Suhe Zhao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Suhe Zhao has a total of 49 co-authors. Here are the top co-authors by number of shared publications:
Xingying Zhang
Key Laboratory of Beijing City on Preparation and Processing of Novel Polymer Materials, Beijing 100029, P. R. China
6 shared publications- Xiao Liu
College of Materials Science and Engineering State Key Laboratory of Materials Low‐Carbon Recycling Beijing University of Technology Beijing China
4 shared publications Yaqin Wang
Beijing University of Chemical Technology
4 shared publicationsLiqun Zhang
State Key Laboratory of Organic–Inorganic Composites
3 shared publications- Liqun Zhang
South China University of Technology
3 shared publications Youping Wu
Key Laboratory of Beijing City on the Preparation and Processing of Novel Polymer Materials Beijing University of Chemical Technology Beijing 100029 China
3 shared publications
Latest Publications
- Open Access
Structure and Dielectric Properties of TPU Composite Filled with CNTs@PDA Nanofibers and MXene Nanosheets
Thermoplastic polyurethane (TPU) is a kind of dielectric elastomer (DE) which can behave as an actuator, altering thickness strain in response to electrical stimulation. The composites are made up of fillers with a very high dielectric constant that are spread in a polymer matrix. It is very difficult to obtain large deformation at low voltage. In this study, we made two-dimensional (2D) MXene nanosheets with excellent conductivity and one-dimensional (1D) polydopamine (PDA)-modified CNT fiber fillers. After that, TPU dielectric elastomer films made of MXene/CNTs or MXene/CNTs@PDA were prepared. The results showed that the dielectric constant and dielectric loss of TPU dielectric film including MXene/CNTs were much higher than that containing MXene/CNTs@PDA, although Young’s modulus and breakdown strength (Eb) were significantly lower. At the same time, these two types of dielectric films had a significantly higher dielectric constant and dielectric loss than pure TPU dielectric film, and their breakdown strength was significantly lower. The compatibility of CNTs@PDA fibers with the TPU matrix improves after PDA modification, and the dispersion of CNTs@PDA fibers improves, resulting in an increase in Young’s modulus. MXene with a two-dimensional nanosheet structure increases the breakdown strength of the TPU dielectric elastomer under the condition of the addition of a tiny quantity. To summarize, the dielectric constant, dielectric loss, Young’s modulus, and dielectric elastomer breakdown strength are mutually restrictive conditions, and the relationship between all parties must be balanced to obtain obvious deformation properties.
Open AccessStructure and Dielectric Properties of TPU Composite Filled with CNTs@PDA Nanofibers and MXene Nanosheets
Thermoplastic polyurethane (TPU) is a kind of dielectric elastomer (DE) which can behave as an actuator, altering thickness strain in response to electrical stimulation. The composites are made up of fillers with a very high dielectric constant that are spread in a polymer matrix. It is very difficult to obtain large deformation at low voltage. In this study, we made two-dimensional (2D) MXene nanosheets with excellent conductivity and one-dimensional (1D) polydopamine (PDA)-modified CNT fiber fillers. After that, TPU dielectric elastomer films made of MXene/CNTs or MXene/CNTs@PDA were prepared. The results showed that the dielectric constant and dielectric loss of TPU dielectric film including MXene/CNTs were much higher than that containing MXene/CNTs@PDA, although Young’s modulus and breakdown strength (Eb) were significantly lower. At the same time, these two types of dielectric films had a significantly higher dielectric constant and dielectric loss than pure TPU dielectric film, and their breakdown strength was significantly lower. The compatibility of CNTs@PDA fibers with the TPU matrix improves after PDA modification, and the dispersion of CNTs@PDA fibers improves, resulting in an increase in Young’s modulus. MXene with a two-dimensional nanosheet structure increases the breakdown strength of the TPU dielectric elastomer under the condition of the addition of a tiny quantity. To summarize, the dielectric constant, dielectric loss, Young’s modulus, and dielectric elastomer breakdown strength are mutually restrictive conditions, and the relationship between all parties must be balanced to obtain obvious deformation properties.
