Abstract
The exceptional stiffness of diamond is strongly anisotropic due to its crystal structure, yet experimental quantification of Young's modulus along different orientations remains limited. Here, we present a direct measurement of elastic anisotropy in microwave plasma chemical vapor deposition (MPCVD) single-crystal diamond (SCD) by analyzing the resonance frequencies of cantilevers aligned along distinct crystallographic directions. The measured Young's modulus exhibited a minimum value of 1085 ± 21 GPa along the ⟨100⟩ direction and a maximum value of 1189 ± 22 GPa along the ⟨110⟩ direction. The compliance constants derived from the MPCVD-SCD differ substantially from previously reported values for natural diamonds and are more consistent with first-principles theoretical values. This method enables precise determination of orientation-dependent stiffness, revealing significant variation in Young's modulus across crystallographic axes. These insights are critical for the design of diamond-based micro- and nano-mechanical systems as well as other high-precision devices, where directional elasticity strongly influences performance.
Funding Information
  • Japan Society for the Promotion of Science (24H00287)
  • Japan Society for the Promotion of Science (JPMXP1225NM5307)
  • Councile for Science, Technology and Innovation (SIP)

This publication has 38 references indexed in Scilit: