Abstract
Novel luminescent bridged polysilsesquioxane monoliths of high transparency have been obtained by hydrolysis and condensation of the precursor under acidic conditions. The monoliths were characterized by FTIR spectroscopy, photoluminescence spectroscopy, and SEM, and they have been used as hosts of Eu3+, Tb3+ and Nd3+ ions. The luminescence lifetime of Tb3+ in this host was 2.1 ms. The interaction between the host and the lanthanide ions could be confirmed by FTIR spectra. The number of water molecules coordinated to the Eu3+ ions was determined to be one. Incorporation of Nd3+ as guest resulted in NIR-luminescent materials.