Yuriy V Blagoveshchenskiy
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Yuriy V Blagoveshchenskiy has a total of 47 co-authors. Here are the top co-authors by number of shared publications:
- Aleksey Vladimirovich Nokhrin
National Research Lobachevsky State University of Nizhny Novgorod, Nizhny Novgorod, Russia
13 shared publications - Maksim Sergeevich Boldin
National Research Lobachevsky State University of Nizhny Novgorod, Nizhny Novgorod, Russia
10 shared publications - Eugeniy A. Lantsev
Materials Science Department, Physico-Technical Research Institure, Lobachevsky State University of Nizhny Novgorod, 603022 Nizhny Novgorod, Russia
9 shared publications - Nataliya V Isaeva
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
9 shared publications - Vladimir Nikolaevich Chuvil’dEev
National Research Lobachevsky State University of Nizhny Novgorod, Nizhny Novgorod, Russia
9 shared publications - Ksenia Evgenievna Smetanina
National Research Lobachevsky State University of Nizhny Novgorod, Nizhny Novgorod, Russia
7 shared publications
Latest Publications
- 23 September 2026
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 17 (5) , 1441-1449
Spark Plasma Sintering Specificity in Nanoscale and Submicron WC—25 wt % TiC Powders
The mechanisms behind sintering nanopowder WC—25 wt % TiC compositions with titanium carbide of varying dispersion are investigated. WC–TiC ceramics are made using spark plasma sintering (SPS) in vacuum within the temperature range of 1000–1400°C at a heating rate of 50°C/min under an applied pressure of 70 MPa and at different dwell times. Plasma‑chemical tungsten monocarbide nanopowders and nano- and submicron‑sized titanium carbide powders are used as initial materials. The microstructure, phase composition, and density of the sintered ceramics are examined. It is demonstrated that SPS allows making WC–TiC ceramics with a homogenous ultrafine-grained structure (0.2–0.5 μm). X-ray phase analysis reveals forming and evolving (W,Ti)C solid solution during sintering. The sintering kinetics exhibit a multistage behavior characteristic of the SPS process developing in WC–TiC systems. It is established that the use of nanoscale titanium carbide particles leads to earlier dominance of mass transfer along grain boundaries and interphase contacts due to an increased fraction of active contact areas. In contrast, submicron TiC particles result in a more pronounced maximum shrinkage rate associated with the rapid involvement of larger material volumes in the diffusion flux. The presence of vacancies in the carbon sublattice of titanium carbide plays a key role in activating diffusive mass transfer and in forming the (W,Ti)C solid solution.
- 23 September 2026
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 17 (5) , 1441-1449
Spark Plasma Sintering Specificity in Nanoscale and Submicron WC—25 wt % TiC Powders
The mechanisms behind sintering nanopowder WC—25 wt % TiC compositions with titanium carbide of varying dispersion are investigated. WC–TiC ceramics are made using spark plasma sintering (SPS) in vacuum within the temperature range of 1000–1400°C at a heating rate of 50°C/min under an applied pressure of 70 MPa and at different dwell times. Plasma‑chemical tungsten monocarbide nanopowders and nano- and submicron‑sized titanium carbide powders are used as initial materials. The microstructure, phase composition, and density of the sintered ceramics are examined. It is demonstrated that SPS allows making WC–TiC ceramics with a homogenous ultrafine-grained structure (0.2–0.5 μm). X-ray phase analysis reveals forming and evolving (W,Ti)C solid solution during sintering. The sintering kinetics exhibit a multistage behavior characteristic of the SPS process developing in WC–TiC systems. It is established that the use of nanoscale titanium carbide particles leads to earlier dominance of mass transfer along grain boundaries and interphase contacts due to an increased fraction of active contact areas. In contrast, submicron TiC particles result in a more pronounced maximum shrinkage rate associated with the rapid involvement of larger material volumes in the diffusion flux. The presence of vacancies in the carbon sublattice of titanium carbide plays a key role in activating diffusive mass transfer and in forming the (W,Ti)C solid solution.
