Microstructure and Mechanical Properties of Mullite Prepared by the Sol‐Gel Method
Authors:
- 1 January 1987
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 70 (1) , C‐7-C‐8
Abstract
Mullite (3Al 2 O 3 ·2SiO 2 ) of stoichiometric composition was prepared by mixing boehmite sol and silica dispersion and gelling at a pH of 3. Complete mullitization takes place at or above 1300°C. Ultrafine mullite powder prepared by calcining gel at 1400°C and attrition milling could be sintered to >98% (theoretical density) at 1650°C for 1.5 h. The flexural strength of the sintered body at room temperature was 405 MPa and 350 MPa at 1300°C. Only traces of a secondary phase were observed along the grain boundary.Keywords
This publication has 8 references indexed in Scilit:
- Sintering and Mechanical Properties of Stoichiometric MulliteJournal of the American Ceramic Society, 1985
- Stable and Metastable Equilibria in the System SiO 2 ‐Al 2 O 3Journal of the American Ceramic Society, 1975
- Creep of Polycrystalline MulliteJournal of the American Ceramic Society, 1975
- Synthesis and Mechanical Properties of Stoichiometric Aluminum Silicate (Mullite)Journal of the American Ceramic Society, 1972
- Diffusion and Reaction Studies in the System Al 2 O 3 ‐SiO 2Journal of the American Ceramic Society, 1972
- Mullite1971
- Revised Phase Diagram for the System Al2O3—SiO2Journal of the American Ceramic Society, 1962
- THE SYSTEM: Al 2 O 3 .SiO 2Journal of the American Ceramic Society, 1924