Yoshiyuki Yanagimoto
Research Subjects
Yoshiyuki Yanagimoto has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- James C. M. Hwang
Cornell University
3 shared publications - Chunyi Li
Department of Materials Science and Engineering, Cornell University, Ithaca, NY, USA
2 shared publications Shana Yanagimoto
EM labs, Inc., Kobe, Japan
2 shared publications- Shana Yanagimoto
EM Labs Inc., Kobe, Hyogo, Japan
2 shared publications - Haonan Liu
Department of Chemical Science and Engineering, Institute of Science Tokyo, 2-12-1-E4-5 Ookayama, Meguro-Ku, Tokyo 152-8552, Japan
1 shared publication - James Grandusky
Crystal IS Inc
1 shared publication
Latest Publications
- 8 May 2026
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Instrumentation and Measurement
- Vol. 75 (00189456) , 6003508
Reproducible Permittivity Measurement Above 110 GHz of Ultralow-Loss High-Purity Semi-Insulating 4H-SiC 2-in Wafers
This paper presents measurement reproducibility on multiple 2” wafers of high-purity semi-insulating 4H SiC. First, ten unthinned wafers with a thickness around 370 μm were measured, resulting in a dielectric constant of 9.745 ± 0.001 and a loss tangent of (1.84 ± 0.09)∙10−5∙[1 + (2.4 ± 0.1)∙10−11∙f], where f is the frequency in Hz. Next, five of these wafers were thinned to 100 μm and remeasured, resulting in a dielectric constant of 9.77 ± 0.01 and a loss tangent of (1.3 ± 0.2)∙10−5∙[−1 + (4.8 ± 0.9)∙10−11∙f]. The relatively small standard deviation indicates high reproducibility of measurements as well as wafer uniformity. The weak thickness dependence indicates weak surface effect. The present results on 100-μm-thick 2” wafers are remarkably consistent with previous results on 100-μm-thick 100-mm wafers, even though previously each 100-mm wafer needed to be quartered to fit the measurement setup.
- 8 May 2026
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Instrumentation and Measurement
- Vol. 75 (00189456) , 6003508
Reproducible Permittivity Measurement Above 110 GHz of Ultralow-Loss High-Purity Semi-Insulating 4H-SiC 2-in Wafers
This paper presents measurement reproducibility on multiple 2” wafers of high-purity semi-insulating 4H SiC. First, ten unthinned wafers with a thickness around 370 μm were measured, resulting in a dielectric constant of 9.745 ± 0.001 and a loss tangent of (1.84 ± 0.09)∙10−5∙[1 + (2.4 ± 0.1)∙10−11∙f], where f is the frequency in Hz. Next, five of these wafers were thinned to 100 μm and remeasured, resulting in a dielectric constant of 9.77 ± 0.01 and a loss tangent of (1.3 ± 0.2)∙10−5∙[−1 + (4.8 ± 0.9)∙10−11∙f]. The relatively small standard deviation indicates high reproducibility of measurements as well as wafer uniformity. The weak thickness dependence indicates weak surface effect. The present results on 100-μm-thick 2” wafers are remarkably consistent with previous results on 100-μm-thick 100-mm wafers, even though previously each 100-mm wafer needed to be quartered to fit the measurement setup.
