Abstract
This paper presents measurement reproducibility on multiple 2” wafers of high-purity semi-insulating 4H SiC. First, ten unthinned wafers with a thickness around 370 μm were measured, resulting in a dielectric constant of 9.745 ± 0.001 and a loss tangent of (1.84 ± 0.09)∙10−5∙[1 + (2.4 ± 0.1)∙10−11∙f], where f is the frequency in Hz. Next, five of these wafers were thinned to 100 μm and remeasured, resulting in a dielectric constant of 9.77 ± 0.01 and a loss tangent of (1.3 ± 0.2)∙10−5∙[−1 + (4.8 ± 0.9)∙10−11∙f]. The relatively small standard deviation indicates high reproducibility of measurements as well as wafer uniformity. The weak thickness dependence indicates weak surface effect. The present results on 100-μm-thick 2” wafers are remarkably consistent with previous results on 100-μm-thick 100-mm wafers, even though previously each 100-mm wafer needed to be quartered to fit the measurement setup.
Funding Information
  • National Science Foundation (ECCS-2117305)
  • National Science Foundation (ECCS-2132323)
  • U.S. Army (W911NF2410023)
  • U.S. Army (W911NF2510002)
  • U.S. Army (W911NF25P0005)
  • Superior Energy-efficient Materials and Devices (SUPREME), one of the Seven Centers
  • Semiconductor Research Corporation and U.S. Defense Advanced Projects Agency through the Joint University Microelectronics Program 2.0 (2023-JU-3137)
  • U.S. Department of Defense through the Northeast Regional Defense Technology Hub (NORDTECH) Microelectronics Commons Hub (N00164-23-9-G061)
  • Cornell NanoScale Facility, a National Nanotechnology Coordinated Infrastructure (NNCI) Member
  • National Science Foundation (NNCI- 1542081)