygen gas separation under humidified conditions
Hydrogen/oxygen separation under wet conditions has recently become important in the production of hydrogen. This study developed an electrolyte membrane, PFST-C8-SO3H, with a poly(fluorene-alt-tetrafluorophenylene) backbone and achieved high hydrogen/oxygen separation performance under wet conditions. Polymer membranes with a normal aromatic backbone frequently exhibit high rigidity and low gas permeability due to π stacking. However, by introducing a long alkyl sulfonic acid side chain and a three-dimensionally twisted structure into the skeleton, it had a high free volume and a specifically high permeability for hydrogen. The membrane shows lower water vapor absorption than a typical polyelectrolyte membrane, leading to retain high permselectivity under wet conditions. By optimizing the structure of the proposed polymer membrane, it is expected to exhibit better separation performance.
- Open Access
- 13 June 2023
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 11 (25) , 9295-9302
Start–Stop Cyclic Durability Analysis of Membrane–Electrode Assemblies Using Polyflourene-Based Electrolytes for an Anion-Exchange Membrane Water Electrolyzer
- 13 June 2023
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 11 (25) , 9295-9302
Open AccessStart–Stop Cyclic Durability Analysis of Membrane–Electrode Assemblies Using Polyflourene-Based Electrolytes for an Anion-Exchange Membrane Water Electrolyzer
- 9 May 2020
- Published by Royal Society of Chemistry (RSC) in Polymer Chemistry
- Vol. 11 (23) , 3812-3820
Highly conductive mechanically robust high M w polyfluorene anion exchange membrane for alkaline fuel cell and water electrolysis application
New, high molecular weight poly-(fluorene-alt-tetrafluorophenylene) anion exchange membranes were synthesized by a Pd-catalyzed C–H activation method. The synthesized membranes exhibited high OH− conductivity over 100 mS cm−1, and membrane swelling could be suppressed by controlling the side chain length of the polymers. The membranes were flexible with high tensile strengh (25–42 MPa), which is comparable to Nafion 211 and likely because of their high molecular weight (Mw = 170–240 kDa). Conductivity and mechanical flexibility of the membranes did not vary significantly in 8 M NaOH at 80 °C for 168 h. These membranes hold promise for both membrane and solid ionomer materials that can be used in alkaline fuel cells or alkaline water electrolysis devices.
- 9 May 2020
- Published by Royal Society of Chemistry (RSC) in Polymer Chemistry
- Vol. 11 (23) , 3812-3820
Highly conductive mechanically robust high M w polyfluorene anion exchange membrane for alkaline fuel cell and water electrolysis application
New, high molecular weight poly-(fluorene-alt-tetrafluorophenylene) anion exchange membranes were synthesized by a Pd-catalyzed C–H activation method. The synthesized membranes exhibited high OH− conductivity over 100 mS cm−1, and membrane swelling could be suppressed by controlling the side chain length of the polymers. The membranes were flexible with high tensile strengh (25–42 MPa), which is comparable to Nafion 211 and likely because of their high molecular weight (Mw = 170–240 kDa). Conductivity and mechanical flexibility of the membranes did not vary significantly in 8 M NaOH at 80 °C for 168 h. These membranes hold promise for both membrane and solid ionomer materials that can be used in alkaline fuel cells or alkaline water electrolysis devices.
- 8 January 2019
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 7 (5) , 2219-2224
Highly durable spirobifluorene-based aromatic anion conducting polymer for a solid ionomer of alkaline fuel cells and water electrolysis cells
New aryl ether-free spirobifluorene-based anion-exchange membranes were synthesized.
- 8 January 2019
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 7 (5) , 2219-2224
Highly durable spirobifluorene-based aromatic anion conducting polymer for a solid ionomer of alkaline fuel cells and water electrolysis cells
New aryl ether-free spirobifluorene-based anion-exchange membranes were synthesized.
- 1 August 2018
- Published by Royal Society of Chemistry (RSC) in Chemical Communications
- Vol. 54 (77) , 10820-10823
Development of a novel durable aromatic anion exchange membrane using a thermally convertible precursor
A new approach for obtaining high-performance anion exchange membranes by using a thermally convertible precursor has been developed.
- 1 August 2018
- Published by Royal Society of Chemistry (RSC) in Chemical Communications
- Vol. 54 (77) , 10820-10823
Development of a novel durable aromatic anion exchange membrane using a thermally convertible precursor
A new approach for obtaining high-performance anion exchange membranes by using a thermally convertible precursor has been developed.
- 26 June 2017
- Published by Royal Society of Chemistry (RSC) in New Journal of Chemistry
- Vol. 41 (16) , 8036-8044
Analysis of the degradation mechanism of the polyarylene ether anion-exchange membrane for alkaline fuel cell and water-splitting cell applications
Model compounds of benzyltrimethylammonium (BTMA)-modified polyethersulfone, polyetheretherketone, and polyetheroctafluorobiphenyl were synthesized to analyze the degradation mechanism in alkaline fuel cell and water-splitting cell applications. From the degradation behavior of the model compounds, it was found that the BTMA-modified polyethersulfone and polyetheretherketone membranes were decomposed via ether cleavage-triggered simultaneous degradation of the backbone and the anion-exchange group. In contrast, polyetheroctafluorobiphenyl anion-exchange membranes were deteriorated by the direct nucleophilic substitution of fluorine groups in the main chain by hydroxide groups. To enhance the alkaline stability of polyarylene ether anion-exchange membranes, it is critical to not introduce electron-withdrawing groups and increase electron density around the ether linkages. The degradation rate of the model compounds was considerably accelerated in alkoxide solution compared with aqueous solution, indicating that the alkaline stability of the membrane was significantly more important in methanol or ethanol fuel cells than in hydrogen fuel cells.
- 26 June 2017
- Published by Royal Society of Chemistry (RSC) in New Journal of Chemistry
- Vol. 41 (16) , 8036-8044
Analysis of the degradation mechanism of the polyarylene ether anion-exchange membrane for alkaline fuel cell and water-splitting cell applications
Model compounds of benzyltrimethylammonium (BTMA)-modified polyethersulfone, polyetheretherketone, and polyetheroctafluorobiphenyl were synthesized to analyze the degradation mechanism in alkaline fuel cell and water-splitting cell applications. From the degradation behavior of the model compounds, it was found that the BTMA-modified polyethersulfone and polyetheretherketone membranes were decomposed via ether cleavage-triggered simultaneous degradation of the backbone and the anion-exchange group. In contrast, polyetheroctafluorobiphenyl anion-exchange membranes were deteriorated by the direct nucleophilic substitution of fluorine groups in the main chain by hydroxide groups. To enhance the alkaline stability of polyarylene ether anion-exchange membranes, it is critical to not introduce electron-withdrawing groups and increase electron density around the ether linkages. The degradation rate of the model compounds was considerably accelerated in alkoxide solution compared with aqueous solution, indicating that the alkaline stability of the membrane was significantly more important in methanol or ethanol fuel cells than in hydrogen fuel cells.