Yusaku Seimiya
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Yusaku Seimiya has a total of 27 co-authors. Here are the top co-authors by number of shared publications:
- Shumpei Ozawa
Department of Advanced Materials Science and Engineering, Chiba Institute of Technology
6 shared publications - Takehiko Ishikawa
Japan Aerospace Exploration Agency
4 shared publications - Chihiro Koyama
Human Spaceflight Technology Directorate, Japan Aerospace Exploration Agency (JAXA), Tsukuba, Japan
2 shared publications - Hidekazu Kobatake
Department of Science of Environmental and Mathematical Modeling, Graduate School of Science and Engineering, Doshisha University, Kyotanabe, Japan
2 shared publications - Jürgen Brillo
Deutsches Zentrum Für Luft- Und Raumfahrt (DLR), Institut Für Materialphysik Im Weltraum, Cologne, Germany
2 shared publications - Ken-Ichi Sugioka
Department of Mechanical Systems Engineering, Toyama Prefectural University
2 shared publications
Latest Publications
- Open Access
- 9 October 2026
- Published by Springer Nature in International Journal of Thermophysics
- Vol. 47 (10) , 170
Surface Tension of Molten Al–Si Alloys Measured by Electromagnetic Levitation: Comparison with Ideal- and Subregular-Solution Calculations
- 9 October 2026
- Published by Springer Nature in International Journal of Thermophysics
- Vol. 47 (10) , 170
Open AccessSurface Tension of Molten Al–Si Alloys Measured by Electromagnetic Levitation: Comparison with Ideal- and Subregular-Solution Calculations
- Open Access
- 21 September 2026
- Published by Springer Nature in International Journal of Thermophysics
- Vol. 47 (10) , 158
Density and Molar Volume of CaO–SiO2–FeO Melts Measured by Electrostatic Levitation Aboard the International Space Station
- 21 September 2026
- Published by Springer Nature in International Journal of Thermophysics
- Vol. 47 (10) , 158
Open AccessDensity and Molar Volume of CaO–SiO2–FeO Melts Measured by Electrostatic Levitation Aboard the International Space Station
- Open Access
- 15 September 2026
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 66 (10) , 1077-1086
Intrinsic Kinetics of Hydrogen Reduction of Molten FeO under Aerodynamic Levitation
The intrinsic kinetics of hydrogen reduction of molten FeO were investigated under container-free conditions using aerodynamic levitation. The hydrogen reduction rate (𝑣red) was determined by quantitatively separating oxygen loss due to reduction from that caused by evaporation through time-resolved volume measurements of levitated droplets.Exposure to Ar–H2 mixtures led to progressive hydrogen reduction, with 𝑣red increasing with hydrogen partial pressure (𝑃H2). Droplets with an initial oxygen content of 22.2 mass% exhibited a linear 𝑣red–𝑃H2 relationship over the investigated range (0.08–0.43 atm), indicating continuous surface coverage by molten FeO. In contrast, droplets with 14.9 mass% initial oxygen content showed saturation-like behavior at high 𝑃H2, reflecting the limited availability of molten FeO to maintain a fully active reaction interface.Gas-side mass-transfer coefficients were evaluated using the Ranz–Marshall Sherwood correlation, enabling the separation of gas-phase transport from intrinsic surface-reaction kinetics through a resistance-in-series analysis. Arrhenius analysis of the intrinsic reaction rate constant (𝑘c) revealed two temperature regimes: intrinsic surface-reaction control at 1745–1835 K with an activation energy of 156 kJ·mol⁻¹ and mixed control at higher temperatures influenced by limitations in molten FeO availability.
- 15 September 2026
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 66 (10) , 1077-1086
Open AccessIntrinsic Kinetics of Hydrogen Reduction of Molten FeO under Aerodynamic Levitation
The intrinsic kinetics of hydrogen reduction of molten FeO were investigated under container-free conditions using aerodynamic levitation. The hydrogen reduction rate (𝑣red) was determined by quantitatively separating oxygen loss due to reduction from that caused by evaporation through time-resolved volume measurements of levitated droplets.Exposure to Ar–H2 mixtures led to progressive hydrogen reduction, with 𝑣red increasing with hydrogen partial pressure (𝑃H2). Droplets with an initial oxygen content of 22.2 mass% exhibited a linear 𝑣red–𝑃H2 relationship over the investigated range (0.08–0.43 atm), indicating continuous surface coverage by molten FeO. In contrast, droplets with 14.9 mass% initial oxygen content showed saturation-like behavior at high 𝑃H2, reflecting the limited availability of molten FeO to maintain a fully active reaction interface.Gas-side mass-transfer coefficients were evaluated using the Ranz–Marshall Sherwood correlation, enabling the separation of gas-phase transport from intrinsic surface-reaction kinetics through a resistance-in-series analysis. Arrhenius analysis of the intrinsic reaction rate constant (𝑘c) revealed two temperature regimes: intrinsic surface-reaction control at 1745–1835 K with an activation energy of 156 kJ·mol⁻¹ and mixed control at higher temperatures influenced by limitations in molten FeO availability.