- 3 June 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (3) , 696-706
Study of the Phase Composition and Microstructure of Complex Carbide (Ti, W)C Obtained by Spark Plasma Sintering of WC and TiC Powders
—The possibility of low-temperature in situ synthesis of (Ti, W)C using plasma-chemical WC nanopowders and industrial micron TiC powders is demonstrated. Sintering/synthesis of WC–(25, 50, and 75) wt % TiC is carried out by electric pulsed (“spark”) plasma sintering (SPS) by heating powders in a vacuum at a rate of 50°C/min to a temperature of more than 1200°C under conditions of applying a stress of 70 MPa. It is established that the synthesis proceeds most efficiently in nanopowders with an addition of 50 and 75 wt % TiC. It is shown that the joint use of plasma-chemical synthesis of nanopowders and SPS makes it possible to obtain fine-grained (with a grain size of less than 1 μm) samples with increased density and satisfactory mechanical properties (Vickers hardness is 17–18 GPa, and minimum Palmquist crack resistance coefficient is ~3 MPa m1/2).
- 3 June 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (3) , 696-706
Study of the Phase Composition and Microstructure of Complex Carbide (Ti, W)C Obtained by Spark Plasma Sintering of WC and TiC Powders
—The possibility of low-temperature in situ synthesis of (Ti, W)C using plasma-chemical WC nanopowders and industrial micron TiC powders is demonstrated. Sintering/synthesis of WC–(25, 50, and 75) wt % TiC is carried out by electric pulsed (“spark”) plasma sintering (SPS) by heating powders in a vacuum at a rate of 50°C/min to a temperature of more than 1200°C under conditions of applying a stress of 70 MPa. It is established that the synthesis proceeds most efficiently in nanopowders with an addition of 50 and 75 wt % TiC. It is shown that the joint use of plasma-chemical synthesis of nanopowders and SPS makes it possible to obtain fine-grained (with a grain size of less than 1 μm) samples with increased density and satisfactory mechanical properties (Vickers hardness is 17–18 GPa, and minimum Palmquist crack resistance coefficient is ~3 MPa m1/2).
- 1 October 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (5-6) , 1441-1450
Electropulse (Spark) Plasma Sintering of Ultrafine-Grained WC–Al2O3 Ceramics
The sintering mechanisms of WC–Al2O3 nanopowder compositions with different contents of al-umina particles (1, 3, and 5 wt %) have been studied. The samples of WC–Al2O3 ceramics are obtained by electropulse (spark) plasma sintering (SPS) in vacuum by heating to a temperature of 1450°C at a rate of 50°C/min under a uniaxial stress of 70 MPa. Plasma-chemical nanopowders of tungsten monocarbide and submicron powders of alumina are used to fabricate the ceramics. The density, microstructure, phase composition, microhardness (HV), and crack resistance (KIC) of the ceramics have been studied. It has been shown that the use of SPS enables the production of WC-Al2O3 ceramics with a high relative density (95.4–98.1%) and a homogeneous microstructure with the ultrafine grain size (0.1–0.2 μm). The X-ray phase analysis has shown that during the SPS of WC–Al2O3 ceramics the formation of undesirable W2C phase occurs which results in a decrease in the crack resistance. To reduce the intensity of formation of W2C particles, free carbon in the form of colloidal graphite (0.1, 0.2, and 0.3 wt %) is introduced into the WC–Al2O3 ceramic. Using the Young–Cutler model and the model of diffusion resorption of pores it has been shown that the main mechanism behind the SPS of WC–Al2O3 ceramics is a grain-boundary diffusion. It has been found that the introduction of graphite leads to a decrease in the activation energy of SPS of the WC–Al2O3 ceramics, which is probably due to a reduction in the W2C particle content to 0.5 wt %.
- 1 October 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (5-6) , 1441-1450
Electropulse (Spark) Plasma Sintering of Ultrafine-Grained WC–Al2O3 Ceramics
The sintering mechanisms of WC–Al2O3 nanopowder compositions with different contents of al-umina particles (1, 3, and 5 wt %) have been studied. The samples of WC–Al2O3 ceramics are obtained by electropulse (spark) plasma sintering (SPS) in vacuum by heating to a temperature of 1450°C at a rate of 50°C/min under a uniaxial stress of 70 MPa. Plasma-chemical nanopowders of tungsten monocarbide and submicron powders of alumina are used to fabricate the ceramics. The density, microstructure, phase composition, microhardness (HV), and crack resistance (KIC) of the ceramics have been studied. It has been shown that the use of SPS enables the production of WC-Al2O3 ceramics with a high relative density (95.4–98.1%) and a homogeneous microstructure with the ultrafine grain size (0.1–0.2 μm). The X-ray phase analysis has shown that during the SPS of WC–Al2O3 ceramics the formation of undesirable W2C phase occurs which results in a decrease in the crack resistance. To reduce the intensity of formation of W2C particles, free carbon in the form of colloidal graphite (0.1, 0.2, and 0.3 wt %) is introduced into the WC–Al2O3 ceramic. Using the Young–Cutler model and the model of diffusion resorption of pores it has been shown that the main mechanism behind the SPS of WC–Al2O3 ceramics is a grain-boundary diffusion. It has been found that the introduction of graphite leads to a decrease in the activation energy of SPS of the WC–Al2O3 ceramics, which is probably due to a reduction in the W2C particle content to 0.5 wt %.
