Microstructural Response of Highly Porous Sintered Nano-silver Particle Die Attachments to Thermomechanical Cycling
Open Access
- 5 January 2024
- journal article
- research article
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 53 (3) , 1374-1398
Abstract
This paper deals with the performance of sintered nano-silver bonds used as wide-bandgap power module die attachment technology. The paper specifically explores the fine-scale microstructures of highly porous sintered attachments under power cycling to provide a deeper understanding of the significance of porosity as a reliability-related microstructural parameter. Attachments prepared at 220°C using a pressure of 6 MPa for 1 s (parameters known to generate approximately 50% porosity from previous work) and subsequently subjected to 650,000 power cycles between 50°C and 200°C are assessed. A correlative workflow integrating x-ray computed tomography, focused ion beam (FIB) and electron backscatter diffraction (EBSD) data is applied to merge meso- and nanoscale microstructural features to illuminate the degradation mechanisms. The as-sintered Ag layer has a high volume of heterogeneously distributed pores, and consists of randomly oriented equiaxed grains whose sizes vary depending on the local density of the region sampled. Power cycling promotes grain growth and the loss of twin boundaries, and these changes are more pronounced within more dense regions of the Ag attachment. In contrast, the copper substrate appears to undergo some grain refinement, with deformation twins visible within finer-grained zones during power cycling. Cracks, which appear to start off within the Ag layer, propagate across the Ag-Cu boundary and transgranularly through fine-grained regions within the copper with little tortuosity. These observations are discussed within the context of reliability behaviour. Graphical AbstractKeywords
Funding Information
- Engineering and Physical Sciences Research Council (EP/P030599/1, EP/K035304/1, EP/R004366/1, EP/R004501/1)
- European Commission (Cleansky2 JU EMINEO)
- Siemens EDA
This publication has 57 references indexed in Scilit:
- Pressureless bonding process using Ag nanoparticle paste for flexible electronics packagingScripta Materialia, 2012
- Mechanical properties of nano-silver joints as die attach materialsJournal of Alloys and Compounds, 2012
- Control of nanosilver sintering attained through organic binder burnoutJournal of Materials Research, 2007
- Effects of uni-axial mechanical stress on IGBT characteristicsMicroelectronics Reliability, 2005
- In Situ Rapid Thermal Oxidation and Reduction of Copper Thin Films and Their Applications in Ultralarge Scale IntegrationJournal of the Electrochemical Society, 2001
- Crack mechanism in wire bonding jointsMicroelectronics Reliability, 1998
- Current issues in recrystallization: a reviewMaterials Science and Engineering: A, 1997
- PREDICTING FATIGUE LIFE IN COMMERCIALLY PURE ALUMINIUM USING A SHORT CRACK GROWTH MODELFatigue & Fracture of Engineering Materials & Structures, 1995
- Secondary recrystallization effects in nanostructured elemental metalsScripta Metallurgica et Materialia, 1992
- Mechanisms of fatigue crack propagation in metals, ceramics and composites: Role of crack tip shieldingMaterials Science and Engineering: A, 1988