- Open Access
Silica Modified by Alcohol Polyoxyethylene Ether and Silane Coupling Agent Together to Achieve High Performance Rubber Composites Using the Latex Compounding Method
The study of preparing silica/rubber composites used in tires with low rolling resistance in an energy-saving method is fast-growing. In this study, a novel strategy is proposed, in which silica was modified by combing alcohol polyoxyethylene ether (AEO) and 3-mercaptopropyltriethoxysilane (K-MEPTS) for preparing silica/natural rubber (NR) master batches. A thermal gravimetric analyzer and Raman spectroscopy results indicated that both AEO and K-MEPTS could be grafted on to the silica surface, and AEO has a chance to shield the mercaptopropyl group on K-MEPTS. Silica modified by AEO and K-MEPTS together was completely co-coagulated with the rubber in preparing silica/NR composites using the latex compounding method with the help of the interaction between AEO and K-MEPTS. The performance of composites prepared by silica/NR master batches was investigated by a rubber process analyzer (RPA), transmission electron microscopy (TEM) and a tensile tester. These results demonstrate that AEO forms a physical interface between silica and rubber, resulting in good silica dispersion in the matrix. K-MEPTS forms a chemical interface between silica and rubber, enhancing the reinforcing effect of silica and reducing the mutual friction between silica particles. In summary, using a proper combination of AEO and K-MEPTS is a user-friendly approach for preparing silica/NR composites with excellent performance.
Open AccessSilica Modified by Alcohol Polyoxyethylene Ether and Silane Coupling Agent Together to Achieve High Performance Rubber Composites Using the Latex Compounding Method
The study of preparing silica/rubber composites used in tires with low rolling resistance in an energy-saving method is fast-growing. In this study, a novel strategy is proposed, in which silica was modified by combing alcohol polyoxyethylene ether (AEO) and 3-mercaptopropyltriethoxysilane (K-MEPTS) for preparing silica/natural rubber (NR) master batches. A thermal gravimetric analyzer and Raman spectroscopy results indicated that both AEO and K-MEPTS could be grafted on to the silica surface, and AEO has a chance to shield the mercaptopropyl group on K-MEPTS. Silica modified by AEO and K-MEPTS together was completely co-coagulated with the rubber in preparing silica/NR composites using the latex compounding method with the help of the interaction between AEO and K-MEPTS. The performance of composites prepared by silica/NR master batches was investigated by a rubber process analyzer (RPA), transmission electron microscopy (TEM) and a tensile tester. These results demonstrate that AEO forms a physical interface between silica and rubber, resulting in good silica dispersion in the matrix. K-MEPTS forms a chemical interface between silica and rubber, enhancing the reinforcing effect of silica and reducing the mutual friction between silica particles. In summary, using a proper combination of AEO and K-MEPTS is a user-friendly approach for preparing silica/NR composites with excellent performance.
- Open Access
- 1 December 2015
- Published by China Science Publishing & Media Ltd. in Chinese Journal of Applied and Environmental Biology
- Vol. 21 (06) , 1037-1043
The influence of Tween 20 concentration on biodesulfurization of ground tire rubber by Sphingomonas sp.
鞘氨醇单胞菌(Sphingomonas sp.)对废胎面胶粉(GTR)中的化合硫有代谢作用,但其与亲油性的橡胶相容性差. 通过在细菌-GTR共培养脱硫过程中添加表面活性剂吐温20可改善两者之间的亲和性,进而提高脱硫效果. 本文研究吐温20用量对鞘氨醇单胞菌生长及鞘氨醇单胞菌对GTR表面一定深度范围内化学结构的影响,并将脱硫废胎面胶粉(DGTR)与丁苯橡胶(SBR)共混,探讨共混胶的性能及形态. 结果表明:在研究的吐温20用量范围内,其对鞘氨醇单胞菌的生长代谢基本无抑制作用,少量吐温20还可促进细菌的生长;当吐温20用量为0.5 g/L时,DGTR-0.5的溶胀值比GTR增加6.6%,交联密度减小9.4%,比未加吐温20的DGTR-0分别增加和减少3%和4%. 橡胶表面的S—S键、S—C键减少,S—O键增多,其中DGTR-0.5的S含量比GTR降低63.6%,比DGTR-0降低37%;氧含量比GTR增加62.1%,比DGTR-0增加16%,此时脱硫效果最好;与GTR/SBR共混胶相比,DGTR/SBR并用胶的物理性能有所改善,胶粉与基胶间的界面相互渗透作用增强. 其中,DGTR-0.5/SBR胶料的力学性能改善最为显著. 所以,在用鞘氨醇单胞菌脱硫废胎面胶的过程中,0.5 g/L为吐温20的最佳使用浓度.