- Open Access
Nonuniform Distribution of Crystalline Phases and Grain Sizes in the Surface Layers of WC Ceramics Produced by Spark Plasma Sintering
The research results conducted on binderless tungsten carbide (WC) ceramics obtained by spark plasma sintering (SPS) of WC powders with different average particle sizes (95, 800, 3000 nm) are presented. Nonuniform distribution of crystalline phases and microstructure of the WC ceramics was studied using layer-by-layer X-ray diffraction (XRD) analysis and scanning electron microscopy (SEM). Surface layers of the WC-based ceramics are characterized by nonuniform distribution of W2C crystalline phase and grain sizes, including the appearance of abnormally large grains. Thickness of the nonuniform layer was at least 50 μm. The effect under study is associated with an intense carbon diffusion from graphite foil. On the one hand, this contributed to a decrease in the intensity of W2C phase particle formation, which is transformed into α-WC phase due to the carbon. On the other hand, it caused abnormal grain growth in the layer where the carbon diffused. The obtained value of the carbon diffusion depth (50 μm) exceeds the values known from the literature (up to 1 μm in the case of volume diffusion even at temperature of 2370 °C and exposure time of ~60 h). The use of boron nitride (BN) as a protective coating on graphite mold parts did not prevent the formation of nonuniform layer on the ceramic surface.
Open AccessNonuniform Distribution of Crystalline Phases and Grain Sizes in the Surface Layers of WC Ceramics Produced by Spark Plasma Sintering
The research results conducted on binderless tungsten carbide (WC) ceramics obtained by spark plasma sintering (SPS) of WC powders with different average particle sizes (95, 800, 3000 nm) are presented. Nonuniform distribution of crystalline phases and microstructure of the WC ceramics was studied using layer-by-layer X-ray diffraction (XRD) analysis and scanning electron microscopy (SEM). Surface layers of the WC-based ceramics are characterized by nonuniform distribution of W2C crystalline phase and grain sizes, including the appearance of abnormally large grains. Thickness of the nonuniform layer was at least 50 μm. The effect under study is associated with an intense carbon diffusion from graphite foil. On the one hand, this contributed to a decrease in the intensity of W2C phase particle formation, which is transformed into α-WC phase due to the carbon. On the other hand, it caused abnormal grain growth in the layer where the carbon diffused. The obtained value of the carbon diffusion depth (50 μm) exceeds the values known from the literature (up to 1 μm in the case of volume diffusion even at temperature of 2370 °C and exposure time of ~60 h). The use of boron nitride (BN) as a protective coating on graphite mold parts did not prevent the formation of nonuniform layer on the ceramic surface.
- 1 June 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (3) , 691-706
Study of High-Speed Sintering of Fine-Grained Hard Alloys Based on Tungsten Carbide with Ultralow Cobalt Content: III. Effect of C Content on Sintering Kinetics of the WC–Co Nanopowders
The features of high-speed spark plasma sintering (SPS) of plasma-chemical nanopowders WC‒(0.3, 0.6, 1) wt % Co with the addition of 0.3 and 0.5 wt % graphite were studied. The structural features of the ultralow-cobalt hard alloys with graphite addition during SPS are due to the simultaneous influence of an increased concentration of oxygen adsorbed on the surface of plasma-chemical WC–Co nanoparticles during mixing with graphite and the effect of graphite, which leads to a decrease in activation energy of sintering owing to a decrease in the intensity of formation of η-phase particles in “oxidized” WC–Co nanopowders, as well as the formation of a fairly uniform fine-grained structure. Samples of fine-grained ultralow-cobalt hard alloys with increased hardness and fracture toughness were obtained (for a WC–0.6 wt % Co–0.3 wt % C hard alloy with an average grain size of ~(1–1.5) μm, the hardness is Hv = 20.2–20.5 GPa with a minimum crack resistance coefficient KIC = 9.2–10.4 MPa m1/2).
