Wear behaviour of hardfaced Fe-Cr-C alloy and austenitic steel under 2-body and 3-body conditions at elevated temperature
Authors:
- E. BadischEBE. Badisch
- C. KatsichCKC. Katsich
- H. WinkelmannHWH. Winkelmann
- F. FranekFFF. Franek
- Manish RoyMRManish Roy
- 1 July 2010
- journal article
- Published by Elsevier in Tribology International
- Vol. 43 (7) , 1234-1244
Abstract
No abstract availableKeywords
This publication has 34 references indexed in Scilit:
- The Solid Particle Erosion Behavior of Carbon/Carbon and Carbon/Phenolic Composite Used in Re-entry VehiclesTribology Transactions, 2009
- The comparison of wear properties of different Fe‐based hardfacing alloys in four kinds of testing methodsTribotest, 2008
- Influence of hardness on the wear resistance of 17-4 PH stainless steel evaluated by the pin-on-disc testingJournal of Materials Processing Technology, 2008
- Abrasion resistance of ductile iron austempered by the two-step processMaterials Science and Engineering: A, 2008
- Elevated temperature erosive wear of metallic materialsJournal of Physics D: Applied Physics, 2006
- A comparison of elevated temperature erosion resistance of four new HVCC coatings with other wire sprayed coatingsJournal of Materials Processing Technology, 2004
- Effect of aging on the microstructure and toughness of the interface zone of a gas tungsten arc (GTA) synthesized Fe–Cr–Si–Mo–C coated low carbon steelSurface and Coatings Technology, 2002
- Developing extreme hardness (>15GPa) in iron based nanocompositesComposites Part A: Applied Science and Manufacturing, 2002
- Reactions in the matrix and interface of the Fe–SiC metal matrix composite systemMaterials Science and Engineering: A, 1999
- High temperature erosion behavior tungsten- and chromium-carbide-based coatingsSurface and Coatings Technology, 1987