Are Metal-Free Monolithic Crowns the Present of Prosthesis? Study of Mechanical Behaviour
Open Access
Abstract
Purpose: To analyze in vitro the mechanical behavior of five types of complete coverage crowns fabricated from different materials. Materials and methods: Seventy-five full coverage crowns were divided into five groups according to material: Group I, metal core with feldspathic ceramic covering (MC- control group); Group II, zirconia core with feldspathic ceramic covering (CZ); Group III, tetragonal monolithic zirconia (TMZ); Group IV, cubic monolithic zirconia (CMZ); Group V, high molecular weight polymethyl methacrylate (PMMAG) doped with graphene nanoparticles. All crowns underwent in vitro fatiguing by dynamic loading in wet conditions to simulate the masticatory forces to which prosthodontic materials are subject in the oral medium. Lastly, fracture resistance was evaluated by static compression testing. Results: The fracture resistance values obtained were as follows: Group MC, 2443.6 ± 238.6 N; Group CZ, 2095.4 ± 329.2 N; Group TMZ, 2494.6 ± 236.6 N; Group CMZ, 1523.6 ± 325.2 N; and Group PMMAG, 1708.9 ± 386.6 N. Group MC presented higher strength with statistically significant differences in comparison with Groups CZ (P = 0.002), CMZ (P < 0.001), and PMMAG (P < 0.001). Weibull distribution showed less probability of cumulative biomechanical failure in Groups MC and TMZ. Conclusions: Metal-ceramic and tetragonal zirconia showed high fracture resistance, while cubic zirconia and PMMA doped with graphene nanoparticles obtained lower values.Keywords
This publication has 23 references indexed in Scilit:
- Optical properties and light irradiance of monolithic zirconia at variable thicknessesDental Materials, 2015
- Load-bearing capacity and the recommended thickness of dental monolithic zirconia single crownsJournal of the Mechanical Behavior of Biomedical Materials, 2014
- Range of indications for translucent zirconia modifications: Clinical and technical aspects2013
- Zirconia versus metal: a preliminary comparative analysis of ceramic veneer behavior.2012
- A practical and systematic review of Weibull statistics for reporting strengths of dental materialsDental Materials, 2010
- Fatigue and fracture properties of yttria partially stabilized zirconia crown systemsDental Materials, 2008
- A systematic review of the survival and complication rates of all‐ceramic and metal–ceramic reconstructions after an observation period of at least 3 years. Part II: fixed dental prostheses.Clinical Oral Implants Research, 2007
- Thin‐wall ceramic CAD/CAM crown copings: strength and fracture patternJournal of Oral Rehabilitation, 2006
- Preparation design and margin distortion in porcelain-fused-to-metal restorationsThe Journal of Prosthetic Dentistry, 2003
- Functional occlusal forces: An investigation by telemetryThe Journal of Prosthetic Dentistry, 1978