The Effect of Finish Line Design on the Fracture Strength of Zirconia Copings.
Open Access
- 1 December 2019
- journal article
- Vol. 20 (4) , 271-275
Abstract
One of the major concerns about all ceramic crowns is their fracture resistance. The purpose of this in vitro study was to evaluate the effect of two marginal designs (shoulder 90°, shoulder 135°) on the fracture resistance of zirconia copings. In this in vitro study, 20 brass dies were prepared using milling machine: 10 with 1mm width shoulder 90° marginal design and the other 10 with 1mm width shoulder 135° finish line design. Zirconia cores with 0.5mm thickness and 30μm cement space were fabricated on brass dies. The copings were cemented on the dies and fracture test was done using a universal testing machine. Data were analyzed using Mann-Whitney test. The mean value of fracture resistance for shoulder 90° finish line design were 368.3±109.4 N and for shoulder 135° finish line design were 518.4±115.5 N. Data analysis revealed a statistically significant difference between groups (p< 0.05). The results of this study showed that the finish line design of zirconia copings influences their fracture resistance. A 135° shoulder finish line design can improve the fracture resistance of zirconia crowns.Keywords
This publication has 15 references indexed in Scilit:
- Marginal Adaptation, Gap Width, and Fracture Strength of Teeth Restored With Different All-Ceramic Vs Metal Ceramic Crown Systems: An in Vitro Study.2016
- Comparison of Marginal Fit and Fracture Strength of a CAD/CAM Zirconia Crown with Two Preparation Designs2015
- The Effect of Preparation Design on the Fracture Resistance of Zirconia Crown Copings (Computer Associated Design/Computer Associated Machine, CAD/CAM System)2011
- The effect of two marginal designs (chamfer and shoulder) on the fracture resistance of all ceramic restorations, Inceram: An in vitro studyJournal of Prosthodontic Research, 2011
- The effect of finish line preparation and layer thickness on the failure load and fractography of ZrO2 copingsThe Journal of Prosthetic Dentistry, 2008
- Effect of margin design on the fracture resistance of Procera all ceram cores: an in vitro study.2008
- Survival of resin-bonded porcelain veneer crowns placed with and without metal reinforcementJournal of Dentistry, 2006
- Clinical considerations for densely sintered alumina and zirconia restorations: Part 1.2005
- Survival of In-Ceram crowns in a private practice: A prospective clinical trialThe Journal of Prosthetic Dentistry, 2000
- Using posterior composites appropriately.1992