Room-Temperature Microfluidics Packaging Using Sequential Plasma Activation Process
Authors:
- S. SueharaSSS. Suehara
- H. TakagiHTH. Takagi
- T.H. KimTKT.H. Kim
- R. MaedaRMR. Maeda
- T. SugaTST. Suga
- 7 August 2006
- journal article
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Advanced Packaging
- Vol. 29 (3) , 448-456
Abstract
A sequential plasma activation process consisting of oxygen reactive ion etching (RIE) plasma and nitrogen radical plasma was applied for microfluidics packaging at room temperature. Si/glass and glass/glass wafers were activated by the oxygen RIE plasma followed by nitrogen microwave radicals. Then, the activated wafers were brought into contact in atmospheric pressure air with hand-applied pressure where they remained for 24 h. The wafers were bonded throughout the entire area and the bonding strength of the interface was as strong as the parents bulk wafers without any post-annealing process or wet chemical cleaning steps. Bonding strength considerably increased with the nitrogen radical treatment after oxygen RIE activation prior to bonding. Chemical reliability tests showed that the bonded interfaces of Si/Si could significantly withstand exposure to various microfluidics chemicals. Si/glass and glass/glass cavities formed by the sequential plasma activation process indicated hermetic sealing behavior. SiOx Ny was observed in the sequentially plasma-treated glass wafer, and it is attributed to binding of nitrogen with Si and oxygen and the implantation of N2 radical in the wafer. High bonding strength observed is attributed to a diffusion of absorbing water onto the wafer surfaces and a reaction between silicon oxynitride layers on the mating wafers. T-shape microfluidic channels were fabricated on glass wafers by bulk micromachining and the sequential plasma-activated bonding process at room temperatureKeywords
This publication has 23 references indexed in Scilit:
- Combined process for wafer direct bonding by means of the surface activation method2004
- Secondary phase inclusions in polycrystalline sheet siliconJournal of Crystal Growth, 2004
- Wafer Level Surface Activated Bonding Tool for MEMS PackagingJournal of the Electrochemical Society, 2004
- Strength and leak testing of plasma activated bonded interfacesSensors and Actuators A: Physical, 2002
- Effects of Plasma Activation on Hydrophilic Bonding of Si and SiO[sub 2]Journal of the Electrochemical Society, 2002
- Fabrication techniques and materials commonly used for the production of microreactors and micro total analytical systemsTrAC Trends in Analytical Chemistry, 2000
- Glass-to-glass anodic bonding with standard IC technology thin films as intermediate layersSensors and Actuators A: Physical, 2000
- Time-Dependent Surface Properties and Wafer Bonding of O[sub 2]-Plasma-Treated Silicon (100) SurfacesJournal of the Electrochemical Society, 2000
- Low-temperature direct bonding of silicon and silicon dioxide by the surface activation methodSensors and Actuators A: Physical, 1998
- Effect of Surface Roughness on Room-Temperature Wafer Bonding by Ar Beam Surface ActivationJapanese Journal of Applied Physics, 1998