Abstract
The influence of the current pulse parameters on the development of the physical contact area between some connectable surfaces during welding of solid dissimilar metals has been studied and the results are presented in this work. Using a composite of steel 20 and copper M1 compressed by a pressure of about 50 MPa as an example, there is determined the most preferable range of the pulse current’s parameters: the current density amplitude with regard to the skin effect within the range from 1 × 109 to 2 × 109 A/m2 and the specific total energy of the treatment within the range from 0.6 × 109 to 1 × 109 J/m3, in which one can efficiently control the processes of the plastic deformation of the surfaces and, thus, control the formation of a butt welded joint.