The type IV dental stone is widely used for the fabrication of dyes and master casts for fixed and removable partial prostheses. It is typically normal to wait at least 24 hours for the casts to dry prior to beginning the laboratory procedures. The waiting time has been shown to be greatly reduced by using microwave drying. This study evaluated the influence of drying techniques at room temperature and microwave oven on the linear dimensional change, compressive strength and detail reproduction in type IV dental stones. Three type IV dental stone brands were selected; elite Rock, Shera Premium and Durone IV. Two different drying protocols were tested in 4 groups (n=10); G-room temperature (25±4 ºC) dried for 2 hours; G2--room temperature dried for 24 hours; G3-room temperature dried for 7 days and G4--microwave oven dried at 800 W for 5 minutes and after 2 hours at room temperature. After drying, the samples were assayed for dimensional charges. The sample surface was submitted to the ImageTool 3.0 software for compressive strength in a universal testing machine with a cell load of 50 KN at a crosshead speed of 0.5 mm/minutes and the detail reproduction was analyzed with a stereomicroscope at 25x magnification. The statistical analysis of the linear dimensional change and compressive strength data were conducted by the ANOVA test followed by the Tukey test (p<0.05). Detailed reproduction values were reported in percentages. For the compressive strength test, Elite Rock and Durone IV did not present significant differences between G2 and G4, while Shera Premium did not present differences between G3 and G4. The best reproduction levels were observed for G3. Dental stone microwave oven drying showed a linear dimensional change similar to after room temperature drying for 24 hours and 7 days. The compressive strength of the stone dried in the microwave oven was similar to those dried at room temperature for 24 hours, with the exception of Shera Premium, which had similar results for microwave and room temperature drying for 7 days. For the microwave drying method the detail reproduction levels for samples dried at room temperature for 24 hours and 7 days were similar, except for the Durone IV.Keywords
This publication has 13 references indexed in Scilit:
- Effect of repeated disinfections by microwave energy on the physical and mechanical properties of denture base acrylic resinsBrazilian Dental Journal, 2009
- Efficacy of high-level microwave disinfection of dental gypsum casts: the effects of number and weight of casts.2007
- Tensile strength of type IV dental stones dried in a microwave ovenThe Journal of Prosthetic Dentistry, 2002
- Detail reproduction, contact angles, and die hardness of elastomeric impression and gypsum die material combinations.2001
- Comparision of diametral tensile strength of microwave and oven-dried investment materialsThe Journal of Prosthetic Dentistry, 1999
- Fracture strength of Type IV and Type V die stone as a function of timeThe Journal of Prosthetic Dentistry, 1997
- Effect of microwave oven drying on surface hardness of dental gypsum productsThe Journal of Prosthetic Dentistry, 1985
- Microwave sterilizationThe Journal of the American Dental Association, 1985
- Microwave oven drying of artificial stoneThe Journal of Prosthetic Dentistry, 1985
- New American Dental Association Specification No. 25 for Dental Gypsum ProductsThe Journal of the American Dental Association, 1972