Study on the structure, morphology, and properties of end‐functionalized star‐shaped solution‐polymerized styrene–butadiene rubber
- 25 September 2012
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 128 (4) , 2516-2524
Abstract
Three kinds of star‐shaped solution‐polymerized styrene–butadiene rubber (S‐SSBR) were synthesized by living anionic polymerization using a self‐made multifunctional organic lithium initiator. One was S‐SSBR with 100% coupling degree. Others were the functionalized S‐SSBR which had macromolecular chain‐free ends terminated directly (ES‐SSBR‐1), and macromolecular chain terminated after dissociation in the polymerization solution (ES‐SSBR‐2) by 3‐chloropropyl trimethoxy siloxane. The molecular structure parameters of three kinds of SSBR were determined and the end‐functionalized efficiency was calculated. The rheological properties, mechanical properties, and dynamic mechanical properties of ES‐SSBR and S‐SSBR composites filled with silica (SiO2)–carbon black (CB) were investigated. The morphology was observed by transmission electron microscopy and high‐resolution transmission electron microscopy, and the dispersion of the two kinds of filler in the composites was distinguished by X‐ray energy spectrometry. The results showed that the mixing speed of hydrophilic SiO2 powder in the ES‐SSBR was higher than that in the S‐SSBR. SiO2‐CB/ES‐SSBR composites presented excellent mechanical properties, high wet‐skid resistance, and low rolling resistance. Two kinds of nanofiller in the ES‐SSBR exhibited outstanding doping nanometer dispersion and good distribution, which indicated that after being coupled and end‐functionalized, the two free ends of the macromolecular chains formed chemical bonding with the surface chemical groups of CB and SiO2, respectively. Accordingly, ES‐SSBR was a remarkable energy‐saving elastomer. © 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013Keywords
This publication has 10 references indexed in Scilit:
- Study on the structure and properties of SSBR with large-volume functional groups at the end of chainsPolymer, 2010
- Tin‐coupled star‐shaped block copolymer of styrene and butadiene (I) synthesis and characterizationJournal of Applied Polymer Science, 2008
- Effects of coagulation processes on properties of epoxidized natural rubberJournal of Applied Polymer Science, 2008
- The influence of surface modification on the structure and properties of a nanosilica filled thermoplastic elastomerComposites Science and Technology, 2007
- Effects of Time and Temperature on the Reaction of Tespt Silane Coupling Agent During Mixing with Silica Filler and Tire RubberRubber Chemistry and Technology, 2002
- Effect of Polymer-Filler and Filler-Filler Interactions on Dynamic Properties of Filled VulcanizatesRubber Chemistry and Technology, 1998
- Viscoelastic Properties of Elastomers and Tire Wet Skid ResistanceRubber Chemistry and Technology, 1997
- Low Strain Dynamic Properties of Filled RubbersRubber Chemistry and Technology, 1971
- Stress softening in natural rubber vulcanizates. Part II. Stress softening effects in pure gum and filler loaded rubbersJournal of Applied Polymer Science, 1965
- The dynamic properties of carbon black‐loaded natural rubber vulcanizates. Part IJournal of Applied Polymer Science, 1962