Safe burst strength of a pipeline with dent–crack defect: Effect of crack depth and operating pressure
Authors:
- Hossein GhaedniaHGHossein Ghaednia
- Sreekanta DasSDSreekanta Das
- Rick WangRWRick Wang
- Richard KaniaRKRichard Kania
- 1 September 2015
- journal article
- Published by Elsevier in Engineering Failure Analysis
- Vol. 55, 288-299
Abstract
No abstract availableFunding Information
- Natural Sciences and Engineering Research Council of Canada (NSERC)
- TransCanada Pipelines
- Center for Engineering Research in Pipelines (CERP)
This publication has 14 references indexed in Scilit:
- Premature failure of superduplex stainless steel pipe by pitting in sea water environmentEngineering Failure Analysis, 2014
- Stress corrosion failure of an X52 grade gas pipelineEngineering Failure Analysis, 2014
- Microstructural and mechanical factors influencing high pH stress corrosion cracking susceptibility of low carbon line pipe steelEngineering Failure Analysis, 2014
- Assessment of a gouge and dent defect in a pipeline by a combined criterionEngineering Failure Analysis, 2014
- A closed-form solution for lateral indentation of pressurized pipes resting on a flexible bedInternational Journal of Mechanical Sciences, 2013
- Failure of Pressurized Corroded Pipeline Subject to Axial Compression: A Parametric StudyJournal of Offshore Mechanics and Arctic Engineering, 2013
- Limit analysis of flaws in pressurized pipes and cylindrical vessels. Part II: Circumferential defectsEngineering Fracture Mechanics, 2013
- Analysis of Pipes Containing Plain and Gouged DentsStrain, 2011
- Denting of internally pressurized tubes under lateral loadsInternational Journal of Mechanical Sciences, 2006
- The effect of dents in pipelines—guidance in the pipeline defect assessment manualInternational Journal of Pressure Vessels and Piping, 2004