- Open Access
- 30 December 2024
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 64 (15) , 2253-2261
Thermophysical Properties of Molten Fe–Cu Alloy Measured Using the Electrostatic Levitation Furnace Aboard the International Space Station (ISS-ELF) under Microgravity Conditions
The thermophysical properties of molten Fe–Cu alloys, including density, surface tension, and viscosity, were measured using the electrostatic levitation furnace aboard the International Space Station (ISS-ELF) under microgravity conditions, which provided an environment that facilitated accurate measurements. The densities of the molten Fe–25at%Cu and Fe–50at%Cu alloys decreased linearly with increasing temperature, and higher copper compositions resulted in increased density. The surface tension of the molten alloys exhibited a unique up-convex temperature dependence curve that initially increased and then decreased as the temperature increased. Viscosity measurements indicated that the viscosity of the molten Fe–Cu alloys decreased with increasing temperature, following a quadratic curve, and that an increase in the copper composition resulted in lower viscosity.
- 30 December 2024
- Published by Iron and Steel Institute of Japan in ISIJ International
- Vol. 64 (15) , 2253-2261
Open AccessThermophysical Properties of Molten Fe–Cu Alloy Measured Using the Electrostatic Levitation Furnace Aboard the International Space Station (ISS-ELF) under Microgravity Conditions
The thermophysical properties of molten Fe–Cu alloys, including density, surface tension, and viscosity, were measured using the electrostatic levitation furnace aboard the International Space Station (ISS-ELF) under microgravity conditions, which provided an environment that facilitated accurate measurements. The densities of the molten Fe–25at%Cu and Fe–50at%Cu alloys decreased linearly with increasing temperature, and higher copper compositions resulted in increased density. The surface tension of the molten alloys exhibited a unique up-convex temperature dependence curve that initially increased and then decreased as the temperature increased. Viscosity measurements indicated that the viscosity of the molten Fe–Cu alloys decreased with increasing temperature, following a quadratic curve, and that an increase in the copper composition resulted in lower viscosity.
- Open Access
- 6 July 2024
- Published by Springer Nature in Journal of Materials Science
- Vol. 59 (28) , 13183-13199
Density and surface tension of liquid Al, V and their binary alloys measured by electromagnetic levitation
Both density and surface tension were systematically investigated over a wide temperature and compositional range for the liquid Al–V alloy system. The thermophysical properties were measured in an electromagnetic levitation device. A linear decrease in surface tension and density with increasing temperature was observed for every alloy composition investigated. Additionally, a decrease in density and surface tension was observed for increasing aluminum content among the different probed samples. This decrease is, a strong deviation from an ideal mixing behavior which was experienced for both properties. Different models, including variants of the well-established Butler model, were employed to better describe the compositional dependence of density and surface tension in the liquid Al–V system. The advantages and disadvantages were discussed for each model describing the measured thermophysical property data. Strong similarities were observed when comparing the mixing behavior and segregation effects of the investigated Al–V system with already established works for the liquid Al–Ti system. The results suggest that both vanadium and titanium show similar mixing behavior when alloyed with aluminum.
- 6 July 2024
- Published by Springer Nature in Journal of Materials Science
- Vol. 59 (28) , 13183-13199
Open AccessDensity and surface tension of liquid Al, V and their binary alloys measured by electromagnetic levitation
Both density and surface tension were systematically investigated over a wide temperature and compositional range for the liquid Al–V alloy system. The thermophysical properties were measured in an electromagnetic levitation device. A linear decrease in surface tension and density with increasing temperature was observed for every alloy composition investigated. Additionally, a decrease in density and surface tension was observed for increasing aluminum content among the different probed samples. This decrease is, a strong deviation from an ideal mixing behavior which was experienced for both properties. Different models, including variants of the well-established Butler model, were employed to better describe the compositional dependence of density and surface tension in the liquid Al–V system. The advantages and disadvantages were discussed for each model describing the measured thermophysical property data. Strong similarities were observed when comparing the mixing behavior and segregation effects of the investigated Al–V system with already established works for the liquid Al–Ti system. The results suggest that both vanadium and titanium show similar mixing behavior when alloyed with aluminum.
- Open Access
- 1 January 2023
- Published by Walter de Gruyter GmbH in High Temperature Materials and Processes
- Vol. 42 (1)
Round-robin measurement of surface tension of high-temperature liquid platinum free of oxygen adsorption by oscillating droplet method using levitation techniques
Round-robin measurement of surface tension of high-temperature liquid platinum was conducted free of any contamination from the supporting materials and oxygen adsorption, using an electrostatic levitator (ESL), two electromagnetic levitator (EML), and an aerodynamic levitator (ADL). The measured temperature dependences of the surface tension using ESL and two EMLs were in good agreement and were expressed as σ = 1,798 ± 74.3 − ( 0.12 ± 0.0445 ) × ( T − 2,041 ) \sigma =\mathrm{1,798}\pm 74.3-(0.12\pm 0.0445)\times (T-\mathrm{2,041}) [10 –3 N·m –1 ] (1,900–2,600 K). However, the surface tension values measured with ADL were slightly lower than those exceeding the uncertainty of the measurement plots at high temperatures.
