KJKim Hyun Jong

Kim Hyun Jong

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Kim Hyun Jong has a total of 3 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Conversion of Li3PO4 Derived from LiFePO4 Cathode Manufacturing Byproducts to Li2CO3 via CaCO3-Assisted CO2 Thermal Treatment

    by Do-Hee Kim, Jei-Pil Wang

    A sequential lithium-recovery process combining hydrogen reduction, water leaching, CaCO3-assisted thermal conversion under a CO2 atmosphere, and a second water-leaching step was investigated using an LFP cathode manufacturing byproduct as the starting material. Hydrogen reduction was first employed to decompose LiFePO4 and redistribute lithium into a Li3PO4-containing phase while Fe and P were predominantly incorporated into Fe-rich phosphide phases. Among the investigated conditions, treatment at 900 °C for 3 h resulted in the disappearance of detectable LiFePO4 peaks and the formation of Li3PO4 and Fe2P as the predominant crystalline phases. The reduced product was subsequently subjected to water leaching, and a solid-to-liquid ratio of 1:100 with a leaching time of 5 h yielded a Li3PO4-rich intermediate with a lithium recovery of 45.06% and a Li content of 17.43 wt.%. The recovered intermediate was then mixed with CaCO3 and thermally treated under a CO2 atmosphere to convert lithium phosphate into lithium carbonate while phosphorus was transferred into a Ca–P-rich phase. The most favorable phase-conversion behavior was obtained at 900 °C using a Li3PO4-to-CaCO3 weight ratio of 1:1 and a holding time of 2 h, where Li2CO3 and Ca2P2O7 were identified as the predominant crystalline products. Subsequent water leaching separated the Li-containing carbonate fraction from the water-insoluble Ca2P2O7-rich residue. A maximum lithium recovery of 93.59% was obtained at a solid-to-liquid ratio of 1:50 in the solid-to-liquid-ratio experiments, while the leaching-time experiments showed a lithium recovery of 92.54% after 5 h under the same solid-to-liquid ratio. XRD analysis of the final recovered product identified Li2CO3 as the predominant crystalline phase. Based on the selected conditions for Stage I and Stage II, the cumulative lithium recovery from the initial LFP feed to the final Li2CO3-rich product was approximately 41.70%, indicating that the first water-leaching and Li3PO4-intermediate recovery step was the principal limitation of the overall process. These results demonstrate the feasibility of recovering lithium from LFP cathode manufacturing byproducts through controlled phase conversion and water-based separation, while also highlighting the need to improve Stage I lithium recovery and to consider the thermal-energy demand associated with solution concentration and drying during future process development.

  • Open Access

    Waste Aluminum Dust-Derived Functional Zeolites for Heavy Metal Removal and Water Softening: Synthesis, Purification, and Ion-Exchange Modification

    by Min-Seo Choi, Jeong-Sik Moon, Jei-Pil Wang

    Waste aluminum dust generated from aluminum refining and machining processes contains high fractions of Al2O3 and SiO2, making it a potential secondary aluminosilicate resource for zeolite synthesis. In this study, waste aluminum dust was converted into functional zeolite materials through dry fusion purification, NaOH-assisted hydrothermal synthesis, acid purification, Si/Al ratio control, and cation-exchange modification. The raw dust was subjected to dry fusion at 1600 °C under an Ar atmosphere to remove metallic impurities and obtain an aluminosilicate precursor. Na-type zeolite was then synthesized using 50 wt.% NaOH solution at 90 °C for 24 h. The as-synthesized Na-type zeolite exhibited an estimated chemical purity of 97.501 wt.% based on measured residual impurities, with Mg, Ca, K, and Ti remaining as major impurities. HCl leaching at 0.25 M for 24 h increased the estimated chemical purity based on measured residual impurities to 98.469 wt.% while retaining the major zeolitic diffraction features. The Si/Al ratio was further controlled using water glass, and the maximum Si/Al ratio of 1.77 was obtained at a Na-type zeolite-to-water-glass mass ratio of 1:2 after reaction at 90 °C for 6 h. The purified and composition-controlled zeolite was subsequently modified with Mg2+ and K+ ions to prepare Mg-modified and K-modified zeolites. Under fixed batch conditions using a relatively high zeolite dosage and a single initial concentration, Mg-modified zeolite reduced Pb, Hg, Cr(VI), and Cd concentrations from 100 ppm to 0.004, 0.00059, 0.018, and 0.004 ppm, respectively, while K-modified zeolite reduced the total hardness of synthetic hard water from 308.3 to 40.13 ppm as CaCO3. These results should be interpreted as preliminary batch-performance results under the tested conditions rather than as maximum adsorption capacities or a complete adsorption-mechanism evaluation. Overall, this study demonstrates the feasibility of valorizing waste aluminum dust into purified and cation-modified zeolite materials for potential water-treatment applications. Further adsorption isotherm, kinetic, dosage-dependent, BET surface area, pore-volume, pore-size distribution, and quantitative phase analyses are required to evaluate adsorption capacity, adsorption mechanism, true zeolite phase purity, and framework–performance relationships.

