Ultrasound-Driven Interfacial-Electrochemical-Radical Synergistic Pathways for Reclaiming Fe/P from Refractory Ferrophosphorus Residue

Authors:

Abstract
Recovering iron and phosphorus from ferrophosphorus residue enables by-product valorization. However, the presence of stable metal phosphides severely hinders conventional leaching, leading to prolonged processing times and substantial waste generation. To address these challenges, this study first subjects the ferrophosphorus residue to high-temperature activation pretreatment, followed by ultrasound-enhanced sulfuric acid/hydrogen peroxide leaching, to achieve efficient recovery of Fe and P. Under optimum conditions, the leaching percentages of iron and phosphorus reach 93.21 and 87.15%, corresponding to absolute increases of 23.26 and 12.05%, respectively, over conventional methods. Kinetic modeling indicates an apparent activation energy reduction of 14.26 kJ/mol, confirming that ultrasonic irradiation lowers the reaction’s energy threshold. Surface energetic evaluations show a 7.91° decrease in water contact angle and a concurrent 5.38 mJ/m2 augmentation of solid surface free energy. This improves wettability, optimizes solid-liquid interfacial kinetics, and reduces mass transfer resistance. Furthermore, Tafel plots reveal a 0.063 V (vs. MSE) cathodic shift in corrosion potential alongside an 8.431 × 10–5 A/cm2 elevation in corrosion current density. Acoustic micro-jets clean the residue surface to maintain high reactivity, while EPR analysis confirms the accelerated generation of ·OH and SO4–· radicals. This radical generation elevates the system’s oxidative capacity, facilitating residue leaching. This work provides a new perspective for applying ultrasonic technology to recover valuable elements from ferrophosphorus residue.
Funding Information
  • ?Yunnan Revitalization Talents Support Plan? - Youth Talent Program
  • National Natural Science Foundation of China (NSFC) (52567025)

This publication has 36 references indexed in Scilit: