Abstract
Polymers have been successfully used for implant applications, however, challenges remain as their design requires a delicate balance between mechanical, chemical, and physical properties to ensure cell survival and tissue formation. Additive manufacturing techniques, such as SLA, offer the opportunity to achieve desired physical and mechanical properties because of the precision and control over architecture. Such control allows manipulation over the distribution of mechanical properties throughout the implant. PMA/HA and PMA/TiO2 solid and porous structures are, therefore, manufactured using room temperature SLA techniques. HA and TiO2 are added to the polymer for bio‐functionalizing purposes. The apatite forming ability of the samples are evaluated using HBSS immersion. All PMA and PMA/TiO2 samples does not show any bioactivity in terms of apatite formation, although limited amounts of CaO is found on PMA surfaces. PMA/HA samples demonstrate bioactivity with newly formed apatite formation observed after 3 and 5 week HBSS immersion.

This publication has 51 references indexed in Scilit: