Abstract
To improve silicon device fabrication processes, it is necessary to monitor bulk minority carrier lifetimes accurately, and this requires surface recombination to be well controlled and, ideally, minimized. Good surface passivation can result from thermal oxidation or by deposition of dielectrics (e.g., Al2O3, SiNx, and amorphous Si), but these forms of passivation can modify the lifetime of the material under investigation. Various schemes can passivate surfaces on a temporary basis without modifying the bulk, and, in this article, the virtues of the iodine–ethanol (I–E) temporary surface passivation scheme are explored. A procedure for preparing the wafer surfaces prior to passivation is developed. For the optimized pretreatment, a series of experiments on 3–5 Ω cm float‐zone wafers cut from the same ingot with different thicknesses is conducted. This enables the material's bulk lifetime to be measured at 1015 cm−3 injection as 46 ms, with the surface recombination velocity being 6.5 ± 0.3 cm s−1. I–E passivation is then compared to a recently developed superacid‐derived temporary passivation scheme. Although the latter is superior on (100)‐orientation substrates, I–E performs much better on (111)‐orientation substrates, making it a better choice for (111)‐orientation wafers, such as those used for power devices.Keywords
Funding Information
- Engineering and Physical Sciences Research Council (EP/M024911/1, EP/J01768X/2, EP/R511808/1, EP/N509796/1)
This publication has 32 references indexed in Scilit:
- Improved quantitative description of Auger recombination in crystalline siliconPhysical Review B, 2012
- A comparative study of silicon surface passivation using ethanolic iodine and bromine solutionsSolar Energy Materials and Solar Cells, 2012
- Determination of Grain Orientations in Multicrystalline Silicon by ReflectometryJournal of the Electrochemical Society, 2010
- Chemical Modification and Patterning of Iodine-Terminated Silicon Surfaces Using Visible LightThe Journal of Physical Chemistry B, 2002
- Effectiveness of 0.08 molar iodine in ethanol solution as a means of chemical surface passivation for photoconductance decay measurementsSolar Energy Materials and Solar Cells, 1997
- Effect of Steady Bias Light on Carrier Lifetime in Silicon Wafers with Chemically Passivated SurfacesJapanese Journal of Applied Physics, 1996
- Monitoring and Optimization of Silicon Surface QualityJournal of the Electrochemical Society, 1995
- Electronic passivation of silicon surfaces by halogensJournal of Electronic Materials, 1994
- In situ bulk lifetime measurement on silicon with a chemically passivated surfaceApplied Surface Science, 1993
- Unusually Low Surface-Recombination Velocity on Silicon and Germanium SurfacesPhysical Review Letters, 1986