Pearl A. Agyakwa
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Pearl A. Agyakwa has a total of 24 co-authors. Here are the top co-authors by number of shared publications:
- Christopher Mark Johnson
Department of Electrical and Electronic Engineering, University of Nottingham, Nottingham, U.K.
5 shared publications L. Yang
Department of Electrical & Electronic Engineering, University of Nottingham, University Park, Nottingham, UK
3 shared publicationsJ.F. Li
The University of Nottingham
2 shared publicationsM.R. Corfield
The University of Nottingham
2 shared publicationsV.M.F. Marques
University of Oxford
2 shared publicationsB. Mouawad
Department of Electrical & Electronic Engineering, University of Nottingham, University Park, Nottingham, UK
1 shared publication
Latest Publications
- Open Access
- 5 January 2024
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 53 (3) , 1374-1398
Microstructural Response of Highly Porous Sintered Nano-silver Particle Die Attachments to Thermomechanical Cycling
This paper deals with the performance of sintered nano-silver bonds used as wide-bandgap power module die attachment technology. The paper specifically explores the fine-scale microstructures of highly porous sintered attachments under power cycling to provide a deeper understanding of the significance of porosity as a reliability-related microstructural parameter. Attachments prepared at 220°C using a pressure of 6 MPa for 1 s (parameters known to generate approximately 50% porosity from previous work) and subsequently subjected to 650,000 power cycles between 50°C and 200°C are assessed. A correlative workflow integrating x-ray computed tomography, focused ion beam (FIB) and electron backscatter diffraction (EBSD) data is applied to merge meso- and nanoscale microstructural features to illuminate the degradation mechanisms. The as-sintered Ag layer has a high volume of heterogeneously distributed pores, and consists of randomly oriented equiaxed grains whose sizes vary depending on the local density of the region sampled. Power cycling promotes grain growth and the loss of twin boundaries, and these changes are more pronounced within more dense regions of the Ag attachment. In contrast, the copper substrate appears to undergo some grain refinement, with deformation twins visible within finer-grained zones during power cycling. Cracks, which appear to start off within the Ag layer, propagate across the Ag-Cu boundary and transgranularly through fine-grained regions within the copper with little tortuosity. These observations are discussed within the context of reliability behaviour. Graphical Abstract
- 5 January 2024
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 53 (3) , 1374-1398
Open AccessMicrostructural Response of Highly Porous Sintered Nano-silver Particle Die Attachments to Thermomechanical Cycling
This paper deals with the performance of sintered nano-silver bonds used as wide-bandgap power module die attachment technology. The paper specifically explores the fine-scale microstructures of highly porous sintered attachments under power cycling to provide a deeper understanding of the significance of porosity as a reliability-related microstructural parameter. Attachments prepared at 220°C using a pressure of 6 MPa for 1 s (parameters known to generate approximately 50% porosity from previous work) and subsequently subjected to 650,000 power cycles between 50°C and 200°C are assessed. A correlative workflow integrating x-ray computed tomography, focused ion beam (FIB) and electron backscatter diffraction (EBSD) data is applied to merge meso- and nanoscale microstructural features to illuminate the degradation mechanisms. The as-sintered Ag layer has a high volume of heterogeneously distributed pores, and consists of randomly oriented equiaxed grains whose sizes vary depending on the local density of the region sampled. Power cycling promotes grain growth and the loss of twin boundaries, and these changes are more pronounced within more dense regions of the Ag attachment. In contrast, the copper substrate appears to undergo some grain refinement, with deformation twins visible within finer-grained zones during power cycling. Cracks, which appear to start off within the Ag layer, propagate across the Ag-Cu boundary and transgranularly through fine-grained regions within the copper with little tortuosity. These observations are discussed within the context of reliability behaviour. Graphical Abstract
- 6 October 2021
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Device and Materials Reliability
- Vol. 21 (4) , 536-543
Reliability and Characterization of Nanosilver Joints Prepared by a Time-Reduced Sintering Process
This study investigates the power cycling reliability of nanosilver sintered joints formed by a time-reduced sintering process, designed for use on a die bonder. A range of sintering parameters, reflecting different levels of manufacturability, were used to produce sintered joints in respect of shear strength and porosity, within a process cycle time of a few seconds. The reliability of the sintered attachments were evaluated against Pb5Sn solder joints under constant temperature swing power cycling conditions over the range 50 to 200 °C. The thermal performance and microstructural changes of the sintered joints were monitored and evaluated non-destructively at regular intervals using transient thermal impedance and X-ray computed tomography. The results show that sintered joints with higher shear strengths (>50 MPa) and lower porosities (<25 %) tend to maintain their thermal performance up to ~100k power cycles before gradual degradation occurs. Sintered joints with intermediate shear strengths (20 to 40 MPa) and with corresponding analogous porosities (35 to 51 %) also demonstrated comparable power cycling behavior; exhibiting a progressive decrease in effective thermal conductivity with increasing cycles. The evaluated lifetime of sintered joints with the highest shear strengths were found to be at least double those for the lower shear strength joints, and up to fourteen times those of a Pb5Sn solder die attachment. Even the most porous sintered joints exhibited lifetimes appreciably longer than a Pb5Sn die attachment. Degradation in thermal resistance was seen to correlate with observed microstructural changes, with a dependence on initial sintering parameters.
