Results from an international interlaboratory study on light‐ and elevated temperature‐induced degradation in solar modules
Open Access
- 5 May 2022
- journal article
- research article
- Published by Wiley in Progress in Photovoltaics: Research and Applications
- Vol. 30 (11) , 1255-1269
Abstract
This paper reports the results of an international interlaboratory comparison study on light‐ and elevated temperature‐induced degradation (LETID) on crystalline silicon photovoltaic (PV) modules. A large global network of PV module manufacturers and PV testing laboratories collaborated to design a protocol for LETID detection and screen a large and diverse set of prototype modules for LETID. Results across labs indicate the reproducibility of LETID testing is likely within ±1% of maximum power (PMP). In intentionally engineered LETID‐sensitive modules, mean degradation after the prescribed detection stress is roughly 6% PMP. In other module types the LETID sensitivity is smaller, and in some we observe essentially negligible degradation attributable to LETID. In LETID‐sensitive modules, both open‐circuit voltage (VOC) and short‐circuit current (ISC) degrade by a roughly similar magnitude. We observe, as do previous studies, that LETID affects each cell in a module differently. An investigation of the potential mismatch losses caused by nonuniform LETID degradation found that mismatch loss is insignificant compared to the estimated loss of cell ISC, which drives loss of module ISC. Overall, this work has helped inform the creation of a forthcoming standard technical specification for LETID testing of PV modules, IEC TS 63342 ED1, and should aid in the interpretation of results from that and other LETID tests.Keywords
Funding Information
- U.S. Department of Energy (DE‐AC36‐08GO28308)
- Economic Development Board - Singapore
- Energy Market Authority of Singapore
- National Research Foundation Singapore
- National University of Singapore
- Office of Energy Efficiency and Renewable Energy
- Solar Energy Technologies Office
This publication has 51 references indexed in Scilit:
- Modulation of Carrier‐Induced Defect Kinetics in Multi‐Crystalline Silicon PERC Cells Through Dark AnnealingSolar RRL, 2017
- Fast Regeneration Processes to Avoid Light-Induced Degradation in Multicrystalline Silicon Solar CellsIEEE Journal of Photovoltaics, 2016
- Degradation of multicrystalline silicon solar cells and modules after illumination at elevated temperatureSolar Energy Materials and Solar Cells, 2015
- Simplified technique for calculating mismatch loss in mass productionSolar Energy Materials and Solar Cells, 2015
- The Recombination Parameter J0Energy Procedia, 2014
- The influence of mismatch of solar cells on relative power loss of photovoltaic modulesSolar Energy, 2013
- Analysis and Optimization of the Bulk and Rear Recombination of Screen-Printed PERC Solar CellsEnergy Procedia, 2012
- Experimental study of mismatch and shading effects in the – characteristic of a photovoltaic moduleSolar Energy Materials and Solar Cells, 2006
- Cell binning method analysis to minimize mismatch losses and performance variation in Si-based modules2003
- Improved value for the silicon intrinsic carrier concentration from 275 to 375 KJournal of Applied Physics, 1991