Copper corrosion issue and analysis on copper damascene process
Authors:
- Yuan-Ping LeeYLYuan-Ping Lee
- 27 June 2005
- journal article
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Device and Materials Reliability
- Vol. 5 (2) , 206-211
Abstract
As semiconductor device features shrink into deep-submicron regime, copper metallization is taking the place of aluminum (Al)-tungsten (W) metallization because of the higher electrical conductivity and electromigration resistance of copper. However, it is very difficult for copper to be etched by dry etching method, thus copper metallization is created with damascene process. In this process, chemical mechanical polishing (CMP) is the key step. The wet chemical treatment in CMP makes copper corrosion to be one of the critical issues for copper metallization. This paper has addressed the three different types of copper corrosion, namely copper chemical corrosion, copper galvanic corrosion and photo assistant copper corrosion. The failure analyses for how to differentiate them and identify their root causes have been also discussed in details.Keywords
This publication has 8 references indexed in Scilit:
- Full copper wiring in a sub-0.25 μm CMOS ULSI technology2002
- Interconnect scaling-the real limiter to high performance ULSI2002
- The investigation of galvanic corrosion in post-copper-CMP cleaning2002
- Investigation of barrier and slurry effects on the galvanic corrosion of copperMicroelectronic Engineering, 2002
- Slurry Chemical Corrosion and Galvanic Corrosion during Copper Chemical Mechanical PolishingJapanese Journal of Applied Physics, 2000
- Copper Metallization for High Performance Silicon TechnologyAnnual Review of Materials Science, 2000
- Microstructure and electromigration in copper damascene linesMicroelectronics Reliability, 2000