Conversion of Li3PO4 Derived from LiFePO4 Cathode Manufacturing Byproducts to Li2CO3 via CaCO3-Assisted CO2 Thermal Treatment
Open Access
Abstract
A sequential lithium-recovery process combining hydrogen reduction, water leaching, CaCO3-assisted thermal conversion under a CO2 atmosphere, and a second water-leaching step was investigated using an LFP cathode manufacturing byproduct as the starting material. Hydrogen reduction was first employed to decompose LiFePO4 and redistribute lithium into a Li3PO4-containing phase while Fe and P were predominantly incorporated into Fe-rich phosphide phases. Among the investigated conditions, treatment at 900 °C for 3 h resulted in the disappearance of detectable LiFePO4 peaks and the formation of Li3PO4 and Fe2P as the predominant crystalline phases. The reduced product was subsequently subjected to water leaching, and a solid-to-liquid ratio of 1:100 with a leaching time of 5 h yielded a Li3PO4-rich intermediate with a lithium recovery of 45.06% and a Li content of 17.43 wt.%. The recovered intermediate was then mixed with CaCO3 and thermally treated under a CO2 atmosphere to convert lithium phosphate into lithium carbonate while phosphorus was transferred into a Ca–P-rich phase. The most favorable phase-conversion behavior was obtained at 900 °C using a Li3PO4-to-CaCO3 weight ratio of 1:1 and a holding time of 2 h, where Li2CO3 and Ca2P2O7 were identified as the predominant crystalline products. Subsequent water leaching separated the Li-containing carbonate fraction from the water-insoluble Ca2P2O7-rich residue. A maximum lithium recovery of 93.59% was obtained at a solid-to-liquid ratio of 1:50 in the solid-to-liquid-ratio experiments, while the leaching-time experiments showed a lithium recovery of 92.54% after 5 h under the same solid-to-liquid ratio. XRD analysis of the final recovered product identified Li2CO3 as the predominant crystalline phase. Based on the selected conditions for Stage I and Stage II, the cumulative lithium recovery from the initial LFP feed to the final Li2CO3-rich product was approximately 41.70%, indicating that the first water-leaching and Li3PO4-intermediate recovery step was the principal limitation of the overall process. These results demonstrate the feasibility of recovering lithium from LFP cathode manufacturing byproducts through controlled phase conversion and water-based separation, while also highlighting the need to improve Stage I lithium recovery and to consider the thermal-energy demand associated with solution concentration and drying during future process development.Keywords
Funding Information
- Ministry of Trade, Industry and Energy (MOTIE), Republic of Korea (20024238)
This publication has 24 references indexed in Scilit:
- Selective recovery of lithium from spent LFP batteries via low temperature sodium salt roastingHydrometallurgy, 2026
- Recycling of spent lithium iron phosphate battery cathode materials: A reviewJournal of Cleaner Production, 2024
- Unlocking the value of recycling scrap from Li-ion battery manufacturing: Challenges and outlookJournal of Power Sources, 2023
- Advances and perspectives towards spent LiFePO4 battery recyclingJournal of Cleaner Production, 2023
- Phosphorus recovery from wastewater via calcium phosphate precipitation: A critical review of methods, progress, and insightsChemosphere, 2023
- Recovery of LiFePO4 from used lithium-ion batteries by sodium-bisulphate-assisted roastingJournal of Cleaner Production, 2022
- NaOH-assisted low-temperature roasting to recover spent LiFePO4 batteriesWaste Management, 2022
- A sodium salt-assisted roasting approach followed by leaching for recovering spent LiFePO4 batteriesJournal of Hazardous Materials, 2022
- A novel process to recycle spent LiFePO4 for synthesizing LiFePO4/C hierarchical microflowersElectrochimica Acta, 2016
- Bioactive calcium pyrophosphate glasses and glass-ceramicsActa Biomaterialia, 2005