Abstract
The intrinsic kinetics of hydrogen reduction of molten FeO were investigated under container-free conditions using aerodynamic levitation. The hydrogen reduction rate (𝑣red) was determined by quantitatively separating oxygen loss due to reduction from that caused by evaporation through time-resolved volume measurements of levitated droplets.Exposure to Ar–H2 mixtures led to progressive hydrogen reduction, with 𝑣red increasing with hydrogen partial pressure (𝑃H2). Droplets with an initial oxygen content of 22.2 mass% exhibited a linear 𝑣red–𝑃H2 relationship over the investigated range (0.08–0.43 atm), indicating continuous surface coverage by molten FeO. In contrast, droplets with 14.9 mass% initial oxygen content showed saturation-like behavior at high 𝑃H2, reflecting the limited availability of molten FeO to maintain a fully active reaction interface.Gas-side mass-transfer coefficients were evaluated using the Ranz–Marshall Sherwood correlation, enabling the separation of gas-phase transport from intrinsic surface-reaction kinetics through a resistance-in-series analysis. Arrhenius analysis of the intrinsic reaction rate constant (𝑘c) revealed two temperature regimes: intrinsic surface-reaction control at 1745–1835 K with an activation energy of 156 kJ·mol⁻¹ and mixed control at higher temperatures influenced by limitations in molten FeO availability.