Electropulse (Spark) Plasma Sintering of Ultrafine-Grained WC–Al2O3 Ceramics
Authors:
- E. A. LantsevELE. A. Lantsev
- A. V. NokhrinA. V. Nokhrin
- M. S. BoldinM. S. Boldin
- K. E. SmetaninaKSK. E. Smetanina
- A. A. MurashovAMA. A. Murashov
- Yu. V. BlagoveshchenskiiYBYu. V. Blagoveshchenskii
- N. V. IsaevaNIN. V. Isaeva
- G. V. ShcherbakGSG. V. Shcherbak
- V. N. Chuvil’DEevVCV. N. Chuvil’DEev
- N. Yu. TabachkovaNTN. Yu. Tabachkova
- A. V. TerentyevATA. V. Terentyev
- 1 October 2023
- journal article
- research article
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (5-6) , 1441-1450
Abstract
The sintering mechanisms of WC–Al2O3 nanopowder compositions with different contents of al-umina particles (1, 3, and 5 wt %) have been studied. The samples of WC–Al2O3 ceramics are obtained by electropulse (spark) plasma sintering (SPS) in vacuum by heating to a temperature of 1450°C at a rate of 50°C/min under a uniaxial stress of 70 MPa. Plasma-chemical nanopowders of tungsten monocarbide and submicron powders of alumina are used to fabricate the ceramics. The density, microstructure, phase composition, microhardness (HV), and crack resistance (KIC) of the ceramics have been studied. It has been shown that the use of SPS enables the production of WC-Al2O3 ceramics with a high relative density (95.4–98.1%) and a homogeneous microstructure with the ultrafine grain size (0.1–0.2 μm). The X-ray phase analysis has shown that during the SPS of WC–Al2O3 ceramics the formation of undesirable W2C phase occurs which results in a decrease in the crack resistance. To reduce the intensity of formation of W2C particles, free carbon in the form of colloidal graphite (0.1, 0.2, and 0.3 wt %) is introduced into the WC–Al2O3 ceramic. Using the Young–Cutler model and the model of diffusion resorption of pores it has been shown that the main mechanism behind the SPS of WC–Al2O3 ceramics is a grain-boundary diffusion. It has been found that the introduction of graphite leads to a decrease in the activation energy of SPS of the WC–Al2O3 ceramics, which is probably due to a reduction in the W2C particle content to 0.5 wt %.Keywords
This publication has 34 references indexed in Scilit:
- Effect of grain boundary state and grain size on the microstructure and mechanical properties of alumina obtained by SPS: A case of the amorphous layer on particle surfaceCeramics International, 2022
- Consolidation and mechanical properties of WC-Al2O3 composite prepared via high energy ball milling and spark plasma sinteringCeramics International, 2022
- Preparation, mechanical and tribological properties of WC-Al2O3 composite doped with graphene plateletsCeramics International, 2020
- A Review on Binderless Tungsten Carbide: Development and ApplicationNano-Micro Letters, 2019
- Field-Assisted Sintering2018
- XPS study of surface chemistry of tungsten carbides nanopowders produced through DC thermal plasma/hydrogen annealing processApplied Surface Science, 2015
- Tungsten Carbides2013
- The sintering kinetics of ultrafine tungsten carbide powdersCeramics International, 2011
- The effect of electric field and pressure on the synthesis and consolidation of materials: A review of the spark plasma sintering methodJournal of Materials Science, 2006
- Carbon self-diffusion in tungsten carbideJournal of Materials Science, 1971