- 1 December 2015
- Published by China Science Publishing & Media Ltd. in Chinese Journal of Applied and Environmental Biology
- Vol. 21 (06) , 1037-1043
Open AccessThe influence of Tween 20 concentration on biodesulfurization of ground tire rubber by Sphingomonas sp.
鞘氨醇单胞菌(Sphingomonas sp.)对废胎面胶粉(GTR)中的化合硫有代谢作用,但其与亲油性的橡胶相容性差. 通过在细菌-GTR共培养脱硫过程中添加表面活性剂吐温20可改善两者之间的亲和性,进而提高脱硫效果. 本文研究吐温20用量对鞘氨醇单胞菌生长及鞘氨醇单胞菌对GTR表面一定深度范围内化学结构的影响,并将脱硫废胎面胶粉(DGTR)与丁苯橡胶(SBR)共混,探讨共混胶的性能及形态. 结果表明:在研究的吐温20用量范围内,其对鞘氨醇单胞菌的生长代谢基本无抑制作用,少量吐温20还可促进细菌的生长;当吐温20用量为0.5 g/L时,DGTR-0.5的溶胀值比GTR增加6.6%,交联密度减小9.4%,比未加吐温20的DGTR-0分别增加和减少3%和4%. 橡胶表面的S—S键、S—C键减少,S—O键增多,其中DGTR-0.5的S含量比GTR降低63.6%,比DGTR-0降低37%;氧含量比GTR增加62.1%,比DGTR-0增加16%,此时脱硫效果最好;与GTR/SBR共混胶相比,DGTR/SBR并用胶的物理性能有所改善,胶粉与基胶间的界面相互渗透作用增强. 其中,DGTR-0.5/SBR胶料的力学性能改善最为显著. 所以,在用鞘氨醇单胞菌脱硫废胎面胶的过程中,0.5 g/L为吐温20的最佳使用浓度.
- 22 December 2014
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 5 (15) , 11317-11324
Effects of plasticizers on the strain-induced crystallization and mechanical properties of natural rubber and synthetic polyisoprene
Effects of liquid isoprene (LIR-50) and naphthenic oil (NPO) on the strain-induced crystallization (SIC) measured by in situ synchrotron wide-angle X-ray diffraction (WAXD) and mechanical properties of vulcanized natural rubber (NR) and synthetic polyisoprene (IR) were studied. The onset strain (αc) of SIC of NR and IR was 250% and 350%, respectively. NR and IR exhibited stress upturns at strain 383% and 450% in stress–strain curves, and the crystallinities of NR and IR were 7.6% and 8.6%, respectively. After vulcanization, LIR-50 became part of the rubber network, while NPO still existed as free small molecules in rubber networks. After the respective addition of LIR-50 and NPO, the αc of NR composites rarely changed, while the αc of IR composites increased. In addition, the crystallinity and tensile strength of NR and IR filled with LIR-50 and NPO, respectively, decreased, and the reduction in IR composites was higher than that in NR composites. The crystallinity and mechanical properties of the NR and IR plasticized by LIR-50, respectively, were higher than those plasticized by NPO. The maintenance of high crystallinity of NR or IR composites may ensure their good mechanical properties. Therefore, LIR-50 can be used as a reactive plasticizer to maintain good mechanical properties for NR and IR.
