Effects of Six Surface Treatment Methods on the Surface Roughness of a Low‐Fusing and an Ultra Low‐Fusing Feldspathic Ceramic Material
- 6 April 2009
- journal article
- Published by Wiley in Journal of Prosthodontics
- Vol. 18 (3) , 217-222
Abstract
Purpose: The purpose of this in vitro study was to determine the effects of six surface treatment methods on the surface roughness of two feldspathic ceramic materials. Materials and Methods: One hundred twenty metal discs were cast (Remanium CS). A low‐fusing feldspathic ceramic (Vita Omega 900) was fired onto 60 metal discs, and an ultra low‐fusing feldspathic ceramic (Finesse) was fired onto the other 60 metal discs. Six surface treatment methods were selected: (1) autoglazing (AUG), (2) overglazing (OVG), (3) polishing (POL), (4) fine diamond disc grinding + polishing + autoglazing (FDPA), (5) coarse diamond disc grinding + polishing + autoglazing (CDPA), (6) polishing + autoglazing (PA). Omega specimens were assigned to six experimental groups representing six surface treatment methods (Om‐AUG, Om‐OVG, Om‐POL, Om‐FDPA, Om‐CDPA, Om‐PA) (n = 10). Finesse specimens were also assigned to six experimental groups (Fn‐AUG, Fn‐OVG, Fn‐POL, Fn‐FDPA, Fn‐CDPA, Fn‐PA) (n = 10). Treated ceramic surfaces were examined by means of profilometry and transmission electron microscopy. Results: In Omega groups mean roughness values ranged as follows: group Om‐AUG = Om‐POL > Om‐OVG > Om‐CDPA = Om‐FDPA > Om‐PA (p < 0.001). No significant difference was found between groups Om‐AUG/Om‐POL and Om‐CDPA/Om‐FDPA (p > 0.05). In Finesse groups mean roughness values ranged as follows: Fn‐CDPA > Fn‐FDPA = Fn‐AUG = Fn‐POL = Fn‐OVG > Fn‐PA (p < 0.001). No significant difference was found between Fn‐FDPA, Fn‐AUG, Fn‐ POL and Fn‐OVG (p > 0.05). Conclusions: For both ceramic types, the smoothest surfaces were obtained with polishing prior to autoglazing. Diamond disc grinding prior to polishing and autoglazing (Fn‐FDPA, Fn‐CDPA) displayed the roughest surfaces in ultra low‐fusing ceramic (Finesse). Autoglazing alone and polishing displayed the roughest surfaces in low‐fusing ceramic material (Om‐AUG, Om‐POL).Keywords
This publication has 23 references indexed in Scilit:
- Effect of various treatment and glazing (coating) techniques on the roughness and wettability of ceramic dental restorative surfacesColloids and Surfaces B: Biointerfaces, 2006
- Factors affecting enamel and ceramic wear: A literature reviewThe Journal of Prosthetic Dentistry, 2002
- The effect of acquired salivary pellicle on the surface free energy and wettability of different denture base materialsJournal of Dentistry, 2001
- Wear of low-fusing dental porcelainsThe Journal of Prosthetic Dentistry, 1999
- In vitro investigation of the wear of human enamel by dental porcelainThe Journal of Prosthetic Dentistry, 1999
- Comparison of surface roughness of oral hard materials to the threshold surface roughness for bacterial plaque retention: A review of the literatureDental Materials, 1997
- The influence of surface roughness and surface‐free energy on supra‐ and subgingival plaque formation in manJournal of Clinical Periodontology, 1995
- Abrasion of Human Enamel by Different Dental Ceramics in vitroJournal of Dental Research, 1991
- The influence of surface free energy and surface roughness on early plaque formationJournal of Clinical Periodontology, 1990
- Porcelain surface texture after reduction and natural glazingThe Journal of Prosthetic Dentistry, 1986