- Open Access
- 29 October 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Microwaves
- Vol. 6 (1) , 229-237
Microwave and Millimeter-Wave Permittivities of Single-Crystal AlN, Including Thickness and Temperature Dependence
For electronic applications, polycrystal AlN has been widely used in packaging. Polycrystal AlN thin films with columnar grains have also been widely used in acoustic filters. Recently, with the availability of single-crystal AlN bulk wafers, transistors based on single-crystal AlN are emerging mainly because AlN has an ultrawide bandgap and high thermal conductivity. This makes AlN transistors especially attractive for high-power and high-frequency applications in harsh environments. To this end, single-crystal AlN wafers ≥ 2 inches in diameter have been in quantity production and commercially available, although their properties are not well characterized. This paper reports the microwave and millimeter-wave permittivities of single-crystal AlN, including its real and imaginary components. Using high-quality resonators of different bandwidths with meticulous care, the dielectric constant is found to be indeed constant at 7.805 ± 0.007 from 10 to 320 GHz, while the loss tangent increases linearly with frequency f according to (0.78 ± 0.01)·10−4·[1 + (2.22 ± 0.02)·10−11·f]. Across the frequency range measured, AlN exhibits lower loss than fused silica, a common low-loss dielectric. The four wafers measured show excellent uniformity with weak temperature dependence and little thickness dependence. Using a cylindrical resonator capable of temperature variation but with a narrow bandwidth around 10 GHz, the temperature coefficients of the dielectric constant and loss tangent are (6.1 ± 0.1)· (T − 300)·10−5 and (3.8 ± 0.1)·(T − 300)·10−3, respectively, where T is the absolute temperature in K. These characteristics confirm the potential of single-crystal AlN for high-power and high-frequency transistors in harsh environments.
- 29 October 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Microwaves
- Vol. 6 (1) , 229-237
Open AccessMicrowave and Millimeter-Wave Permittivities of Single-Crystal AlN, Including Thickness and Temperature Dependence
For electronic applications, polycrystal AlN has been widely used in packaging. Polycrystal AlN thin films with columnar grains have also been widely used in acoustic filters. Recently, with the availability of single-crystal AlN bulk wafers, transistors based on single-crystal AlN are emerging mainly because AlN has an ultrawide bandgap and high thermal conductivity. This makes AlN transistors especially attractive for high-power and high-frequency applications in harsh environments. To this end, single-crystal AlN wafers ≥ 2 inches in diameter have been in quantity production and commercially available, although their properties are not well characterized. This paper reports the microwave and millimeter-wave permittivities of single-crystal AlN, including its real and imaginary components. Using high-quality resonators of different bandwidths with meticulous care, the dielectric constant is found to be indeed constant at 7.805 ± 0.007 from 10 to 320 GHz, while the loss tangent increases linearly with frequency f according to (0.78 ± 0.01)·10−4·[1 + (2.22 ± 0.02)·10−11·f]. Across the frequency range measured, AlN exhibits lower loss than fused silica, a common low-loss dielectric. The four wafers measured show excellent uniformity with weak temperature dependence and little thickness dependence. Using a cylindrical resonator capable of temperature variation but with a narrow bandwidth around 10 GHz, the temperature coefficients of the dielectric constant and loss tangent are (6.1 ± 0.1)· (T − 300)·10−5 and (3.8 ± 0.1)·(T − 300)·10−3, respectively, where T is the absolute temperature in K. These characteristics confirm the potential of single-crystal AlN for high-power and high-frequency transistors in harsh environments.
- Open Access
- 20 September 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Microwaves
- Vol. 4 (4) , 666-674
Ordinary and Extraordinary Permittivities of 4H SiC at Different Millimeter-Wave Frequencies, Temperatures, and Humidities
Hexagonal semiconductors such as 4H SiC have important high-frequency, high-power, and high-temperature applications. The applications require accurate knowledge of both ordinary and extraordinary relative permittivities, ϵ ⊥ and ϵ || , perpendicular and parallel, respectively, to the c axis of these semiconductors. However, due to challenges for suitable test setups and precision high-frequency measurements, little reliable data exists for these semiconductors especially at millimeter-wave frequencies. Recently, we reported ϵ || of 4H SiC from 110 to 170 GHz. This paper expands on the previous report to include both ϵ ⊥ and ϵ || of the same material from 55 to 330 GHz, as well as their temperature and humidity dependence enabled by improving the measurement precision to two decimal points. For example, at room temperature, real ϵ ⊥ and ϵ || are constant at 9.77 ± 0.01 and 10.20 ± 0.05, respectively. By contrast, the ordinary loss tangent increases linearly with the frequency f in the form of (4.9 ± 0.1) × 10 −16 f . The loss tangent, less than 1 × 10 −4 over most millimeter-wave frequencies, is significantly lower than that of sapphire, our previous low-loss standard. Finally, both ϵ ⊥ and ϵ || have weak temperature coefficients on the order of 10 −4 /°C. The knowledge reported here is especially critical to millimeter-wave applications of 4H SiC, not only for solid-state devices and circuits, but also as windows for high-power vacuum electronics.