- 1 June 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (3) , 691-706
Study of High-Speed Sintering of Fine-Grained Hard Alloys Based on Tungsten Carbide with Ultralow Cobalt Content: III. Effect of C Content on Sintering Kinetics of the WC–Co Nanopowders
The features of high-speed spark plasma sintering (SPS) of plasma-chemical nanopowders WC‒(0.3, 0.6, 1) wt % Co with the addition of 0.3 and 0.5 wt % graphite were studied. The structural features of the ultralow-cobalt hard alloys with graphite addition during SPS are due to the simultaneous influence of an increased concentration of oxygen adsorbed on the surface of plasma-chemical WC–Co nanoparticles during mixing with graphite and the effect of graphite, which leads to a decrease in activation energy of sintering owing to a decrease in the intensity of formation of η-phase particles in “oxidized” WC–Co nanopowders, as well as the formation of a fairly uniform fine-grained structure. Samples of fine-grained ultralow-cobalt hard alloys with increased hardness and fracture toughness were obtained (for a WC–0.6 wt % Co–0.3 wt % C hard alloy with an average grain size of ~(1–1.5) μm, the hardness is Hv = 20.2–20.5 GPa with a minimum crack resistance coefficient KIC = 9.2–10.4 MPa m1/2).
- 1 June 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (3) , 677-690
Study of High-Speed Sintering of Fine-Grained Hard Alloys Based on Tungsten Carbide with Ultralow Cobalt Content: II. Hard Alloys WC–(0.3–1) wt % Co
The features of spark plasma sintering (SPS) of plasma-chemical nanopowders WC–(0.3, 0.6, 1) wt % Co were studied. The SPS process of ultralow-cobalt hard alloys can be sequentially represented as a change of the following stages: rearrangement of particles at lower temperatures (Stage I) → sintering of WC–Co particles due to Coble creep of γ phase of cobalt, the intensity of which is determined by the grain boundary diffusion rate (Stage II) → sintering due to diffusion creep, the rate of which is limited by the bulk diffusion in cobalt (Stage III-1) → sintering of tungsten carbide particles along the intergranular boundaries of WC/WC under conditions of intense grain growth (Stage III-2). Samples with a high density (96.4–98.4%) and high mechanical properties were obtained (for the WC–0.3% Co hard alloy: Hv ~ 20.5 GPa, K1C = 7.1 MPa m1/2).
- 1 June 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (3) , 677-690
Study of High-Speed Sintering of Fine-Grained Hard Alloys Based on Tungsten Carbide with Ultralow Cobalt Content: II. Hard Alloys WC–(0.3–1) wt % Co
The features of spark plasma sintering (SPS) of plasma-chemical nanopowders WC–(0.3, 0.6, 1) wt % Co were studied. The SPS process of ultralow-cobalt hard alloys can be sequentially represented as a change of the following stages: rearrangement of particles at lower temperatures (Stage I) → sintering of WC–Co particles due to Coble creep of γ phase of cobalt, the intensity of which is determined by the grain boundary diffusion rate (Stage II) → sintering due to diffusion creep, the rate of which is limited by the bulk diffusion in cobalt (Stage III-1) → sintering of tungsten carbide particles along the intergranular boundaries of WC/WC under conditions of intense grain growth (Stage III-2). Samples with a high density (96.4–98.4%) and high mechanical properties were obtained (for the WC–0.3% Co hard alloy: Hv ~ 20.5 GPa, K1C = 7.1 MPa m1/2).
- Open Access
- 16 May 2023
- Published by MDPI AG in Preprints.org
Nonuniform Distribution of Crystalline Phases and Grain Sizes in the Surface Layers of WC Ceramics Produced by Spark Plasma Sintering
The research results conducted on binderless tungsten carbide (WC) ceramics obtained by Spark Plasma Sintering (SPS) of WC powders with different average particle sizes (0.095, 0.8, 3 μm) are presented. Nonuniform distribution of crystalline phases and microstructure of the WC ceramics was studied using layer-by-layer XRD analysis and SEM. Surface layers of the WC-based ceramics are characterized by nonuniform distribution of W2C crystalline phase and grain sizes, including the appearance of abnormally large grains. Thickness of the nonuniform layer was at least 50 μm. The effect under study is associated with an intense carbon diffusion from graphite foil. On the one hand, this contributed to a decrease in the intensity of W2C phase particle formation, which is transformed into α-WC phase due to the carbon. On the other hand, it caused abnormal grain growth in the layer where the carbon diffused. The obtained value of the carbon diffusion depth exceeds the values known from the literature (up to 1 μm in the case of volume diffusion even at temperature of 2370℃ and exposure time of ~ 60 h). The use of boron nitride (BN) as a protective coating on graphite mold parts did not prevent the formation of nonuniform layer on the ceramic surface.
