Analysis of organic-coated steels by using small-angle neutron scattering
Authors:
- 24 December 2014
- journal article
- Published by Pleiades Publishing Ltd in Physics of Metals and Metallography
- Vol. 115 (13) , 1333-1337
Abstract
Small angle neutron scattering (SANS) was applied to analyze the degradation of an organic coating layer on steel and for the non-destructive evaluation of the corrosion behavior of the coated steels. The steel was a modified AISI 1004 steel with 1.2% aluminum and 0.8% chromium to improve corrosion resistance. The organic coating layer was epoxy primer, which was painted with about 250-μm thickness on the steel. The organic-coated specimen was subjected to wet-and-dry cyclic corrosion conditions for 112 days in artificial sea water at 40°C. The corrosion potential and the corrosion rate of the steel were −1.1 VSHE and 8.8 × 10−5 A/cm2, respectively. SANS spectra showed that nano-sized defects were not formed in the organic layers after the 112-day wet-and-dry corrosion test. Artificial cracks of the organic layer by X-cutting made corrosion spots of submicron size after a 2-day wet-and-dry corrosion test, which were monitored by SANS.Keywords
This publication has 10 references indexed in Scilit:
- Small-angle neutron scattering study of the wet and dry high-temperature oxidation of alumina- and chromia-forming stainless steelsCorrosion Science, 2012
- Small-angle neutron scattering study of nanophase separated epoxy hydrogelsJournal of Non-Crystalline Solids, 2010
- Overview of processing, microstructure and mechanical properties of ultrafine grained bcc steelsMaterials Science and Engineering: A, 2006
- Structure and swelling behaviour of hydrophilic epoxy networks investigated by SANSPolymer, 2006
- Texture and anisotropyReports on Progress in Physics, 2004
- Calculation of the surface energy of bcc metals by using the modified embedded‐atom methodSurface and Interface Analysis, 2003
- Modeling of texture development during recrystallization of interstitial free steelActa Materialia, 1997
- Microtexture analysis of interstitial-free steelMaterials Characterization, 1997
- A thermodynamic evaluation of the Fe-Cr-Mn-C systemMetallurgical Transactions A, 1993
- Determination of the corrosion products of iron in sea water with and without sulphidesMaterials and Corrosion, 1983