The effect of the TiC particle size on the preferred oxidation temperature for self-healing of oxide ceramic matrix materials
Authors:
Open Access
- 4 January 2018
- journal article
- research article
- Published by Springer Nature in Journal of Materials Science
- Vol. 53 (8) , 5973-5986
Abstract
No abstract availableKeywords
Funding Information
- FP7 People: Marie-Curie Actions (290308)
This publication has 33 references indexed in Scilit:
- On the use of TiC as high-temperature healing particles in alumina based compositesJournal of the European Ceramic Society, 2016
- Selection of healing agents for autonomous healing of alumina at high temperaturesJournal of the European Ceramic Society, 2016
- Demonstrating the self-healing behaviour of some selected ceramics under combustion chamber conditionsSmart Materials and Structures, 2016
- Enhancement of the self-healing ability in oxidation induced self-healing ceramic by modifying the healing agentSmart Materials and Structures, 2012
- Crack Disappearance by High-Temperature Oxidation of Alumina Toughened by Ni Nano-ParticlesAdvanced Materials Research, 2009
- A new methodology to guarantee the structural integrity of Al2O3/SiC composite using crack healing and a proof testFatigue & Fracture of Engineering Materials & Structures, 2007
- Strength recovery behavior of machined Al2O3/SiC nano-composite ceramics by crack-healingJournal of the European Ceramic Society, 2007
- Crack‐healing and mechanical behaviour of Al2O3/SiC composites at elevated temperatureFatigue & Fracture of Engineering Materials & Structures, 2004
- Fatigue strength of crack‐healed Si3N4/SiC composite ceramicsFatigue & Fracture of Engineering Materials & Structures, 1999