- 6 October 2021
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Device and Materials Reliability
- Vol. 21 (4) , 536-543
Reliability and Characterization of Nanosilver Joints Prepared by a Time-Reduced Sintering Process
This study investigates the power cycling reliability of nanosilver sintered joints formed by a time-reduced sintering process, designed for use on a die bonder. A range of sintering parameters, reflecting different levels of manufacturability, were used to produce sintered joints in respect of shear strength and porosity, within a process cycle time of a few seconds. The reliability of the sintered attachments were evaluated against Pb5Sn solder joints under constant temperature swing power cycling conditions over the range 50 to 200 °C. The thermal performance and microstructural changes of the sintered joints were monitored and evaluated non-destructively at regular intervals using transient thermal impedance and X-ray computed tomography. The results show that sintered joints with higher shear strengths (>50 MPa) and lower porosities (<25 %) tend to maintain their thermal performance up to ~100k power cycles before gradual degradation occurs. Sintered joints with intermediate shear strengths (20 to 40 MPa) and with corresponding analogous porosities (35 to 51 %) also demonstrated comparable power cycling behavior; exhibiting a progressive decrease in effective thermal conductivity with increasing cycles. The evaluated lifetime of sintered joints with the highest shear strengths were found to be at least double those for the lower shear strength joints, and up to fourteen times those of a Pb5Sn solder die attachment. Even the most porous sintered joints exhibited lifetimes appreciably longer than a Pb5Sn die attachment. Degradation in thermal resistance was seen to correlate with observed microstructural changes, with a dependence on initial sintering parameters.
- Open Access
- 9 May 2019
- Published by Wiley in Journal of Microscopy
- Vol. 277 (3) , 140-153
Three‐dimensional damage morphologies of thermomechanically deformed sintered nanosilver die attachments for power electronics modules
Summary: A time‐lapse study of thermomechanical fatigue damage has been undertaken using three‐dimensional X‐ray computer tomography. Morphologies were extracted from tomography data and integrated with data from microscopy modalities at different resolution levels. This enables contextualization of some of the fine‐scale properties which underpin the large‐scale damage observed via tomography. Lateral views of crack development are presented, which show networks analogous to mud‐cracks. Crack fronts which develop in the most porous regions within the sintered attachment layer travel across the boundary into the copper substrate. The propagation characteristics of these cracks within the substrate are analysed. Evidence is provided of heterogeneous densification within the sintered joint under power cycling, and this is shown to play a major role in driving the initiation and propagation of the cracks. Examination of the texture (differing levels of X‐ray absorption) of virtual cross‐sectional images reveals the origins of the nonuniformity of densification. Finally, cracks within the sintered joint are shown to have a negligible impact on the conduction pathway of the joint due to their aspect ratio and orientation with respect to the assembly.Lay Description: This paper concerns the use of three‐dimensional (3D) X‐ray tomography, a nondestructive technique, to perform cradle‐to‐grave studies of sintered nanosilver die‐attachments under operation. Sintered nanosilver die‐attachments have been proposed as a more reliable and environmentally friendly alternative to solder alloy joints for emerging power electronics module designs. However, their degradation mechanisms are not as well understood. This same sample‐study is about observing how the fine‐scale structure of a sintered attachment evolves and degrades over time. Using 3D tomography affords otherwise infeasible perspectives, such as virtual cross‐sections in the lateral plane of the attachment. These perspectives provide qualitative information which elucidates the degradation mechanisms. They demonstrate, for example, that the structure of the sintered attachment densifies under operation, and a consequence of this is the formation of shrinkage cracks in the most porous regions, much like mud‐cracks. Other imaging techniques (metallographic etching and scanning electron microscopy) have been used in correlation with 3D renderings of these cracks to analyse their propagation and reveal their relationship both with the internal structure of the sintered attachment itself, and the structure of the substrate to which it is joined. It is shown that the cracks develop within the sintered attachment layer and eventually cross over into the substrate. A comparison of two sintered attachments with contrasting bulk porosities allows the effect of initial bond quality on crack development to be examined.
