Etching efficacy and bonding performance of resin to lithium disilicate ceramic using self-etching primer with different reaction times
- 12 March 2019
- journal article
- research article
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 33 (11) , 1215-1225
Abstract
The purpose of this study was to evaluate the effect of self-etching primer on glass-ceramic at different reaction durations. Fifty specimens of lithium disilicate ceramic were divided into five groups based on the surface treatment (n = 10); Group A (control): no treatment, Group B: treated with 5%-hydrofluoric acid (HF) followed by a primer, Group C: treated with one-bottle system self-etching primer; (Monobond Etch & Prime (MEP)) for 20 s plus 40 s reaction time, Group D: MEP for 20 s plus 80 s reaction time, Group E: MEP for 20 s plus 120 s reaction time. The outcomes of shear bond strength (SBS), failure mode and surface topography were assessed. Statistical analyses were performed using ANOVA, Chi-squared test and Tukey’s test at a significance level of α = 0.05. The control group (A) demonstrated the lowest SBS value (0.11MPa, SD:0.022) which was statistically significant, compared to other groups (P < 0.0001). However, the mean SBS values were not statistically significant among the other four experimental groups. Group B yielded the highest SBS value (13.79MPa, SD:3.57), although was not statistically significant when compared to group C (11.60MPa, SD:1.23), group D (11.94MPa, SD:1.24), and group E (11.67MPa, SD:0.64), P > 0.05. Scanning electron microscope (SEM) showed increased surface roughness in HF/primer specimens compared to MEP. Stereomicroscopy analyses showed that the main mode of failure was adhesive failure in group A, while was mixed failure in the other experimental groups, with no statistical significance between the groups. The self-etching system can be considered as an alternative for the glass-ceramic surface treatment without compromising the bond strength. The time required for conditioning seems to be sufficient with 40 seconds reaction time.Keywords
This publication has 23 references indexed in Scilit:
- Possible hazardous effects of hydrofluoric acid and recommendations for treatment approach: a reviewClinical Oral Investigations, 2011
- The Influence of Surface Standardization of Lithium Disilicate Glass Ceramic on Bond Strength to a Dual Resin CementOperative Dentistry, 2011
- The effect of different etching times of acidulated phosphate fluoride gel on the shear bond strength of high-leucite ceramics bonded to composite resinThe Journal of Prosthetic Dentistry, 2007
- Effect of various surface treatment methods on the bond strength of the heat‐pressed ceramic samplesJournal of Oral Rehabilitation, 2004
- Work of adhesion of resin on treated lithia disilicate-based ceramicDental Materials, 2004
- All-ceramic crowns: bonding or cementing?Clinical Oral Investigations, 2002
- Micro-shear bond strength of dual-cured resin cement to glass ceramicsDental Materials, 2002
- Comparison of acidulated phosphate fluoride gel and hydrofluoric acid etchants for porcelain-composite repairThe Journal of Prosthetic Dentistry, 1994
- The influence of surface conditions and silane agents on the bond of resin to dental porcelainDental Materials, 1992
- Hydrofluoric acid: A review of toxicityThe Journal of Emergency Medicine, 1992