Agnieszka Szabłowska
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Agnieszka Szabłowska has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Adrian Najmrodzki
Biomaterials Research Group, Łukasiewicz Research Network–Institute of Ceramics and Building Materials, Center of Ceramic and Concrete in Warsaw, Cementowa 8, 31-983 Kraków, Poland
1 shared publication - Agata Kurzyk
Biomaterials Research Group, Łukasiewicz Research Network–Institute of Ceramics and Building Materials, Center of Ceramic and Concrete in Warsaw, Cementowa 8, 31-983 Kraków, Poland
1 shared publication - Agnieszka Antosik
Łukasiewicz Research Network - Institute of Ceramics and Building Materials
1 shared publication - Agnieszka Krupa
Department of Immunology and Infectious Biology, Faculty of Biology and Environmental Protection, University of Lodz, Banacha 12/16, 90-237 Lodz, Poland
1 shared publication - Andrzej Plichta
Faculty of Chemistry, Warsaw University of Technology, Warsaw, Poland
1 shared publication - Anna Woźniak
Biomaterials Research Group, Ceramic and Concrete Division in Warsaw, Łukasiewicz Research Network-Institute of Ceramics and Building Materials, Cementowa 8, 31-983 Kraków, Poland
1 shared publication
Latest Publications
- Open Access
- 9 September 2022
- Published by MDPI AG in International Journal of Molecular Sciences
- Vol. 23 (18) , 10454
Effects of Sterilization and Hydrolytic Degradation on the Structure, Morphology and Compressive Strength of Polylactide-Hydroxyapatite Composites
Composites based on polylactide (PLA) and hydroxyapatite (HA) were prepared using a thermally induced phase separation method. In the experimental design, the PLA with low weight-average molar mass (Mw) and high Mw were tested with the inclusion of HA synthesized as whiskers or hexagonal rods. In addition, the structure of HA whiskers was doped with Zn, whereas hexagonal rods were mixed with Sr salt. The composites were sterilized and then incubated in phosphate-buffered saline for 12 weeks at 37 °C, followed by characterization of pore size distribution, molecular properties, density and mechanical strength. Results showed a substantial reduction of PLA Mw for both polymers due to the preparation of composites, their sterilization and incubation. The distribution of pore size effectively increased after the degradation process, whereas the sterilization, furthermore, had an impact on pore size distribution depending on HA added. The inclusion of HA reduced to some extent the degradation of PLA quantitatively in the weight loss in vitro compared to the control without HA. All produced materials showed no cytotoxicity when validated against L929 mouse skin fibroblasts and hFOB 1.19 human osteoblasts. The lack of cytotoxicity was accompanied by the immunocompatibility with human monocytic cells that were able to detect pyrogenic contaminants.
- 9 September 2022
- Published by MDPI AG in International Journal of Molecular Sciences
- Vol. 23 (18) , 10454
Open AccessEffects of Sterilization and Hydrolytic Degradation on the Structure, Morphology and Compressive Strength of Polylactide-Hydroxyapatite Composites
Composites based on polylactide (PLA) and hydroxyapatite (HA) were prepared using a thermally induced phase separation method. In the experimental design, the PLA with low weight-average molar mass (Mw) and high Mw were tested with the inclusion of HA synthesized as whiskers or hexagonal rods. In addition, the structure of HA whiskers was doped with Zn, whereas hexagonal rods were mixed with Sr salt. The composites were sterilized and then incubated in phosphate-buffered saline for 12 weeks at 37 °C, followed by characterization of pore size distribution, molecular properties, density and mechanical strength. Results showed a substantial reduction of PLA Mw for both polymers due to the preparation of composites, their sterilization and incubation. The distribution of pore size effectively increased after the degradation process, whereas the sterilization, furthermore, had an impact on pore size distribution depending on HA added. The inclusion of HA reduced to some extent the degradation of PLA quantitatively in the weight loss in vitro compared to the control without HA. All produced materials showed no cytotoxicity when validated against L929 mouse skin fibroblasts and hFOB 1.19 human osteoblasts. The lack of cytotoxicity was accompanied by the immunocompatibility with human monocytic cells that were able to detect pyrogenic contaminants.