Effects of Fabrication Procedures on Fatigue Resistance of Welded Joints in Steel Orthotropic Decks
- 1 September 2009
- journal article
- Published by American Society of Civil Engineers (ASCE) in Journal of Bridge Engineering
- Vol. 14 (5) , 366-373
Abstract
A common practice for the fabrication of steel orthotropic bridge decks in the United States is to use 80% partial joint penetration (PJP) groove welds between the closed ribs and deck plate. However, it is difficult to eliminate weld melt-through with the thin rib plates. Heat straightening after welding, sometimes combined with precambering, is used to meet the deck plate flatness requirement. To study the effects of both weld melt-through and distortion control measures on the fatigue resistance of the rib-to-deck plate welded joint, six full-scale two-span orthotropic deck specimens were subjected to laboratory testing. Specimens, 10 m long and 3 m wide with four closed ribs, were fabricated with and without weld melt-through and were heat straightened; three specimens were also precambered. To simulate the effect of repetitive truck traffic, each specimen was tested up to 8 million cycles. Test results showed that six cracks initiated from the weld toe outside the rib. Only one crack developed at the...Keywords
This publication has 5 references indexed in Scilit:
- Fatigue cracks in longitudinal ribs of steel orthotropic deckInternational Journal of Fatigue, 2006
- Full-scale fatigue tests of steel orthotropic deck panel for the Bronx – Whitestone Bridge rehabilitationBridge Structures, 2005
- Full-Scale Fatigue Tests of Steel Orthotropic Decks for the Williamsburg BridgeJournal of Bridge Engineering, 2003
- In-Service Response of an Orthotropic Steel Deck Compared with Design AssumptionsTransportation Research Record: Journal of the Transportation Research Board, 2000
- Steel Orthotropic Decks: Developments in the 1990sTransportation Research Record: Journal of the Transportation Research Board, 1999