Abstract
A method was proposed for increasing the oxidation resistance of promising wrought Ti2AlNb ortho-alloys by depositing γ-TiAl-based coatings. Using original vacuum pulse-arc melting of 100 μm thick granule layers, coatings with different Al/Ti ratios and a thickness of 50–60 µm were obtained on the surface of the Ti50Al25Nb25 alloy. Granules Ti50Al44Nb4.9Mo1B0.1 (at.%), 20–60 μm in size, were employed. To vary Al content, initial granules and their mixture with Al powder were used. Excellent adhesion of the coatings is ensured by the similar chemical composition and structure of the substrate and coatings, as well as micro-metallurgical reactions between granules and the substrate that occur during treatment. The resulting coatings had a submicron gradient structure consisting of TiAl and Ti3Al intermetallic compounds. During oxidation at 850 °C for 10 h, an oxide layer consisting of a mixture of α-Al2O3, TiO2, and AlNbO4 was formed on the coating surfaces. With an increase in the annealing duration to 100 h, a dense α-Al2O3 oxide layer, approximately 0.5 µm thick, was formed over the primary oxide mixture, the quality of which was higher in coatings enriched with aluminum.Keywords
Funding Information
- Russian Science Foundation (22-29-00757)
This publication has 44 references indexed in Scilit:
- Thermal barrier coatings on γ-TiAl protected by the halogen effectSurface and Coatings Technology, 2012
- Oxidation Behavior and Related Issues2011
- Light-Weight Intermetallic Titanium Aluminides – Status of Research and DevelopmentAdvanced Materials Research, 2011
- Grain refinement by low boron additions in niobium-rich TiAl-based alloysIntermetallics, 2008
- High temperature corrosion mechanisms of certain new TiAl-based intermetallic alloys in an aggressive H2/H2O/H2S environment at 850°CCorrosion Science, 2007
- Formation of silicide coatings on the surface of a TiAl-based alloy and improvement in oxidation resistanceMaterials Science and Engineering: A, 2005
- Sulfidation properties of TiAl–2 at.% X (X=Si, Mn, Ni, Ge, Y, Zr, La and Ta) alloys at 1173 K and 1.3 Pa sulfur pressure in an H2S–H2 gas mixtureIntermetallics, 2002
- Formation of fcc titanium during heating high energy ball milled Al–Ti powdersMaterials Letters, 2002
- The intermetallic Ti2AlNbProgress in Materials Science, 1997
- Fundamentals of TiAl oxidation – A critical reviewMaterials and Corrosion, 1995