- 9 May 2019
- Published by Wiley in Journal of Microscopy
- Vol. 277 (3) , 140-153
Open AccessThree‐dimensional damage morphologies of thermomechanically deformed sintered nanosilver die attachments for power electronics modules
Summary: A time‐lapse study of thermomechanical fatigue damage has been undertaken using three‐dimensional X‐ray computer tomography. Morphologies were extracted from tomography data and integrated with data from microscopy modalities at different resolution levels. This enables contextualization of some of the fine‐scale properties which underpin the large‐scale damage observed via tomography. Lateral views of crack development are presented, which show networks analogous to mud‐cracks. Crack fronts which develop in the most porous regions within the sintered attachment layer travel across the boundary into the copper substrate. The propagation characteristics of these cracks within the substrate are analysed. Evidence is provided of heterogeneous densification within the sintered joint under power cycling, and this is shown to play a major role in driving the initiation and propagation of the cracks. Examination of the texture (differing levels of X‐ray absorption) of virtual cross‐sectional images reveals the origins of the nonuniformity of densification. Finally, cracks within the sintered joint are shown to have a negligible impact on the conduction pathway of the joint due to their aspect ratio and orientation with respect to the assembly.Lay Description: This paper concerns the use of three‐dimensional (3D) X‐ray tomography, a nondestructive technique, to perform cradle‐to‐grave studies of sintered nanosilver die‐attachments under operation. Sintered nanosilver die‐attachments have been proposed as a more reliable and environmentally friendly alternative to solder alloy joints for emerging power electronics module designs. However, their degradation mechanisms are not as well understood. This same sample‐study is about observing how the fine‐scale structure of a sintered attachment evolves and degrades over time. Using 3D tomography affords otherwise infeasible perspectives, such as virtual cross‐sections in the lateral plane of the attachment. These perspectives provide qualitative information which elucidates the degradation mechanisms. They demonstrate, for example, that the structure of the sintered attachment densifies under operation, and a consequence of this is the formation of shrinkage cracks in the most porous regions, much like mud‐cracks. Other imaging techniques (metallographic etching and scanning electron microscopy) have been used in correlation with 3D renderings of these cracks to analyse their propagation and reveal their relationship both with the internal structure of the sintered attachment itself, and the structure of the substrate to which it is joined. It is shown that the cracks develop within the sintered attachment layer and eventually cross over into the substrate. A comparison of two sintered attachments with contrasting bulk porosities allows the effect of initial bond quality on crack development to be examined.
- Open Access
- 20 April 2016
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 45 (7) , 3659-3672
Damage Evolution in Al Wire Bonds Subjected to a Junction Temperature Fluctuation of 30 K
- 20 April 2016
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 45 (7) , 3659-3672
Open AccessDamage Evolution in Al Wire Bonds Subjected to a Junction Temperature Fluctuation of 30 K
- Open Access
- 30 September 2013
- Published by Elsevier in Intermetallics
- Vol. 40, 50-59
A numerical method to determine interdiffusion coefficients of Cu6Sn5 and Cu3Sn intermetallic compounds
- 30 September 2013
- Published by Elsevier in Intermetallics
- Vol. 40, 50-59
Open AccessA numerical method to determine interdiffusion coefficients of Cu6Sn5 and Cu3Sn intermetallic compounds
- 5 January 2013
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 42 (3) , 537-544
Room-Temperature Nanoindentation Creep of Thermally Cycled Ultrasonically Bonded Heavy Aluminum Wires
- 5 January 2013
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 42 (3) , 537-544
Room-Temperature Nanoindentation Creep of Thermally Cycled Ultrasonically Bonded Heavy Aluminum Wires
- 19 September 2010
- Published by Elsevier in Microelectronics Reliability
- Vol. 51 (2) , 406-415
Microstructural evolution of ultrasonically bonded high purity Al wire during extended range thermal cycling
- 19 September 2010
- Published by Elsevier in Microelectronics Reliability
- Vol. 51 (2) , 406-415
Microstructural evolution of ultrasonically bonded high purity Al wire during extended range thermal cycling