- 16 May 2023
- Published by MDPI AG in Preprints.org
Open AccessNonuniform Distribution of Crystalline Phases and Grain Sizes in the Surface Layers of WC Ceramics Produced by Spark Plasma Sintering
The research results conducted on binderless tungsten carbide (WC) ceramics obtained by Spark Plasma Sintering (SPS) of WC powders with different average particle sizes (0.095, 0.8, 3 μm) are presented. Nonuniform distribution of crystalline phases and microstructure of the WC ceramics was studied using layer-by-layer XRD analysis and SEM. Surface layers of the WC-based ceramics are characterized by nonuniform distribution of W2C crystalline phase and grain sizes, including the appearance of abnormally large grains. Thickness of the nonuniform layer was at least 50 μm. The effect under study is associated with an intense carbon diffusion from graphite foil. On the one hand, this contributed to a decrease in the intensity of W2C phase particle formation, which is transformed into α-WC phase due to the carbon. On the other hand, it caused abnormal grain growth in the layer where the carbon diffused. The obtained value of the carbon diffusion depth exceeds the values known from the literature (up to 1 μm in the case of volume diffusion even at temperature of 2370℃ and exposure time of ~ 60 h). The use of boron nitride (BN) as a protective coating on graphite mold parts did not prevent the formation of nonuniform layer on the ceramic surface.
- Open Access
- 15 May 2023
- Published by MDPI AG in Preprints.org
Combined Effect of SiC and Carbon on Sintering Kinetics, MI-Crostructure and Mechanical Properties of Fine-Grained Binder-Less Tungsten Carbide
This paper investigates the density, phase composition, microstructure and mechanical properties (microhardness, fracture toughness) of binderless WC + SiC ceramics obtained by conventional pressureless sintering (CPS) and Spark Plasma Sintering (SPS). α-WC nanopowders obtained by DC arc plasma chemical synthesis and β-SiC powders have been used as raw materials. The content of SiC particles was 1, 3, 5% wt. Excess graphite (0.3, 0.5% wt.) was added to α-WC nanopowders to decrease the volume fraction of W2C particles that negatively affect the mechanical properties of ceramics. WC + 1% wt. SiC + 0.3% wt. C ceramics are shown to have a homogeneous fine-grained microstructure, high relative density, increased microhardness and Palmquist fracture toughness. The CPS and SPS activation energies of WC + SiC nanopowders at an intensive shrinkage stage are determined using the Young-Cutler model. The effect of carbon and SiC particles on the CPS and SPS activation energies of tungsten carbide nanopowders has been analyzed. The CPS activation energies of WC, WC + C and WC + SiC + C nanopowders are shown to be closer to the carbon diffusion activation energy along α-WC grain boundaries. The SPS activation energies of WC and WC + SiC nanopowders turn out to be lower than the carbon grain boundary diffusion activation energy of α-WC.
- 15 May 2023
- Published by MDPI AG in Preprints.org
Open AccessCombined Effect of SiC and Carbon on Sintering Kinetics, MI-Crostructure and Mechanical Properties of Fine-Grained Binder-Less Tungsten Carbide
This paper investigates the density, phase composition, microstructure and mechanical properties (microhardness, fracture toughness) of binderless WC + SiC ceramics obtained by conventional pressureless sintering (CPS) and Spark Plasma Sintering (SPS). α-WC nanopowders obtained by DC arc plasma chemical synthesis and β-SiC powders have been used as raw materials. The content of SiC particles was 1, 3, 5% wt. Excess graphite (0.3, 0.5% wt.) was added to α-WC nanopowders to decrease the volume fraction of W2C particles that negatively affect the mechanical properties of ceramics. WC + 1% wt. SiC + 0.3% wt. C ceramics are shown to have a homogeneous fine-grained microstructure, high relative density, increased microhardness and Palmquist fracture toughness. The CPS and SPS activation energies of WC + SiC nanopowders at an intensive shrinkage stage are determined using the Young-Cutler model. The effect of carbon and SiC particles on the CPS and SPS activation energies of tungsten carbide nanopowders has been analyzed. The CPS activation energies of WC, WC + C and WC + SiC + C nanopowders are shown to be closer to the carbon diffusion activation energy along α-WC grain boundaries. The SPS activation energies of WC and WC + SiC nanopowders turn out to be lower than the carbon grain boundary diffusion activation energy of α-WC.
