Abstract
As part of the Capital Improvement Program at Tulsa International Airport, reconstruction of the runways 18-36 and 8-26 intersection was conducted to address Foreign Object Debris (FOD) caused by D-cracking deterioration of the concrete in the form of joint and corner spalling and popouts. Detailed planning and design for the reconstruction of the intersection was conducted to meet the Airport’s requirements of having at least one runway open for passenger and cargo traffic during weekdays. To limit interruptions to traffic operations, reconstruction of the runway intersection was conducted over weekend closures with limited night week closures for minor work. The concrete pavement was constructed with dowels but it was designed assuming no load transfer at the joints to provide a conservative approach. The approach allowed using the existing non-stabilized aggregate base since stabilized bases are required under rigid pavements serving aircraft weighing 100,000 lbs or more. To limit damage of the existing aggregate base/clayey subgrade system the slabs were to be removed by the lift method only. The design required removing the existing 25 foot concrete slabs and replacing them with 18.75 foot by 20 foot concrete slabs at a slightly different grade than existing. To accomplish this and to minimize the number of weekend closures, the new concrete was to be placed in 37.5 foot paving lanes with a saw cut in the middle. This required careful considerations during demolition since the runway intersection was to be operational during weekdays. The contractor paved 38.5 foot lanes to provide grade transition to existing. The transition portion was saw cut during removal of the adjacent lane. The design also required the use of conventional concrete mixes with dense graded aggregates mixes to attain a flexural strength of 550 psi after 24 hours and 650 psi at 28 days. This was accomplished by using dense graded aggregates, and 7.5 sacks of cementitious material which included 25% fly ash replacement. The proposed mixture was considered adequate for the cold to moderate air temperatures expected during construction. Construction details included measures for avoiding sympathy cracking, thermo-cracking impact due to temperature variations, transitions from existing to new grades, requirements for back-up equipment, etc.