Preparation of a Gradient Anti-Oxidation Coating for Aircraft C/C Composite Brake Disc and Its High-Temperature In Situ Self-Healing Performance
Open Access
Abstract
We studied a gradient anti-oxidation coating of C/C composite materials for aircraft brake discs with a simple process and low costs. The gradient coating consists of two layers, of which the inner layer is prepared with tetraethyl orthosilicate (Si (OC2H5)4), C2H5OH, H3PO4 and B4C, and the outer layer is prepared with Na2B4O7.10H2O, B2O3, and SiO2 powder. The experimental results show that after being oxidized at 700 °C for 15 h, the oxidation weight loss of the sample with the coating was only −0.17%. At the same time, after 50 thermal cycles in air at 900 °C, the sample’s oxidation weight loss was only −0.06%. We conducted the 1:1 dynamic simulation test for aircraft brake discs, and the brake disc did not oxidize, thus meeting the requirements for aircraft use. In addition, the anti-oxidation mechanism of the coating was analyzed via scanning electron microscopy (SEM), X-ray diffraction (XRD), differential thermal analysis (DSC-TGA), and high-temperature in situ SEM.Keywords
Funding Information
- National Natural Science Foundation of China (U2141205, 2212042)
- Beijing Municipal Natural Science Foundation (U2141205, 2212042)
This publication has 10 references indexed in Scilit:
- Comparative study on the oxidation behavior of Si2BC3N/Ta4HfC5 ceramics at 1000 °C and 1500 °C: Microstructural evolution and kinetics considerationJournal of the European Ceramic Society, 2024
- Ablation Resistance of High-entropy Oxide Coatings on C/C CompositesJournal of Inorganic Materials, 2024
- Designing porous C/C composites for oxidation resistance with an analytical model based on the kinetic and architectural features of fibers and matrixComposites Part B: Engineering, 2023
- Enhancing anti-oxidation and thermal-radiation performance of the repaired borosilicate glass coating on C/C composites by Sm-dopingJournal of Materiomics, 2022
- SiBCN-precursor-derived gradient oxidation protective ceramic coating for C/C compositesSurface and Coatings Technology, 2018
- A mullite oxidation protective coating on SiC coated carbon/carbon composites by hot dippingCeramics International, 2016
- Preparation of β‐Sialon Anti‐Oxidation Ceramic Coating for C/C Composites and Infrared Stealthy Characteristic2014
- Anti-oxidation property of a multi-layer coating for carbon/carbon composites in a wind tunnel at 1500 °CNew Carbon Materials, 2010
- A phosphate-based antioxidation coating for carbon/carbon compositesNew Carbon Materials, 2006
- The thermal expansion of carbon/carbon composites from room temperature to 1400 °CJournal of Materials Science, 2006