Effect of Temperature on Thermal Oxidation Behavior of Ti-6Al-4V ELI Alloy
Open Access
Abstract
In this paper, the morphological, micromechanical and tribological characteristics of the Ti-6Al-4V ELI alloy after thermal oxidation (TO) were identified. TO was carried out at temperatures of 848 K, 898 K and 948 K over a period of 50 h. Microscopic examination revealed that an increase in temperature resulted in an improved uniformity of coverage and an increased oxide grain size. Micromechanical tests showed that TO of the Ti-6Al-4V ELI alloy led to an increase in hardness and deformation resistance. Following oxidation, a decrease (by approximately 10–22%) was observed in the total mechanical work of indentation, Wtotal, compared to the as-received material. The formation of protective oxide films on the Ti-6Al-4V ELI alloy also led to the improvement of tribological characteristics, both when tested under dry friction conditions and in Ringer’s solution. The sliding wear resistance increased with an increase in the oxidation temperature. However, a greater degree of wear reduction (by approximately 30–50%) was found for the lubricated contact in comparison with the dry friction tests. Surface roughness also increased with the increase in temperature.Keywords
This publication has 30 references indexed in Scilit:
- Corrosion behaviors of TA2 and TA36 titanium alloys in a high-sulfur environmentInternational Journal of Electrochemical Science, 2024
- Effect of thermal oxidation on the dry sliding friction and wear behaviour of CP-Ti on CP-Ti tribopairsSurface Science and Technology, 2023
- Titanium: An Overview of Resources and Production MethodsMinerals, 2021
- Improving the Adhesion of a Hard Oxide Layer on Ti6Al4V by a Three‐Step Thermal Oxidation ProcessAdvanced Engineering Materials, 2021
- Indentation Modulus, Indentation Work and Creep of Metals and Alloys at the Macro-Scale Level: Experimental Insights into the Use of a Primary Vickers Hardness Standard MachineMaterials, 2021
- Mechanical Properties, Corrosion Resistance and Bioactivity of Oxide Layers Formed by Isothermal Oxidation of Ti-6Al-7Nb AlloyCoatings, 2021
- Opportunities and Issues in the Application of Titanium Alloys for Aerospace ComponentsMetals, 2020
- Surface medication of Ti–15Mo alloy by thermal oxidation: Evaluation of surface characteristics and corrosion resistance in Ringer's solutionApplied Surface Science, 2015
- Tribological Behaviour of Orthopaedic Ti-13Nb-13Zr and Ti-6Al-4V AlloysTribology Letters, 2010
- Multilaboratory tribotesting: Results from the Versailles Advanced Materials and Standards programme on wear test methodsWear, 1987