Comparative evaluation of fracture resistance of different CAD/CAM fabricated endocrowns - in vitro study
Author:
Open Access
- 1 October 2023
- journal article
- research article
- Published by Egyptian Knowledge Bank in Egyptian Dental Journal
- Vol. 69 (4) , 2917-2922
Abstract
Background: The aim of the study was to compare the fracture resistance of recent CAD/CAM restorative materials that recently used for the fabrication of endocrown restorations.Methods: 30 endocrowns were fabricated on 3D printed resin dies and divided into three groups (n=10) according to the endocrown material. Group A: lithium disilicate Endocrowns (IPS E-max CAD), Group B: resin infiltrated ceramic (Vita Enamic), and group C: Nanohybrid composite (Brilliant Crios). All endocrowns were subjected to axial compressive strength using a universal testing machine, until failure, and the values were recorded. Fracture resistance values in Newton (N) and failure modes of the restorations were evaluated using an optical microscope. All collected data were tabulated and statistically analyzed. Numerical data were described as mean and standard deviation and compared using a Two-way ANOVA test. The level of significance was set at α P≤0.05.Results: fracture resistance values of all tested materials were within the acceptable clinical range for all groups. The lithium disilicates endocrowns showed statistically significantly higher mean fracture resistance values than the polymer infiltrated and nanohybrid composite endocrowns. While the nanohybrid composite Endocrowns showed better mode of fracture than that of lithium disilicate. Conclusions: Within the limitations of this study, Emax endocrowns showed better fracture resistance followed by Vita enamic endocrowns. While brilliant crios Endocrowns revealed a better mode of failure despite it’s low fracture resistance values.Keywords
This publication has 12 references indexed in Scilit:
- MARGINAL ADAPTATION AND FRACTURE RESISTANCE OF ENDOCROWN RESTORATIONS CONSTRUCTED FROM TWO CAD/CAM BLOCKS.Egyptian Dental Journal, 2021
- Fracture resistance and failure modes of endocrowns manufactured with different CAD/CAM materials under axial and lateral loadingJournal of Esthetic and Restorative Dentistry, 2019
- Marginal Fit Comparison of CAD/CAM Crowns Milled from Two Different MaterialsJournal of Prosthodontics, 2017
- Effect of Endocrown Pulp Chamber Extension Depth on Molar Fracture ResistanceOperative Dentistry, 2017
- Edge chipping resistance and flexural strength of polymer infiltrated ceramic network and resin nanoceramic restorative materialsThe Journal of Prosthetic Dentistry, 2016
- Effect of the Crystallization Process on the Marginal and Internal Gaps of Lithium Disilicate CAD/CAM CrownsBioMed Research International, 2016
- Comparison of mechanical properties of three machinable ceramics with an experimental fluorophlogopite glass ceramicThe Journal of Prosthetic Dentistry, 2015
- Evaluation of failure risks in ceramic restorations for endodontically treated premolar with MOD preparationDental Materials, 2011
- Stress distributions in adhesively cemented ceramic and resin-composite Class II inlay restorations: a 3D-FEA studyDental Materials, 2004
- Fracture strength and survival rate of endodontically treated maxillary incisors with approximal cavities after restoration with different post and core systems: an in-vitro studyJournal of Dentistry, 2001