Fracture resistance of glazed, full-contour ZLS incisor crowns
- 1 July 2017
- journal article
- research article
- Published by Japan Prosthodontic Society in Journal of Prosthodontic Research
- Vol. 61 (3) , 344-349
Abstract
To compare the failure behaviour of zirconia-reinforced lithium silicate (Celtra Duo, DeguDent) with that of lithium disilicate (IPS e.max CAD, Ivoclar Vivadent) and feldspar (Mark II, VITA) ceramics. Three groups of sixteen glazed maxillary incisor crowns were produced. The inner surfaces of the crowns were etched, then luted to metal dies with self-adhesive cement. Single load-to-failure tests were performed before and after thermo-mechanical ageing. To simulate clinical conditions, the specimens were thermocycled (10,000 cycles between 6.5°C and 60°C) and underwent chewing simulation (1,200,000 cycles, Fmax=86N). Statistical analyses were performed by use of non-parametric Kruskal-Wallis and Mann-Whitney U-tests. Before ageing, all the monolithic incisor crowns fractured at test forces >285N. Mean fracture loads were highest for zirconia-reinforced lithium silicate (725N, SD 162N), slightly lower for lithium disilicate (701N, SD 276N), and lowest for feldspar (554N, SD 190N). The differences between the results were not statistically significant. After ageing, fracture resistance decreased for all materials except zirconia-reinforced lithium silicate. Mean fracture loads were highest for zirconia-reinforced lithium silicate (766N, SD 98N) and significantly lower for both lithium disilicate (485N, SD 64N) and feldspar (372N, SD 116N). Monolithic restorations fabricated from zirconia-reinforced lithium silicate retain high fracture resistance after extensive thermo-mechanical ageing. This preclinical study suggests that cohesive failures of monolithic anterior crowns produced of these ceramics will not be a major problem in dental practice.Keywords
This publication has 18 references indexed in Scilit:
- Clinical outcomes of lithium disilicate single crowns and partial fixed dental prostheses: A systematic reviewThe Journal of Prosthetic Dentistry, 2014
- Fracture Resistance of a Selection of Full-Contour All-Ceramic Crowns: An In Vitro StudyThe International Journal of Prosthodontics, 2014
- Chair-side generated posterior lithium disilicate crowns after 4 yearsClinical Oral Investigations, 2012
- Clinical results of lithium-disilicate crowns after up to 9 years of serviceClinical Oral Investigations, 2012
- Chipping behaviour of all-ceramic crowns with zirconia framework and CAD/CAM manufactured veneerJournal of Dentistry, 2012
- Effect of firing protocols on cohesive failure of all-ceramic crownsJournal of Dentistry, 2010
- A Clinical Evaluation of Chairside Lithium Disilicate CAD/CAM CrownsThe Journal of the American Dental Association, 2010
- Fracture Loads of All‐Ceramic Crowns under Wet and Dry Fatigue ConditionsJournal of Prosthodontics, 2009
- Fracture load of composite resin and feldspathic all-ceramic CAD/CAM crownsThe Journal of Prosthetic Dentistry, 2006
- A three-dimensional mathematical model of the human masticatory system predicting maximum possible bite forcesJournal of Biomechanics, 1988