- 22 December 2014
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 5 (15) , 11317-11324
Effects of plasticizers on the strain-induced crystallization and mechanical properties of natural rubber and synthetic polyisoprene
Effects of liquid isoprene (LIR-50) and naphthenic oil (NPO) on the strain-induced crystallization (SIC) measured by in situ synchrotron wide-angle X-ray diffraction (WAXD) and mechanical properties of vulcanized natural rubber (NR) and synthetic polyisoprene (IR) were studied. The onset strain (αc) of SIC of NR and IR was 250% and 350%, respectively. NR and IR exhibited stress upturns at strain 383% and 450% in stress–strain curves, and the crystallinities of NR and IR were 7.6% and 8.6%, respectively. After vulcanization, LIR-50 became part of the rubber network, while NPO still existed as free small molecules in rubber networks. After the respective addition of LIR-50 and NPO, the αc of NR composites rarely changed, while the αc of IR composites increased. In addition, the crystallinity and tensile strength of NR and IR filled with LIR-50 and NPO, respectively, decreased, and the reduction in IR composites was higher than that in NR composites. The crystallinity and mechanical properties of the NR and IR plasticized by LIR-50, respectively, were higher than those plasticized by NPO. The maintenance of high crystallinity of NR or IR composites may ensure their good mechanical properties. Therefore, LIR-50 can be used as a reactive plasticizer to maintain good mechanical properties for NR and IR.
- 24 September 2014
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 132 (8)
Influence of liquid isoprene on rheological behavior and mechanical properties of polyisoprene rubber
Prevention of plasticizer leaching from polymers has been a difficult task. Conventional oily plasticizers (COPs) often migrate from rubber matrix, leading to a poor stability of rubber products and serious environmental problem during long‐term use. In the present study, liquid isoprene (LIP) with appropriate molecular weight and no migration was prepared by anionic polymerization. The effects of LIP on the comprehensive properties of carbon black filled polyisoprene rubber (CB/IR) composites were compared with those of one COP, naphthenic oil (NPO). The results showed that LIP reduced the Mooney viscosity and apparent viscosity, and improved the processability of CB/IR composites. LIP improved the mixing efficiency and the dispersion of the CB particles because its compatibility with CB/IR composites was higher than the compatibility of NPO and CB/IR composites. Furthermore, LIP did not migrate from the CB/IR composites because of its participation in the vulcanization reaction. Compared with CB/IR/NPO composites, CB/IR/LIP composites possessed higher mechanical properties, better aging resistance and long‐term dimensional stability. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015, 132, 41485.
- 24 September 2014
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 132 (8)
Influence of liquid isoprene on rheological behavior and mechanical properties of polyisoprene rubber
Prevention of plasticizer leaching from polymers has been a difficult task. Conventional oily plasticizers (COPs) often migrate from rubber matrix, leading to a poor stability of rubber products and serious environmental problem during long‐term use. In the present study, liquid isoprene (LIP) with appropriate molecular weight and no migration was prepared by anionic polymerization. The effects of LIP on the comprehensive properties of carbon black filled polyisoprene rubber (CB/IR) composites were compared with those of one COP, naphthenic oil (NPO). The results showed that LIP reduced the Mooney viscosity and apparent viscosity, and improved the processability of CB/IR composites. LIP improved the mixing efficiency and the dispersion of the CB particles because its compatibility with CB/IR composites was higher than the compatibility of NPO and CB/IR composites. Furthermore, LIP did not migrate from the CB/IR composites because of its participation in the vulcanization reaction. Compared with CB/IR/NPO composites, CB/IR/LIP composites possessed higher mechanical properties, better aging resistance and long‐term dimensional stability. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015, 132, 41485.