  • Open Access

    Carbothermic Reduction and Sulfidation Behavior for Fe–Ni–S Matte Production from Synthetic Saprolitic Nickel Ore

    by Chang Ho Jung, Jei-Pil Wang

    This study investigates the production behavior of Fe–Ni–S matte from synthetic nickel ore designed to simulate low-grade saprolitic laterite. The synthetic feed was formulated based on XRF and XRD analyses of magnetically upgraded laterite concentrate. Thermodynamic modeling, including phase stability analysis, Ellingham evaluation, viscosity prediction, and sulfidation equilibria, was employed to define optimal smelting conditions. Carbothermic reduction at 1550 °C enabled selective reduction in NiO and FeO, leading to the formation of Fe–Ni alloy droplets, which subsequently reacted with FeS to produce Fe–Ni–S matte. The carbon ratio played a critical role in controlling FeO content in slag, thereby influencing slag basicity and viscosity. An optimal carbon ratio of 0.2–0.4 mol maintained slag viscosity within the industrially favorable range (2–5 poise) and minimized crucible dissolution. Thermodynamic analysis confirmed that FeS is the only stable sulfide phase at high temperature and dissolves into the Fe–Ni melt, promoting stable matte formation. Under optimized carbon and FeS addition conditions, a maximum nickel recovery of approximately 88% was achieved, attributed to improved slag composition, controlled viscosity, and enhanced matte–slag separation. These results demonstrate that simultaneous carbothermic reduction and sulfidation is an effective route for Fe–Ni–S matte production from saprolite-derived oxide feed. Control of carbon ratio, FeS addition, and Al2O3 flux is essential for achieving stable matte formation and efficient metal–slag separation.

  • Open Access

    Preparation and Recovery Behavior of Lithium Chloride (LiCl) from Lithium Iron Phosphate (LiFePO4) Cathode Active Materials via Hydrogen Reduction and CaCl2-Assisted Thermal Chlorination

    by Tae-Jun Jeon, Jei-Pil Wang

    In this study, lithium was recovered from LiFePO4 (LFP) cathode active materials through a two-step thermal process combining hydrogen reduction and chlorination roasting. Hydrogen reduction was conducted while varying temperature and holding time to promote oxygen removal from LFP and induce phase separation into Li3PO4 and iron phosphides (FeP and Fe2P). Based on stoichiometric assessment using the degree of LFP decomposition and the reduction in oxygen moles, the optimal hydrogen-reduction condition was determined to be 900 °C for 1 h. Subsequently, CaCl2 was selected as an appropriate chlorination agent using thermodynamic considerations, and the hydrogen-reduced product was reacted with CaCl2 to convert Li3PO4 into water-soluble LiCl. The mass of LiCl produced was quantified as a function of reaction temperature. Water leaching enabled the separation of LiCl from the insoluble residues, resulting in an overall lithium recovery of 71.7%.


  • Open Access

    A Study on the Recovery of Valuable Metals from Solar Cells Using Acid Leaching and Substitution Reactions

    by Kim Hyun Jong, Erdenebold Urtnasan, Jei-Pil Wang

    This study was conducted to recover valuable metals (silicon and silver) using acid leaching and substitution reactions with copper powder from the pulverized solar cell separated from the PV ribbon. Leaching experiments were conducted according to nitric acid concentration by molar solution as 1M, 2M, and 3M using an ultrasonic cleaner at a reaction temperature of 60 °C for the leaching times of 30 to 120 minutes. Si phases were detected at all leaching reaction times, it was confirmed that the aluminium was removed effectively if the nitric acid leaching time was more than 30 minutes, and silicon with a purity above 99% could be recovered. The silver was precipitated by adding copper, which has greater reducibility than Cu, Al, Si, Pb, and Sn. When the addition of copper powder was 0.75 and 1.0 g, precipitate was produced 0.23 and 0.55 g, respectively. The optimal condition for the recovery of silver by the addition of copper powder was 1 g, where is recovery rate reached 93.3%.