Structural, microstructural, and electrical properties of gold films and Schottky contacts on remote plasma-cleaned, n-type ZnO{0001} surfaces
- 6 May 2005
- journal article
- conference paper
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 97 (10) , 103517
Abstract
Current–voltage measurements of Au contacts deposited on ex situ cleaned, -type ZnO(0001) surfaces showed reverse bias leakage current densities of at 4.6 (3.75) V reverse bias and ideality factors (both surfaces) before sharp, permanent breakdown (soft breakdown). This behavior was due primarily to the presence of monolayers (ML) of hydroxide, which forms an electron accumulation layer and increases the surface conductivity. In situ remote plasma cleaning of the (0001) surfaces using a mixture for the optimized temperatures, times, and pressure of , 60 (30) min, and 0.050 Torr reduced the thickness of the hydroxide layer to and completely eliminated all detectable hydrocarbon contamination. Subsequent cooling of both surfaces in the plasma ambient resulted in the chemisorption of oxygen and a change from 0.2 eV of downward band bending for samples cooled in vacuum to 0.3 eV of upward band bending indicative of the formation of a depletion layer of lower surface conductivity. Cooling in either ambient produced stoichiometric ZnO{0001} surfaces having an ordered crystallography as well as a step-and-terrace microstructure on the surface; the (0001) surface was without distinctive features. Sequentially deposited, unpatterned Au films, and presumably the rectifying gold contacts, initially grew on both surfaces cooled in the plasma ambient via the formation of islands that subsequently coalesced, as indicated by calculations from x-ray photoelectron spectroscopy data and confirmed by transmission electron microscopy. Calculations from the current–voltage data of the best contacts revealed barrier heights on the (0001) surfaces of , a saturation current density of , a lower value of , a significantly lower leakage current density of at 8.5 (7.0) V reverse bias prior to sharp, permanent breakdown (soft breakdown). All measured barrier heights were lower than the predicted Schottky–Mott value of 1.0 eV, indicating that the interface structure and the associated interface states affect the Schottky barrier. However, the constancy in the full width at half maximum of the core levels for Zn and O , before and after sequential in situ Au depositions, indicated an abrupt, unreacted interface. Transmission electron microscopy confirmed the abruptness of an epitaxial interface. Annealing the contacts on the (0001) surface to and resulted in decreases in the ideality factors to and and increases in saturation current density to 9.05 and , the barrier height to and , and in the leakage current densities to at 6 V and at 7 V, respectively.
Keywords
This publication has 32 references indexed in Scilit:
- Recent progress in processing and properties of ZnOSuperlattices and Microstructures, 2003
- Electrical characterization of vapor-phase-grown single-crystal ZnOApplied Physics Letters, 2002
- Production of nitrogen acceptors in ZnO by thermal annealingApplied Physics Letters, 2002
- Electrical characterization of 1.8 MeV proton-bombarded ZnOApplied Physics Letters, 2001
- Recent advances in ZnO materials and devicesMaterials Science and Engineering: B, 2001
- Hydrogen as a Cause of Doping in Zinc OxidePhysical Review Letters, 2000
- First-principles study of native point defects in ZnOPhysical Review B, 2000
- Admittance Spectroscopy of ZnO CrystalsJapanese Journal of Applied Physics, 1990
- The influence of incongruent decomposition and oxygen chemisorption on the temperature and pressure dependence of the conductivity of zinc oxide filmsApplied Surface Science, 1987
- Ultraviolet detectors in thin sputtered ZnO filmsApplied Optics, 1986