Repair bond strength and surface topography of resin‐ceramic and ceramic restorative blocks treated by laser and conventional surface treatments
Authors:
- 8 December 2020
- journal article
- research article
- Published by Wiley in Microscopy Research and Technique
- Vol. 84 (6) , 1145-1154
Abstract
This study intended to compare the repair bond strength of computer‐aided design/computer‐aided manufacturing (CAD/CAM) blocks consisting of resin and feldspathic ceramics following different surface treatments using the microtensile bond strength (μTBS) test. Ten specimens were prepared with 4 mm height for Vita Enamic (VE), Lava Ultimate (LU), Vita Mark II (VM), and thermocycled (10,000 cycle, 5–55°C). Each material was categorized into one of five subgroups according to following surface treatments: (a) bur grinding (BG), (b) hydrofluoric acid etching (HF), (c) neodymium‐doped yttrium aluminum garnet (Nd:YAG or NY), (d) erbium‐doped yttrium aluminum garnet (Er:YAG or EY), and (e) erbium, chromium‐doped yttrium, scandium, gallium, and garnet (Er,Cr:YSGG or ECY) laser conditioning. After surface treatment procedures, specimens were properly restored to 4 mm high with a micro‐hybrid composite resin. Bar specimens (1 × 1 × 8 mm) were obtained using a low‐speed cutting machine and then thermocycled (10,000 cycle, 5–55°C). The μTBS was tested at 1 mm/min crosshead speed, and failure modes were evaluated. Data were analyzed with two‐way ANOVA and post hoc Tukey tests. LU‐BG showed significantly higher μTBS (32.94 ± 5.80 MPa) compared to LU‐laser groups (p < .05). VE‐BG showed significantly higher μTBS (22.06 ± 4.26 MPa) compared to other VE groups (p < .05). Among the laser groups, the NY laser produced the lowest (p < .05) μTBS for LU (13.42 ± 3.44 MPa) and VE (2.27 ± 0.85 MPa), while EY showed the highest (p < .05). Laser‐treated VM groups were all prefailured. VM‐HF produced a higher μTBS (18.73 ± 3.75 MPa) than VM‐BG (5.05 ± 1.76 MPa) (p < .05).Keywords
This publication has 52 references indexed in Scilit:
- Adhesion of veneering resins to polymethylmethacrylate-based CAD/CAM polymers after various surface conditioning methodsActa Odontologica Scandinavica, 2012
- Effects of different surface treatments on shear bond strength in two different ceramic systemsLasers in Medical Science, 2012
- FDI World Dental Federation: clinical criteria for the evaluation of direct and indirect restorations—update and clinical examplesClinical Oral Investigations, 2010
- The effect of different surface treatments on roughnessand bond strength in low fusing ceramicsLasers in Medical Science, 2010
- Effect of the amount of 3-methacyloxypropyltrimethoxysilane coupling agent on physical properties of dental resin nanocompositesDental Materials, 2009
- Effect of Feldspathic Ceramic Surface Treatments on Bond Strength to Resin CementPhotomedicine and Laser Surgery, 2007
- Bond Strengths of All-Ceramics: Acid vs Laser EtchingOperative Dentistry, 2007
- Microtensile bond strength of different components of core veneered all-ceramic restorationsDental Materials, 2006
- Ablation of composite resins using Er:YAG laser—comparison with enamel and dentinLasers in Surgery and Medicine, 2003
- Bonding of restorative and veneering composite resin to somepolymeric compositesDental Materials, 2001