Abstract
Luminescence dosimetry continues to advance through efforts to improve detector sensitivity, stability, and cost‑effectiveness. Within this scope, Al2O3 crystals were produced by the flux‑growth method, a low‑cost crystal growth technique, using MoO3 precursors with purities from 99.0% to 99.95%, and Al2O3 of 99.99% and 99.999% purity. Elemental characterization was pursued using µ-PIXE and PIGE. The thermoluminescence (TL) and optically stimulated luminescence (OSL) characteristic response to 90Sr/90Y β-radiation over the dose range of 30 mGy to 15 Gy was investigated, with emphasis on the role of precursor purity, using the Risø-DA20 reader. Variations in MoO3 purity resulted in differences in trap distribution, reflected in both TL and OSL behavior. All samples showed supralinear TL and OSL dose‑response without saturation within the studied range and demonstrated high signal reproducibility (< 5%). Increasing MoO3 purity led to substantial improvements in TL/OSL intensity and low‑dose sensitivity, with 99.95% purity providing the best performance-cost balance. The results confirm that precursor purity is a critical parameter controlling luminescence efficiency in flux‑grown sapphire. Overall, the flux‑growth method emerges as a promising and economically attractive route for producing Al2O3 dosimetric materials, including for low‑dose applications, using the appropriate starting materials. Further optimization of growth conditions or targeted doping strategies may enable additional improvements in detector sensitivity and performance.