- 21 June 2014
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 131 (21)
Half‐submerged cultivation method for the microbial desulfurization of waste latex rubber
The common method for microbial desulfurization is the submerged cultivation method. However, its cost is high because of the high consumption of the medium. To cut costs and improve the desulfurization effect, the new half‐submerged cultivation method was used in the microbial desulfurization of waste latex rubber (WLR) by Sphingomonas species With this method, much more WLR was added per unit volume of the culture medium to be desulfurized, and the desulfurization process was done without stirring. The technical conditions, such as the addition of WLR, the addition of polysorbate 80 (Tween 80), and the desulfurization time, for the half‐submerged cultivation method were studied, and its desulfurization effect was compared with that of the traditional submerged cultivation method. The results show that the optimum conditions for the half‐submerged cultivation method were the addition of 40% w/v WLR in the medium without Tween 80 and desulfurization for 10 days. The X‐ray photoelectron spectroscopy and Fourier transform infrared spectroscopy results demonstrate that the decreases in the content of sulfur, SC bonds, and SS bonds on the surface of WLR after desulfurization by the half‐submerged cultivation method were greater than those after desulfurization by the submerged cultivation method. The composite of waste latex rubber desulfurized by the submerged cultivation method (SDWLR) and styrene–butadiene rubber (SBR) had better mechanical properties than the composite of waste latex rubber desulfurized by the half‐submerged cultivation method (HDWLR) and SBR. Scanning electron microscopy photographs showed that the combinations of HDWLR and the matrix were better than those of SDWLR and the matrix. Compared with the submerged cultivation method, the half‐submerged cultivation method not only reduced the cost of desulfurization but also improved the desulfurization effect. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014, 131, 41039.
- 21 June 2014
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 131 (21)
Half‐submerged cultivation method for the microbial desulfurization of waste latex rubber
The common method for microbial desulfurization is the submerged cultivation method. However, its cost is high because of the high consumption of the medium. To cut costs and improve the desulfurization effect, the new half‐submerged cultivation method was used in the microbial desulfurization of waste latex rubber (WLR) by Sphingomonas species With this method, much more WLR was added per unit volume of the culture medium to be desulfurized, and the desulfurization process was done without stirring. The technical conditions, such as the addition of WLR, the addition of polysorbate 80 (Tween 80), and the desulfurization time, for the half‐submerged cultivation method were studied, and its desulfurization effect was compared with that of the traditional submerged cultivation method. The results show that the optimum conditions for the half‐submerged cultivation method were the addition of 40% w/v WLR in the medium without Tween 80 and desulfurization for 10 days. The X‐ray photoelectron spectroscopy and Fourier transform infrared spectroscopy results demonstrate that the decreases in the content of sulfur, SC bonds, and SS bonds on the surface of WLR after desulfurization by the half‐submerged cultivation method were greater than those after desulfurization by the submerged cultivation method. The composite of waste latex rubber desulfurized by the submerged cultivation method (SDWLR) and styrene–butadiene rubber (SBR) had better mechanical properties than the composite of waste latex rubber desulfurized by the half‐submerged cultivation method (HDWLR) and SBR. Scanning electron microscopy photographs showed that the combinations of HDWLR and the matrix were better than those of SDWLR and the matrix. Compared with the submerged cultivation method, the half‐submerged cultivation method not only reduced the cost of desulfurization but also improved the desulfurization effect. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014, 131, 41039.
- 16 June 2014
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 53 (7) , 1270-1285
Comparison of Structure, Morphology, and Properties of Miktoarms Star Styrene-Butadiene Rubber and Star-Shaped Styrene-Butadiene Rubbe/Polybutadiene Rubber Blends
Four miktoarms star-shaped polybutadiene-Sn-poly(styrene-butadiene) rubber (MSS-PB-PSBR) with 1,1-diphenylhexyl at the ends of the arms were prepared by two different coupling techniques. One technique was a one-step technology, from which two miktoarms star styrene-butadiene rubbers, called AMSS-PB-PSBR, were obtained in which the four arm stars had varying ratios of PB:PSBR arms; another was a two-step technology, from which another two miktoarms star styrene-butadiene rubbers, called BMSS-PB-PSBR, were obtained in which all consisted of PB-Sn-(PSBR)3 stars. The molecular structure parameters and morphology-properties of the four MSS-PB-PSBR were determined and studied, and compared with that of a star-shaped styrene-butadiene rubber (S-SSBR)/poly butadiene rubber (PBR) blend. The results showed that the total coupling efficiency (the ratio of the total number of polymer chains (arms) coupled by SnCl4 to that of the total number of polymer chains) of the MSS-PB-PSBR was higher than 60%. However, the coupling efficiency of the polybutadiene arms of BMSS-PB-PSBR was obviously higher than that of the AMSS-PB-PSBR. Compared with the S-SSBR/PBR blend, MSS-PB-PSBR had a more uniform distribution of the PB phase and a smaller phase size of PB. It was found that MSS-PB-PSBR composites filled with carbon black (CB) had a lower Payne effect than the S-SSBR/PBR/CB composite, with the BMSS-PB-PSBR/CB composites being especially lower. The BMSS-PB-PSBR/CB composites had higher mechanical properties and lower rolling resistance than the AMSS-PB-PSBR/CB composites due to the high coupling efficiency of the polybutadiene arms; the results indicated that the two-step technology was better than the one-step technology for preparing the tread material of “green” tires.
