Enhanced Energy Storage Properties of BNT–ST–AN Relaxor Ferroelectric Ceramics Fabrication by the Solid‐State Combustion Technique
- 1 July 2022
- journal article
- research article
- Published by Wiley in Physica Status Solidi (a)
- Vol. 220 (10)
Abstract
The performance of high energy storage lead free 0.722(Bi0.5Na0.5TiO3)−0.228(SrTiO3)−0.05(AgNbO3) (BNT–ST–AN) ceramics prepared by the solid‐state combustion technique, using glycine as fuel is studied here. All samples are investigated for their phase formation, microstructure, dielectric, ferroelectric, and energy storage characteristics. A single perovskite phase of BNT–ST–AN is obtained from the powder calcined at 750 °C for 4 h. The sintered BNT–ST–AN ceramics present a single perovskite structure with coexisting rhombohedral (R) and cubic (C) phases in all samples. The percentage of the R phase increases while the percentage of the C phase decreases when the sintering temperature increases from 1075 to 1125 °C and then shows an opposite trend. A good microstructure, the highest density (5.42 g cm−3), the highest dielectric constant (ε r ≈ 1871 and ε m ≈ 3396), the highest electric breakdown strength (E b ≈ 130 kV cm−1) and excellent total energy storage density (W total ≈ 3.07 J cm−3), recoverable energy storage density (W rec ≈ 2.25 J cm−3) and efficiency (η ≈ 75.88%) with coexisting phases of R (62%) and C (38%) are achieved from the sample sintered at 1125 °C for 2 h. Moreover, this sample exhibits temperature and frequency stability of the energy storage properties in the range from 25 to 150 °C and 1 to 20 Hz, respectively.Keywords
This publication has 41 references indexed in Scilit:
- High Energy Storage Density and Optical Transparency of Microwave Sintered Homogeneous (Na0.5Bi0.5)(1–x)BaxTi(1–y)SnyO3 CeramicsACS Sustainable Chemistry & Engineering, 2018
- Enhanced dielectric and ferroelectric behavior in 0.94BNT-0.06BCTS lead free piezoelectric ceramics synthesized by the solid state combustion techniqueIntegrated Ferroelectrics, 2018
- Novel Strontium Titanate-Based Lead-Free Ceramics for High-Energy Storage ApplicationsACS Sustainable Chemistry & Engineering, 2017
- The preparation of lead-free bismuth sodium titanate ceramics via the solid state combustion techniqueIntegrated Ferroelectrics, 2017
- Large electrocaloric response and high energy-storage properties over a broad temperature range in lead-free NBT-ST ceramicsJournal of the European Ceramic Society, 2016
- Low Firing Temperatures and High Ferroelectric Properties of (Ba0.85Ca0.15)(Ti0.90Zr0.10)O3Lead-Free Ceramics Synthesized by the Combustion TechniqueFerroelectrics, 2016
- Lead-free piezoelectric ceramics based on (1 − x)BNKLLT–xBCTZ binary solid solutions synthesized by the solid-state combustion techniqueJournal of Materials Science, 2016
- Anti-Ferroelectric Ceramics for High Energy Density CapacitorsMaterials, 2015
- Enhanced energy storage properties of dysprosium doped strontium titanate ceramicsCeramics International, 2014
- c / a Ratio‐Dependent Energy‐Storage Density in (0.9−x) Bi 0.5 Na 0.5 TiO 3 –xBaTiO 3 –0.1K 0.5 Na 0.5 NbO 3 CeramicsJournal of the American Ceramic Society, 2011