Linda Boatemaa
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Linda Boatemaa has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Ann-Sophie Farle
Department of Materials Science and Engineering Delft University of Technology Delft The Netherlands
1 shared publication - Guo-Ping Bei
Department of Materials Science (Glass and Ceramics) University of Erlangen‐Nuernberg Martensstr. 5 Erlangen 91058 Germany
1 shared publication J. C. Brouwer
Delft University of Technology
1 shared publicationMyrthe Bosch
Department of Materials Science and Engineering Delft University of Technology Delft The Netherlands
1 shared publicationS. van der Zwaag
Delft University of Technology
1 shared publication- Sybrand van der Zwaag
Novel Aerospace Materials Group, Faculty of Aerospace Engineering, Delft University of Technology, Delft, The Netherlands
1 shared publication
Latest Publications
- Open Access
- 25 May 2018
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 101 (12) , 5684-5693
Autonomous high‐temperature healing of surface cracks in Al 2 O 3 containing Ti 2 AlC particles
In this work, the oxidation‐induced crack healing of Al 2 O 3 containing 20 vol.% of Ti 2 AlC MAX phase inclusions as healing particles was studied. The oxidation kinetics of the Ti 2 AlC particles having an average diameter of about 10 μm was studied via thermogravimetry and/or differential thermal analysis. Surface cracks of about 80 μm long and 0.5 μm wide were introduced into the composite by Vickers indentation. After annealing in air at high temperatures, the cracks were filled with stable oxides of Ti and Al as a result of the decomposition of the Ti 2 AlC particles. Crack healing was studied at 800, 900, and 1000°C for 0.25, 1, 4, and 16 hours, and the strength recovery was measured by 4‐point bending. Upon indentation, the bending strength of the samples dropped by about 50% from 402 ± 35 to 229 ± 14 MPa. This bending strength increased to about 90% of the undamaged material after annealing at 1000°C for just 15 minutes, while full strength was recovered after annealing for 1 hour. As the healing temperature was reduced to 900 and 800°C, the time required for full‐strength recovery increased to 4 and 16 hours, respectively. The initial bending strength and the fracture toughness of the composite material were found to be about 19% lower and 20% higher than monolithic alumina, respectively, making this material an attractive substitute for monolithic alumina used in high‐temperature applications.
- 25 May 2018
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 101 (12) , 5684-5693
Open AccessAutonomous high‐temperature healing of surface cracks in Al 2 O 3 containing Ti 2 AlC particles
In this work, the oxidation‐induced crack healing of Al 2 O 3 containing 20 vol.% of Ti 2 AlC MAX phase inclusions as healing particles was studied. The oxidation kinetics of the Ti 2 AlC particles having an average diameter of about 10 μm was studied via thermogravimetry and/or differential thermal analysis. Surface cracks of about 80 μm long and 0.5 μm wide were introduced into the composite by Vickers indentation. After annealing in air at high temperatures, the cracks were filled with stable oxides of Ti and Al as a result of the decomposition of the Ti 2 AlC particles. Crack healing was studied at 800, 900, and 1000°C for 0.25, 1, 4, and 16 hours, and the strength recovery was measured by 4‐point bending. Upon indentation, the bending strength of the samples dropped by about 50% from 402 ± 35 to 229 ± 14 MPa. This bending strength increased to about 90% of the undamaged material after annealing at 1000°C for just 15 minutes, while full strength was recovered after annealing for 1 hour. As the healing temperature was reduced to 900 and 800°C, the time required for full‐strength recovery increased to 4 and 16 hours, respectively. The initial bending strength and the fracture toughness of the composite material were found to be about 19% lower and 20% higher than monolithic alumina, respectively, making this material an attractive substitute for monolithic alumina used in high‐temperature applications.
- Open Access
- 4 January 2018
- Published by Springer Nature in Journal of Materials Science
- Vol. 53 (8) , 5973-5986
The effect of the TiC particle size on the preferred oxidation temperature for self-healing of oxide ceramic matrix materials
- 4 January 2018
- Published by Springer Nature in Journal of Materials Science
- Vol. 53 (8) , 5973-5986
Open AccessThe effect of the TiC particle size on the preferred oxidation temperature for self-healing of oxide ceramic matrix materials