- 20 September 2024
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Microwaves
- Vol. 4 (4) , 666-674
Open AccessOrdinary and Extraordinary Permittivities of 4H SiC at Different Millimeter-Wave Frequencies, Temperatures, and Humidities
Hexagonal semiconductors such as 4H SiC have important high-frequency, high-power, and high-temperature applications. The applications require accurate knowledge of both ordinary and extraordinary relative permittivities, ϵ ⊥ and ϵ || , perpendicular and parallel, respectively, to the c axis of these semiconductors. However, due to challenges for suitable test setups and precision high-frequency measurements, little reliable data exists for these semiconductors especially at millimeter-wave frequencies. Recently, we reported ϵ || of 4H SiC from 110 to 170 GHz. This paper expands on the previous report to include both ϵ ⊥ and ϵ || of the same material from 55 to 330 GHz, as well as their temperature and humidity dependence enabled by improving the measurement precision to two decimal points. For example, at room temperature, real ϵ ⊥ and ϵ || are constant at 9.77 ± 0.01 and 10.20 ± 0.05, respectively. By contrast, the ordinary loss tangent increases linearly with the frequency f in the form of (4.9 ± 0.1) × 10 −16 f . The loss tangent, less than 1 × 10 −4 over most millimeter-wave frequencies, is significantly lower than that of sapphire, our previous low-loss standard. Finally, both ϵ ⊥ and ϵ || have weak temperature coefficients on the order of 10 −4 /°C. The knowledge reported here is especially critical to millimeter-wave applications of 4H SiC, not only for solid-state devices and circuits, but also as windows for high-power vacuum electronics.
- 3 June 2024
- Published by AIP Publishing in Applied Physics Letters
- Vol. 124 (23)
Frequency-dependent dielectric properties of aromatic polyimides in the 25–330 GHz range
The dielectric constants (Dk) and dissipation factors (Df) of 11 types of polyimides (PIs) were systematically measured between 25 and 330 GHz using Fabry–Pérot resonators. Herein, the relationships between their frequency dependence and chemical structure are discussed. As the frequency increased, all the PIs exhibited a continuous decrease in Dk and a consistent increase in Df. Notably, no distinct peaks were observed over the entire frequency range. The decrease in Dk with frequency gradually approached the square of the refractive index (n2) in the near-infrared region. Additionally, based on the correlation between the dielectric dispersion and dielectric polarization (Pt), Dk showed a stronger correlation with the electronic polarization (Pe) at higher frequencies than with the dipolar orientational polarization (Pd). Moreover, in fluorine-containing PIs, Dk declined faster with increasing frequency as the fluorine content (F%) increased. Meanwhile, the increase in Df showed a negative correlation with the weight fraction of polar groups (polar%), and the PIs containing –CF3 groups in the diamine moieties exhibited a similar rapid increase in Df with frequency, suggesting characteristic absorptions in the terahertz (THz) domain. These data will be beneficial for developing high-performance polymer-based insulating materials for 5th/6th generation wireless communication technologies.