- 16 June 2014
- Published by Taylor & Francis in Journal of Macromolecular Science, Part B
- Vol. 53 (7) , 1270-1285
Comparison of Structure, Morphology, and Properties of Miktoarms Star Styrene-Butadiene Rubber and Star-Shaped Styrene-Butadiene Rubbe/Polybutadiene Rubber Blends
Four miktoarms star-shaped polybutadiene-Sn-poly(styrene-butadiene) rubber (MSS-PB-PSBR) with 1,1-diphenylhexyl at the ends of the arms were prepared by two different coupling techniques. One technique was a one-step technology, from which two miktoarms star styrene-butadiene rubbers, called AMSS-PB-PSBR, were obtained in which the four arm stars had varying ratios of PB:PSBR arms; another was a two-step technology, from which another two miktoarms star styrene-butadiene rubbers, called BMSS-PB-PSBR, were obtained in which all consisted of PB-Sn-(PSBR)3 stars. The molecular structure parameters and morphology-properties of the four MSS-PB-PSBR were determined and studied, and compared with that of a star-shaped styrene-butadiene rubber (S-SSBR)/poly butadiene rubber (PBR) blend. The results showed that the total coupling efficiency (the ratio of the total number of polymer chains (arms) coupled by SnCl4 to that of the total number of polymer chains) of the MSS-PB-PSBR was higher than 60%. However, the coupling efficiency of the polybutadiene arms of BMSS-PB-PSBR was obviously higher than that of the AMSS-PB-PSBR. Compared with the S-SSBR/PBR blend, MSS-PB-PSBR had a more uniform distribution of the PB phase and a smaller phase size of PB. It was found that MSS-PB-PSBR composites filled with carbon black (CB) had a lower Payne effect than the S-SSBR/PBR/CB composite, with the BMSS-PB-PSBR/CB composites being especially lower. The BMSS-PB-PSBR/CB composites had higher mechanical properties and lower rolling resistance than the AMSS-PB-PSBR/CB composites due to the high coupling efficiency of the polybutadiene arms; the results indicated that the two-step technology was better than the one-step technology for preparing the tread material of “green” tires.
- 16 January 2014
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 131 (11)
Dynamic properties of star‐shaped, solution‐polymerized styrene–butadiene rubber and its cocoagulated rubber‐filled with silica/carbon black
The dynamic properties, including the dynamic mechanical properties, flex fatigue properties, dynamic compression properties, and rolling loss properties, of star‐shaped solution‐polymerized styrene–butadiene rubber (SSBR) and organically modified nanosilica powder/star‐shaped styrene–butadiene rubber cocoagulated rubber (N‐SSBR), both filled with silica/carbon black (CB), were studied. N‐SSBR was characterized by 1H‐NMR, gel permeation chromatography, energy dispersive spectrometry, and transmission electron microscopy. The results show that the silica particles were homogeneously dispersed in the N‐SSBR matrix. In addition, the N‐SSBR/SiO2/CB–rubber compounds' high bound rubber contents implied good filler–polymer interactions. Compared with SSBR filled with silica/CB, the N‐SSBR filled with these fillers exhibited better flex fatigue resistance and a lower Payne effect, internal friction loss, compression permanent set, compression heat buildup, and power loss. The nanocomposites with excellent flex fatigue resistance showed several characteristics of branched, thick, rough, homogeneously distributed cross‐sectional cracks, tortuous flex crack paths, few stress concentration points, and obscure interfaces with the matrix. Accordingly, N‐SSBR would be an ideal matrix for applications in the tread of green tires. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014, 131, 40348.