- 1 January 2023
- Published by Walter de Gruyter GmbH in High Temperature Materials and Processes
- Vol. 42 (1)
Open AccessRound-robin measurement of surface tension of high-temperature liquid platinum free of oxygen adsorption by oscillating droplet method using levitation techniques
Round-robin measurement of surface tension of high-temperature liquid platinum was conducted free of any contamination from the supporting materials and oxygen adsorption, using an electrostatic levitator (ESL), two electromagnetic levitator (EML), and an aerodynamic levitator (ADL). The measured temperature dependences of the surface tension using ESL and two EMLs were in good agreement and were expressed as σ = 1,798 ± 74.3 − ( 0.12 ± 0.0445 ) × ( T − 2,041 ) \sigma =\mathrm{1,798}\pm 74.3-(0.12\pm 0.0445)\times (T-\mathrm{2,041}) [10 –3 N·m –1 ] (1,900–2,600 K). However, the surface tension values measured with ADL were slightly lower than those exceeding the uncertainty of the measurement plots at high temperatures.
- Open Access
Round-Robin Measurement of Surface Tension for Liquid Titanium by Electromagnetic Levitation (EML) and Electrostatic Levitation (ESL)
To accurately measure the surface tension of liquid titanium free of contamination from chemical reaction with the supporting materials and dissolution of atmospheric oxygen, the measurement was performed by using electromagnetic levitation (EML) and electrostatic levitation (ESL) in consideration of the influence of oxygen partial pressure of the measurement atmosphere, . When liquid titanium was maintained at 2000 K under Ar–He gas with of 10 Pa flowing at 2 L·min−1 using EML, the surface tension decreased with time due to the dissolution of atmospheric oxygen into the sample. When the of the gas was decreased to 10−2 Pa, the oxygen content and the surface tension were confirmed to not vary, even after 120 min. Even though further decreased to 10−11 Pa under Ar–He–H2 gas, the surface tension slightly increased with time due to gas phase equilibrium between H2 and H2O that allowed for a continuous dissolution of atmospheric oxygen into the liquid titanium. The surface tension of liquid titanium measured by ESL, which prevents contamination of the sample from supporting materials and the high 10−5 Pa vacuum inhibits the dissolution of oxygen, showed almost the same value as that measured under Ar–He gas at of 10−2 Pa by EML. From the measurement results of EML and ESL, the surface tension of the 99.98 mass % pure liquid titanium, free from any contaminations from chemical reactions, with the supporting material and dissolved oxygen was expressed as (10−3 N·m−1).Open AccessRound-Robin Measurement of Surface Tension for Liquid Titanium by Electromagnetic Levitation (EML) and Electrostatic Levitation (ESL)
To accurately measure the surface tension of liquid titanium free of contamination from chemical reaction with the supporting materials and dissolution of atmospheric oxygen, the measurement was performed by using electromagnetic levitation (EML) and electrostatic levitation (ESL) in consideration of the influence of oxygen partial pressure of the measurement atmosphere, . When liquid titanium was maintained at 2000 K under Ar–He gas with of 10 Pa flowing at 2 L·min−1 using EML, the surface tension decreased with time due to the dissolution of atmospheric oxygen into the sample. When the of the gas was decreased to 10−2 Pa, the oxygen content and the surface tension were confirmed to not vary, even after 120 min. Even though further decreased to 10−11 Pa under Ar–He–H2 gas, the surface tension slightly increased with time due to gas phase equilibrium between H2 and H2O that allowed for a continuous dissolution of atmospheric oxygen into the liquid titanium. The surface tension of liquid titanium measured by ESL, which prevents contamination of the sample from supporting materials and the high 10−5 Pa vacuum inhibits the dissolution of oxygen, showed almost the same value as that measured under Ar–He gas at of 10−2 Pa by EML. From the measurement results of EML and ESL, the surface tension of the 99.98 mass % pure liquid titanium, free from any contaminations from chemical reactions, with the supporting material and dissolved oxygen was expressed as (10−3 N·m−1). - Open Access
- 23 March 2022
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 131 (12) , 129902
Erratum: “Influence of oxygen adsorption from atmosphere on surface tension of liquid silicon” [J. Appl. Phys. 130, 135101 (2021)]
- 23 March 2022
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 131 (12) , 129902
Open AccessErratum: “Influence of oxygen adsorption from atmosphere on surface tension of liquid silicon” [J. Appl. Phys. 130, 135101 (2021)]