Martensite decay in micropitted gears
Authors:
- 1 February 2005
- journal article
- research article
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part J: Journal of Engineering Tribology
- Vol. 219 (2) , 77-83
Abstract
Metallographic examination performed on a number of micropitted gears has revealed microstructural features similar to those reported in the literature in fatigued bearings, namely, dark etching regions and white etching bands. In addition, a new type of fatigue-induced microstructural constituent was observed close to the surface below asperities referred to as the plastic deformation region. Finally, it is shown that the initiation and propagation of cracks leading to the formation of micropits are related to the phase transformations mentioned previously.Keywords
This publication has 38 references indexed in Scilit:
- Micropitting resistant industrial gear oils with balanced performanceIndustrial Lubrication and Tribology, 2000
- Contact fatigue of automotive gears: evolution and effects of residual stresses introduced by surface treatmentsFatigue & Fracture of Engineering Materials & Structures, 2000
- Effect of material, heat treatment, grinding and shot peening on contact fatigue life of carburised steelsInternational Journal of Fatigue, 1999
- The effect of the white layer on micro-pitting and surface contact fatigue failure of nitrided gearsProceedings of the Institution of Mechanical Engineers, Part J: Journal of Engineering Tribology, 1999
- An Experimental Investigation of Micropitting Using a Roller Disk MachineTribology Transactions, 1995
- Micropitting in Rolling and Sliding Contact Under Mixed LubricationJournal of Tribology, 1989
- The Influence of Crack Face Friction and Trapped Fluid on Surface Initiated Rolling Contact Fatigue CracksJournal of Tribology, 1988
- An investigation of surface failure of surface-hardened gears by scanning electron microscopy observationsWear, 1983
- Some Factors Influencing the Pitting, Micro-Pitting (Frosted Areas) and Slow Speed Wear of Surface Hardened GearsJournal of Mechanical Design, 1981
- Micropitting in Hertzian ContactsJournal of Lubrication Technology, 1980