- 16 January 2014
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 131 (11)
Dynamic properties of star‐shaped, solution‐polymerized styrene–butadiene rubber and its cocoagulated rubber‐filled with silica/carbon black
The dynamic properties, including the dynamic mechanical properties, flex fatigue properties, dynamic compression properties, and rolling loss properties, of star‐shaped solution‐polymerized styrene–butadiene rubber (SSBR) and organically modified nanosilica powder/star‐shaped styrene–butadiene rubber cocoagulated rubber (N‐SSBR), both filled with silica/carbon black (CB), were studied. N‐SSBR was characterized by 1H‐NMR, gel permeation chromatography, energy dispersive spectrometry, and transmission electron microscopy. The results show that the silica particles were homogeneously dispersed in the N‐SSBR matrix. In addition, the N‐SSBR/SiO2/CB–rubber compounds' high bound rubber contents implied good filler–polymer interactions. Compared with SSBR filled with silica/CB, the N‐SSBR filled with these fillers exhibited better flex fatigue resistance and a lower Payne effect, internal friction loss, compression permanent set, compression heat buildup, and power loss. The nanocomposites with excellent flex fatigue resistance showed several characteristics of branched, thick, rough, homogeneously distributed cross‐sectional cracks, tortuous flex crack paths, few stress concentration points, and obscure interfaces with the matrix. Accordingly, N‐SSBR would be an ideal matrix for applications in the tread of green tires. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014, 131, 40348.
- 16 October 2013
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 131 (6)
Preparation, structure, and properties of end‐functionalized miktoarms star‐shaped polybutadiene–sn–poly(styrene–butadiene) rubber
Two miktoarm star‐shaped rubbers with large‐volume functional groups of 1,1‐diphenylhexyl at the ends of arms (DMS–PB–SBR) and one miktoarm star‐shaped rubber with n‐butyl groups at the ends of arms (BMS–PB–SBR) were prepared by 1,1‐diphenylhexyllithium (DPHLi) and n‐butyl lithium as initiators, respectively. The molecular structures and morphological properties of the three rubbers (MS–PB–SBR) were studied and compared with those acquired from the blend consisting of star‐shaped solution‐polymerized butadiene styrene rubber (S‐SSBR) and butadiene rubber (PBR) prepared by ourselves. The results showed that MS–PB–SBR exhibited a more uniform distribution of PBR phase and a smaller phase size of PBR than that of S‐SSBR/PBR blend. It is found that MS–PB–SBR composites filled with CB showed the lower Payne effect than that of S‐SSBR/PBR/CB composite, suggesting that the MS–PB–SBR/CB composite (particularly the DMS–PB–SBR/CB composites) would possess excellent mechanical properties, high wet‐skid resistance, and low rolling resistance. For the studied MS–PB–SBR systems, the contribution of large‐volume functional groups at the end of PBR molecular chains to decrease the rolling resistance was larger than that of Sn coupling effect. It is envisioned that the miktoarm star‐shaped rubbers with 1,1‐diphenylhexyl groups at the molecular ends would be useful for making treads of green tires. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2014, 131, 40002.
- 16 October 2013
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 131 (6)
Preparation, structure, and properties of end‐functionalized miktoarms star‐shaped polybutadiene–sn–poly(styrene–butadiene) rubber
Two miktoarm star‐shaped rubbers with large‐volume functional groups of 1,1‐diphenylhexyl at the ends of arms (DMS–PB–SBR) and one miktoarm star‐shaped rubber with n‐butyl groups at the ends of arms (BMS–PB–SBR) were prepared by 1,1‐diphenylhexyllithium (DPHLi) and n‐butyl lithium as initiators, respectively. The molecular structures and morphological properties of the three rubbers (MS–PB–SBR) were studied and compared with those acquired from the blend consisting of star‐shaped solution‐polymerized butadiene styrene rubber (S‐SSBR) and butadiene rubber (PBR) prepared by ourselves. The results showed that MS–PB–SBR exhibited a more uniform distribution of PBR phase and a smaller phase size of PBR than that of S‐SSBR/PBR blend. It is found that MS–PB–SBR composites filled with CB showed the lower Payne effect than that of S‐SSBR/PBR/CB composite, suggesting that the MS–PB–SBR/CB composite (particularly the DMS–PB–SBR/CB composites) would possess excellent mechanical properties, high wet‐skid resistance, and low rolling resistance. For the studied MS–PB–SBR systems, the contribution of large‐volume functional groups at the end of PBR molecular chains to decrease the rolling resistance was larger than that of Sn coupling effect. It is envisioned that the miktoarm star‐shaped rubbers with 1,1‐diphenylhexyl groups at the molecular ends would be useful for making treads of green tires. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2014, 131, 40002.
