Effects of Sterilization and Hydrolytic Degradation on the Structure, Morphology and Compressive Strength of Polylactide-Hydroxyapatite Composites
Authors:
- Mirosław KasprzakMKMirosław Kasprzak
- Agnieszka SzabłowskaASAgnieszka Szabłowska
- Agata KurzykAKAgata Kurzyk
- Paulina Tymowicz-GrzybPTPaulina Tymowicz-Grzyb
- Adrian NajmrodzkiANAdrian Najmrodzki
- Anna WoźniakAWAnna Woźniak
- Agnieszka AntosikAAAgnieszka Antosik
- Joanna PagaczJPJoanna Pagacz
- Piotr SzternerPSPiotr Szterner
- Andrzej PlichtaAndrzej Plichta
- Piotr WiecińskiPWPiotr Wieciński
- Paulina Rusek-WalaPRPaulina Rusek-Wala
Open Access
- 9 September 2022
- journal article
- research article
- Published by MDPI AG in International Journal of Molecular Sciences
- Vol. 23 (18) , 10454
Abstract
Composites based on polylactide (PLA) and hydroxyapatite (HA) were prepared using a thermally induced phase separation method. In the experimental design, the PLA with low weight-average molar mass (Mw) and high Mw were tested with the inclusion of HA synthesized as whiskers or hexagonal rods. In addition, the structure of HA whiskers was doped with Zn, whereas hexagonal rods were mixed with Sr salt. The composites were sterilized and then incubated in phosphate-buffered saline for 12 weeks at 37 °C, followed by characterization of pore size distribution, molecular properties, density and mechanical strength. Results showed a substantial reduction of PLA Mw for both polymers due to the preparation of composites, their sterilization and incubation. The distribution of pore size effectively increased after the degradation process, whereas the sterilization, furthermore, had an impact on pore size distribution depending on HA added. The inclusion of HA reduced to some extent the degradation of PLA quantitatively in the weight loss in vitro compared to the control without HA. All produced materials showed no cytotoxicity when validated against L929 mouse skin fibroblasts and hFOB 1.19 human osteoblasts. The lack of cytotoxicity was accompanied by the immunocompatibility with human monocytic cells that were able to detect pyrogenic contaminants.Keywords
Funding Information
- Fundacja na rzecz Nauki Polskiej (POIR.04.04.00-00-16D7/18)
- European Union
- European Regional Development Fund
This publication has 43 references indexed in Scilit:
- Biodegradable synthetic polymers: Preparation, functionalization and biomedical applicationProgress in Polymer Science, 2012
- Sterilization of Biomaterials of Synthetic and Biological Origin2011
- Optimization of electrospun polylactide‐based ultrathin fibers for osteoconductive bone scaffoldsJournal of Applied Polymer Science, 2011
- Bone mineral: update on chemical composition and structureOsteoporosis International, 2009
- Biodegradable implantable fluconazole delivery rods designed for the treatment of fungal osteomyelitis: Influence of gamma sterilizationJournal of Biomedical Materials Research Part A, 2006
- Effect of β-tricalcium phosphate addition on the in vitro degradation of self-reinforced poly-l,d-lactidePolymer Degradation and Stability, 2005
- In vitro degradation behavior of a novel bioresorbable composite material based on PLA and a soluble CaP glassActa Biomaterialia, 2005
- Degradation of polydispersed poly(l-lactic acid) to modulate lactic acid releaseBiomaterials, 1995
- Ultra‐high‐strength absorbable self‐reinforced polyglycolide (SR‐PGA) composite rods for internal fixation of bone fractures: In vitro and in vivo studyJournal of Biomedical Materials Research, 1991
- Crystal structure of octacalcium bis(hydrogenphosphate) tetrakis(phosphate)pentahydrate, Ca8(HP04)2(PO4)4 5H2OJournal of Chemical Crystallography, 1988