Abstract
The aim of this study was to evaluate the influence of different surface treatments (air abrasion, acid etching, and laser irradiation) on the surface roughness and bond strength of a low fusing ceramic. Thirty-six discs of low fusing ceramic (Finesse, Ceramco) were prepared (10 mm in diameter and 2 mm in thickness) according to the manufacturer’s instructions. Specimens were divided into three groups (n = 12), and the following treatments were performed: Air abrasion with alumina particles (50 μm), acid etching with 5% HF and Nd:YAG laser irradiation (distance: 1 mm, 100 mJ, 20 Hz, 2 W, and 141.54 J/cm2). Following determination of surface roughness (Ra) by profilometry, specimens were examined with scanning electron microscopy (SEM). The luting cement (Clearfil Esthetic Cement) was bonded to the ceramic specimens using Teflon tubes. After 24 h of water storage, shear bond strength test was performed using a universal testing machine at a crosshead speed of 1 mm/min. The data were analyzed with two-way analysis of variance (ANOVA) and Tukey HSD tests (α = .05). Two-way ANOVA indicated that surface roughness was significantly affected by surface treatments (p < .001). Tukey honestly significant difference (HSD) indicated that the air abrasion group had a significantly higher mean value (p < .05) than the other groups. Shear bond strength was significantly affected by surface treatments (p < .001). Tukey HSD indicated that the air abrasion group had a significantly higher mean value (p < .05) than the other groups. No significant difference was found between the acid-etching and laser-irradiation groups (p > .05). The SEM image of the laser irradiation surface appeared to be relatively smooth as compared to the images of other the groups. Air abrasion of low-fusing porcelain surfaces was effective in improving the bond strength as compared to the acid-etching and laser-irradiation methods.Keywords
This publication has 45 references indexed in Scilit:
- Surface roughness and bond strengths of glass-infiltrated alumina-ceramics prepared using various surface treatmentsJournal of Dentistry, 2009
- Surface modification for enhanced silanation of zirconia ceramicsDental Materials, 2009
- Strength influencing variables on CAD/CAM zirconia frameworksDental Materials, 2008
- Porcelain surface treatment by laser for bracket-porcelain bondingAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2005
- Bonding of an auto-adhesive luting material to enamel and dentinDental Materials, 2004
- Influence of various surface-conditioning methods on the bond strength of metal brackets to ceramic surfacesAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2003
- In vitro dentinal surface reaction of 9.5% buffered hydrofluoric acid in repair of ceramic restorations: A scanning electron microscopic investigationThe Journal of Prosthetic Dentistry, 2000
- Bonding of resin composite to carbon dioxide laser-modified human enamelDental Materials, 1994
- Enamel surface roughness analysis after laser ablation and acid‐etchingJournal of Oral Rehabilitation, 1993
- Bond strength of composite to porcelain treated with new porcelain repair agentsDental Materials, 1992