- 25 September 2012
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 128 (4) , 2516-2524
Study on the structure, morphology, and properties of end‐functionalized star‐shaped solution‐polymerized styrene–butadiene rubber
Three kinds of star‐shaped solution‐polymerized styrene–butadiene rubber (S‐SSBR) were synthesized by living anionic polymerization using a self‐made multifunctional organic lithium initiator. One was S‐SSBR with 100% coupling degree. Others were the functionalized S‐SSBR which had macromolecular chain‐free ends terminated directly (ES‐SSBR‐1), and macromolecular chain terminated after dissociation in the polymerization solution (ES‐SSBR‐2) by 3‐chloropropyl trimethoxy siloxane. The molecular structure parameters of three kinds of SSBR were determined and the end‐functionalized efficiency was calculated. The rheological properties, mechanical properties, and dynamic mechanical properties of ES‐SSBR and S‐SSBR composites filled with silica (SiO2)–carbon black (CB) were investigated. The morphology was observed by transmission electron microscopy and high‐resolution transmission electron microscopy, and the dispersion of the two kinds of filler in the composites was distinguished by X‐ray energy spectrometry. The results showed that the mixing speed of hydrophilic SiO2 powder in the ES‐SSBR was higher than that in the S‐SSBR. SiO2‐CB/ES‐SSBR composites presented excellent mechanical properties, high wet‐skid resistance, and low rolling resistance. Two kinds of nanofiller in the ES‐SSBR exhibited outstanding doping nanometer dispersion and good distribution, which indicated that after being coupled and end‐functionalized, the two free ends of the macromolecular chains formed chemical bonding with the surface chemical groups of CB and SiO2, respectively. Accordingly, ES‐SSBR was a remarkable energy‐saving elastomer. © 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013
- 25 September 2012
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 128 (4) , 2516-2524
Study on the structure, morphology, and properties of end‐functionalized star‐shaped solution‐polymerized styrene–butadiene rubber
Three kinds of star‐shaped solution‐polymerized styrene–butadiene rubber (S‐SSBR) were synthesized by living anionic polymerization using a self‐made multifunctional organic lithium initiator. One was S‐SSBR with 100% coupling degree. Others were the functionalized S‐SSBR which had macromolecular chain‐free ends terminated directly (ES‐SSBR‐1), and macromolecular chain terminated after dissociation in the polymerization solution (ES‐SSBR‐2) by 3‐chloropropyl trimethoxy siloxane. The molecular structure parameters of three kinds of SSBR were determined and the end‐functionalized efficiency was calculated. The rheological properties, mechanical properties, and dynamic mechanical properties of ES‐SSBR and S‐SSBR composites filled with silica (SiO2)–carbon black (CB) were investigated. The morphology was observed by transmission electron microscopy and high‐resolution transmission electron microscopy, and the dispersion of the two kinds of filler in the composites was distinguished by X‐ray energy spectrometry. The results showed that the mixing speed of hydrophilic SiO2 powder in the ES‐SSBR was higher than that in the S‐SSBR. SiO2‐CB/ES‐SSBR composites presented excellent mechanical properties, high wet‐skid resistance, and low rolling resistance. Two kinds of nanofiller in the ES‐SSBR exhibited outstanding doping nanometer dispersion and good distribution, which indicated that after being coupled and end‐functionalized, the two free ends of the macromolecular chains formed chemical bonding with the surface chemical groups of CB and SiO2, respectively. Accordingly, ES‐SSBR was a remarkable energy‐saving elastomer. © 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013