- 3 June 2024
- Published by AIP Publishing in Applied Physics Letters
- Vol. 124 (23)
Frequency-dependent dielectric properties of aromatic polyimides in the 25–330 GHz range
The dielectric constants (Dk) and dissipation factors (Df) of 11 types of polyimides (PIs) were systematically measured between 25 and 330 GHz using Fabry–Pérot resonators. Herein, the relationships between their frequency dependence and chemical structure are discussed. As the frequency increased, all the PIs exhibited a continuous decrease in Dk and a consistent increase in Df. Notably, no distinct peaks were observed over the entire frequency range. The decrease in Dk with frequency gradually approached the square of the refractive index (n2) in the near-infrared region. Additionally, based on the correlation between the dielectric dispersion and dielectric polarization (Pt), Dk showed a stronger correlation with the electronic polarization (Pe) at higher frequencies than with the dipolar orientational polarization (Pd). Moreover, in fluorine-containing PIs, Dk declined faster with increasing frequency as the fluorine content (F%) increased. Meanwhile, the increase in Df showed a negative correlation with the weight fraction of polar groups (polar%), and the PIs containing –CF3 groups in the diamine moieties exhibited a similar rapid increase in Df with frequency, suggesting characteristic absorptions in the terahertz (THz) domain. These data will be beneficial for developing high-performance polymer-based insulating materials for 5th/6th generation wireless communication technologies.
- 8 March 2022
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Instrumentation and Measurement
- Vol. 71 (00189456) , 1-9
Permittivity Measurement Method for Thin Sheets Using Split-Cylinder Resonator With Protrusions
We propose a permittivity measurement method for a thin, low-loss sheet sample using a split-cylinder resonator (SCR) with protrusions. In the SCR, the TM 111 mode is separated from the TE 011 mode because the resonant frequency of the TM 111 mode is shifted toward a higher frequency band because of the protrusions. If an SCR does not have protrusions (or grooves), it is impossible to measure the permittivity of thin samples, which are commonly measured samples in the marketplace. When a sample is inserted between the flanges of the SCR with protrusions, the resonance curve of the TE 011 mode never overlaps with that of the TM 111 mode, and the permittivity of the sample is measurable until the resonance curve of the TE 011 mode overlaps with that of the TM 110 mode, where the resonant frequency of the TM 011 mode is much lower than that of the TE 011 mode. In addition, we newly derive an inequality that expresses a range for measurable permittivity based on the thickness of a sample and show that the range is much greater than that for an SCR with grooves. Moreover, we demonstrate the estimation accuracy for permittivity using a dimension correction method in which only the TE 011 mode is used, and we demonstrate that relative permittivity can be estimated within 0.3% over a permittivity range of less than 10 below 50 GHz if the real dimensions of the radius and length of an SCR have no deviation or deviate from the design dimension by the same ratio.
- 8 March 2022
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Instrumentation and Measurement
- Vol. 71 (00189456) , 1-9
Permittivity Measurement Method for Thin Sheets Using Split-Cylinder Resonator With Protrusions
We propose a permittivity measurement method for a thin, low-loss sheet sample using a split-cylinder resonator (SCR) with protrusions. In the SCR, the TM 111 mode is separated from the TE 011 mode because the resonant frequency of the TM 111 mode is shifted toward a higher frequency band because of the protrusions. If an SCR does not have protrusions (or grooves), it is impossible to measure the permittivity of thin samples, which are commonly measured samples in the marketplace. When a sample is inserted between the flanges of the SCR with protrusions, the resonance curve of the TE 011 mode never overlaps with that of the TM 111 mode, and the permittivity of the sample is measurable until the resonance curve of the TE 011 mode overlaps with that of the TM 110 mode, where the resonant frequency of the TM 011 mode is much lower than that of the TE 011 mode. In addition, we newly derive an inequality that expresses a range for measurable permittivity based on the thickness of a sample and show that the range is much greater than that for an SCR with grooves. Moreover, we demonstrate the estimation accuracy for permittivity using a dimension correction method in which only the TE 011 mode is used, and we demonstrate that relative permittivity can be estimated within 0.3% over a permittivity range of less than 10 below 50 GHz if the real dimensions of the radius and length of an SCR have no deviation or deviate from the design dimension by the same ratio.