- 30 May 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (3) , 761-774
Study of High-Speed Sintering of Fine-Grained Hard Alloys Based on Tungsten Carbide with Ultralow Cobalt Content: Part I. Pure Tungsten Carbide
The results of studies of the kinetics of high-speed spark plasma sintering (SPS) of plasma-chemical nanosized and industrial micron tungsten carbide powders are described. During SPS, the carburization of the surface layer of tungsten carbide samples occurs, leading to differences in the phase composition and hardness of the surface and central regions of sintered ceramics. The process of SPS of tungsten carbide can be sequentially represented as a change of the following mechanisms: rearrangement of particles at lower temperatures (Stage I) → sintering of particles due to grain boundary diffusion (Stage II) → sintering due to diffusion in the crystal lattice (Stage III-1) → sintering under conditions of intense grain growth with an abnormally low diffusion activation energy (Stage III-2).
- 30 May 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (3) , 761-774
Study of High-Speed Sintering of Fine-Grained Hard Alloys Based on Tungsten Carbide with Ultralow Cobalt Content: Part I. Pure Tungsten Carbide
The results of studies of the kinetics of high-speed spark plasma sintering (SPS) of plasma-chemical nanosized and industrial micron tungsten carbide powders are described. During SPS, the carburization of the surface layer of tungsten carbide samples occurs, leading to differences in the phase composition and hardness of the surface and central regions of sintered ceramics. The process of SPS of tungsten carbide can be sequentially represented as a change of the following mechanisms: rearrangement of particles at lower temperatures (Stage I) → sintering of particles due to grain boundary diffusion (Stage II) → sintering due to diffusion in the crystal lattice (Stage III-1) → sintering under conditions of intense grain growth with an abnormally low diffusion activation energy (Stage III-2).
- Open Access
A Study of the Impact of Graphite on the Kinetics of SPS in Nano- and Submicron WC-10%Co Powder Compositions
This study investigates the impact of carbon on the kinetics of the spark plasma sintering (SPS) of nano- and submicron powders WC-10 wt.%Co. Carbon, in the form of graphite, was introduced into powders by mixing. The activation energy of solid-phase sintering was determined for the conditions of isothermal and continuous heating. It has been demonstrated that increasing the carbon content leads to a decrease in the fraction of η-phase particles and a shift of the shrinkage curve towards lower heating temperatures. It has been established that increasing the graphite content in nano- and submicron powders has no significant effect on the SPS activation energy for “mid-range” heating temperatures, QS(I). The value of QS(I) is close to the activation energy of grain-boundary diffusion in cobalt. It has been demonstrated that increasing the content of graphite leads to a significant decrease in the SPS activation energy, QS(II), for “higher-range” heating temperatures due to lower concentration of tungsten atoms in cobalt-based γ-phase. It has been established that the sintering kinetics of fine-grained WC-Co hard alloys is limited by the intensity of diffusion creep of cobalt (Coble creep).
Open AccessA Study of the Impact of Graphite on the Kinetics of SPS in Nano- and Submicron WC-10%Co Powder Compositions
This study investigates the impact of carbon on the kinetics of the spark plasma sintering (SPS) of nano- and submicron powders WC-10 wt.%Co. Carbon, in the form of graphite, was introduced into powders by mixing. The activation energy of solid-phase sintering was determined for the conditions of isothermal and continuous heating. It has been demonstrated that increasing the carbon content leads to a decrease in the fraction of η-phase particles and a shift of the shrinkage curve towards lower heating temperatures. It has been established that increasing the graphite content in nano- and submicron powders has no significant effect on the SPS activation energy for “mid-range” heating temperatures, QS(I). The value of QS(I) is close to the activation energy of grain-boundary diffusion in cobalt. It has been demonstrated that increasing the content of graphite leads to a significant decrease in the SPS activation energy, QS(II), for “higher-range” heating temperatures due to lower concentration of tungsten atoms in cobalt-based γ-phase. It has been established that the sintering kinetics of fine-grained WC-Co hard alloys is limited by the intensity of diffusion creep of cobalt (Coble creep).