Open Access
Abstract
Conventional material aging and testing protocols involve exposing coupon samples to saturation in application fluid(s) at temperature and pressure conditions typically encountered during service, followed by mechanical testing at ambient conditions. This practice can generate misleading results for materials for which fluid ingress is rapidly reversible, most notably at elevated temperatures. A recently developed in situ punch–shear device has been successfully used to establish experimental correlations between the tensile properties (ASTM D638) and shear properties (ASTM D732) of Polyethylene of Raised Temperature (PERT) under dry conditions. It also enabled measurement of shear properties of select polymers while immersed (saturated) in fluids at elevated pressure and temperature. The present work extends the treatment to a suite of commercially available thermoplastic polymers spanning the commodity, engineering, and high-performance polymer grades with varying degrees of hygroscopicity. The objectives of this contribution are three-fold, namely: (i) assess the effect of sample preparation method on measured mechanical properties, (ii) compare the experimentally established correlations between shear and tensile tests for the different class of polymer grades before fluid exposure, and (iii) gauge reversibility of the measured tensile and shear properties after aging in deionized water to saturation at 95 °C. Results indicate that (i) the test coupon preparation method affects the tensile to shear correlation and must be standardized to enable systematic comparison of in situ properties, (ii) individual correlations segregate by polymer family, and (iii) conventional tensile testing after a saturation–dehydration cycle yields optimistic mechanical properties.Keywords
Funding Information
- Mitacs (IT28258, ALLRP 568487–21)
- Natural Sciences and Engineering Research Council of Canada (NSERC) (IT28258, ALLRP 568487–21)
This publication has 25 references indexed in Scilit:
- Effects of polypropylene compositions and processing conditions on its aging resistance under tropical environmentsPolymer Degradation and Stability, 2024
- The aging behavior of HDPE pipe bodies and butt-fusion welded joints: effects of thermal oxidative and hydrothermal accelerated agingMechanics of Time-Dependent Materials, 2024
- Degradation and characterization methods for polyethylene gas pipes after natural and accelerated agingPolymer Degradation and Stability, 2022
- In Situ Testing of Polymers Immersed in Aging Fluids at Elevated Temperature and PressureMaterials, 2022
- Investigation on thermal degradation mechanism of poly(phenylene sulfide)Polymer Degradation and Stability, 2022
- Aging of Polyethylene of Raised Temperature Resistance Pipe Liner After a Four-Year Service in a Crude Oil Gathering SystemJournal of Failure Analysis and Prevention, 2021
- Composite Material Recycling Technology—State-of-the-Art and Sustainable Development for the 2020sJournal of Composites Science, 2021
- Ageing of polyethylene at raised temperature in contact with chlorinated sanitary hot water. Part I – Chemical aspectsPolymer Degradation and Stability, 2012
- Polyethylene yielding behaviour: What is behind the correlation between yield stress and crystallinity?Polymer, 2009
- Polypropylene natural aging studied by X-ray photoelectron spectroscopyJournal of Electron Spectroscopy and Related Phenomena, 2000