Abstract
A promising method of joining silicon with glass is the solid phase welding method that can be carried out in an air atmosphere, at low temperatures, using insignificant external compression forces and with the application of an electrostatic field of high voltage. The widespread use of the method limits a significant drawback – the instability of the quality indicators of welded joints, the main of which is mechanical strength. Primarily this is due to the imperfection of the methods for determining the welding time, during which it is possible to obtain welded joints with a given level of service properties. The influence of the dimensional parameters of glass parts and the presence of surface conductivity in them on the course of the welding process is been determined. It is shown that the welding time required to ensure the connection of KEF-4.5/0.1 silicon with Pyrex glass along the entire contact plane is determined by the peak value of the welding current at the moment of applying the electric welding voltage. The corresponding functional dependencies have been obtained for the first time. The influence of geometrical parameters of welded parts on strength of glass-silicon nodes is been investigated. The results of the experiments showed that with an increase in the ratio of the nominal contact area of the parts to the total perimeter of the side surfaces of the tubular glass part from 0.5 to 1.02 mm2/mm, the welding time increases. Computer simulation of the stress state in the nodes has been carried out. It has been found that in order to improve the performance of welded glass-silicon units by reducing the level of residual stresses, they must be designed so that the ratio of the nominal contact area of the parts to the total perimeter of the side surfaces of the tubular glass part is minimal.